Vacuum solution nitriding is a promising technique for increasing the surface hardness, load-bearing capability, and fatigue strength of martensitic stainless steels without sacrificing corrosion resistance. This article examines the effects of nitriding pressure and temperature on surface nitrogen content and case depth in four martensitic stainless steels.