Abstract
To meet the rigorous demands of next-generation computer technology, new approaches to nondestructive measurement for early stage, temperature dependent materials characterization are needed. Terahertz spectroscopy bypasses the limitations of other characterization techniques by enabling nondestructive measurement under variable temperature and high magnetic field conditions.