Abstract
The unique metallurgy and microstructure of Cu-Ni-Sn spinodal alloys provide a combination of strength, toughness, hardness, and corrosion resistance, suiting them for applications ranging from bearings, bushings, and friction surfaces in all sorts of machinery to electrical connectors and EMI shielding gaskets.