Aluminum, one of the most widely used structural metals in modern industry, is produced in quantities exceeded only by steel. Its light weight, corrosion resistance, high strength after heat treatment, and global availability of bauxite ores make aluminum attractive for everything from kitchen utensils to spacecraft. This article describes early work to develop low-cost aluminum for industrial applications.