Abstract
Modeling and simulation are proving to be an effective alternative to the trial-and-error practices often used when developing and evaluating nondestructive tests for materials characterization. This article demonstrates the benefits of modeling in different cases where eddy current and ultrasonic inspection methods are employed.
This content is only available as a PDF.