Abstract
Because alloy steel hardenability is such an important factor in part manufacturing, the Center for Heat Treating Excellence (CHTE) is conducting research through simulations and laboratory testing aimed at learning more about the performance of gas quenching systems used to harden newer alloy steels. The primary goal of the study is to establish a standard method to evaluate gas-quench steel hardenability. Heat transfer coefficients will be determined for different gas pressures and during the cooling phase.