Abstract
Thermal spraying is being incorporated into more manufacturing processes where its primary role is to deposit a layer of material or a free-standing structure that has a functional, rather than a passive, role. Examples include thermally sprayed membranes, electrodes, antennas, thermocouples, inductors, and electrical contacts.