Abstract
Optimizing the integrity and performance of highly engineered surfaces and structures requires the ability to visualize and understand material behavior over multiple length and time scales from a three-dimensional perspective. The Electron Microscopy Centre at the University of Manchester is equipped for such work as demonstrated in problem-solving scenarios involving multiscale imaging and analysis of the progression of intergranular corrosion in Al alloy 2024, the catalytic effect of silver nanoparticles in seawater, recrystallization in a volume element of a bronze alloy, and defect progression on graphene surfaces.