Abstract
The 10th Liège Conference on Materials for Advanced Power Engineering was held in September 2014. This article presents conference highlights, including the current state of European materials research for advanced power engineering applications; European multinational programs in this area; and critical research topics including creep-fatigue, new alloy development, and materials developments for gas turbines.