This article briefly describes a new carbon nanocoating that provides corrosion protection through a two-coat system that is applied like paint, acts like plating, and relies on a much lower zinc content than existing three-coat solutions. Lost conductivity resulting from reduced zinc content is offset by highly conductive carbon nanotubes in the base layer.