Capable of stopping 50-caliber, armor-piercing rounds, ALON and Spinel are hard and durable transparent polycrystalline materials manufactured using powder based processes. This article describes their unique combination of mechanical, optical, and chemical properties, and reports on recent advances in manufacturing to enable their use for critical defense, industrial, and consumer applications.