1-20 of 259

Search Results for welded joints

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Proceedings Papers

AM-EPRI2016, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Eighth International Conference, 544-555, October 11–14, 2016,
... Abstract This study is concerned with the creep damage evaluation for the welded joint of modified 9Cr-1Mo steels. A finite element prediction method based on ductility exhaustion approach has been proposed. Degradation of creep ductility under multi-axial stress state has been formulated from...
Proceedings Papers

AM-EPRI2013, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Seventh International Conference, 537-548, October 22–25, 2013,
... Abstract In this paper, the performance of T23 and 12Cr1MoVG water wall tubes as well as their welded joints in engineering applications is reported. It was found that the T23 water wall tube may have water leak problems during its operation. In order to make sure the safe operation, leakage...
Proceedings Papers

AM-EPRI2013, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Seventh International Conference, 948-959, October 22–25, 2013,
... Abstract The creep rupture properties of welded joints of advanced 9%Cr-Mo-Co-B steel used for 620°C USC steam turbine have been studied. The welded joints were prepared by means of shielded metal arc welding (SMAW). A lot of creep tests have been conducted and the results indicate...
Proceedings Papers

AM-EPRI2013, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Seventh International Conference, 992-1005, October 22–25, 2013,
... are unquestionable. This article presents experience gained while welding dissimilar joints of advanced steels TEMPALOY AA-1 and T92, with the use of EPRI P87, Inconel 82 and Inconel 617 filler metals. The tests involving the said steel grades belong to the very few carried out in the world. austenitic...
Proceedings Papers

AM-EPRI2004, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Fourth International Conference, 899-918, October 25–28, 2004,
... the framework of COST 522 program concerning the influence of simulation of element temperature operating conditions on Chaгpy V notch toughness, HV10 hardness, microstructure of simulated HAZ's, assessment of steel weldability, strength properties. The welded joints structure stability and HAZ after stress...
Proceedings Papers

AM-EPRI2004, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Fourth International Conference, 930-949, October 25–28, 2004,
... heat-affected zone low cycle fatigue microstructural observations welded joints httpsdoi.org/10.31399/asm.cp.am-epri-2004p0930 Copyright © 2005 ASM International® 930 931 932 933 934 935 936 937 938 939 940 941 942 943 944 945 946 947 948 949 Copyright © 2004 ASM International. All rights...
Proceedings Papers

AM-EPRI2004, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Fourth International Conference, 967-986, October 25–28, 2004,
... been evaluated. At REMAK- Opole (Enterprise for the Modernisation of Power Installations) and RAFAKO tube and pipe test joints were welded, to select proper fabrication conditions. Mechanical properties of the welded test joints, KV notch toughness of weld metals and HAZ’s and microstructures were...
Proceedings Papers

AM-EPRI2010, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Sixth International Conference, 584-602, August 31–September 3, 2010,
... to develop a comprehensive database on the creep-fatigue behavior of Grade 92 steel's base metal and welded joints and to establish a suitable life estimation procedure. Key findings include: (i) a thick pipe with submerged arc welding (SAW) was manufactured for testing; (ii) base metal and cross-weld...
Proceedings Papers

AM-EPRI2007, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Fifth International Conference, 303-319, October 3–5, 2007,
..., technological properties, and microstructure of welded joints produced at RAFAKO S.A. The extensive research program encompassed a broad range of tests on both parent material and welded joints, including mechanical property assessments at room temperature, creep resistance evaluations, low-cycle fatigue...
Proceedings Papers

AM-EPRI2007, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Fifth International Conference, 762-782, October 3–5, 2007,
... Abstract The strength of welded joints in high-chromium steels is a critical concern for operators of ultra-supercritical thermal power plants. To investigate this, a series of creep-fatigue tests with tensile strain holds were conducted on welded joints of two widely used high-chromium steels...
Proceedings Papers

AM-EPRI2007, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Fifth International Conference, 874-883, October 3–5, 2007,
... occurs in HAZ of the weldment. In the creep rupture test of these welded joints the rupture strength is lower than that of the parent metal, and sometimes this reduction of strength is caused by TypelV cracking. To develop an effective method to improve the rupture strength of welded joint, advanced...
Proceedings Papers

AM-EPRI2019, 2019 Joint EPRI – 123HiMAT International Conference on Advances in High-Temperature Materials, 1123-1131, October 21–24, 2019,
... Abstract Welded joints of Ni-base alloys are often the critical part of components operated under high temperature service conditions. Especially welds in thick-walled structures are susceptible to various crack phenomena. Creep rupture and deformation behavior of different similar welds...
Proceedings Papers

AM-EPRI2024, Advances in Materials, Manufacturing, and Repair for Power Plants: Proceedings from the Tenth International Conference, 760-765, February 25–28, 2025,
... Abstract In this study, the creep strength of welded joints of Grade 91 Type 1 and Type 2 steels was evaluated. It was determined that impurity elements in the Type 1 steel reduced its creep strength. This reduction was attributed to an increase in the amount of residual carbides in the fine...
Proceedings Papers

AM-EPRI2016, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Eighth International Conference, 974-982, October 11–14, 2016,
... liquation crack initiation site FB2 steel hot ductility test Laves phase thermal cycle turbine rotors weld joints welding Advances in Materials Technology for Fossil Power Plants Proceedings from the Eighth International Conference October 11 14, 2016, Albufeira, Algarve, Portugal httpsdoi.org...
Proceedings Papers

AM-EPRI2016, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Eighth International Conference, 931-938, October 11–14, 2016,
... Abstract Developed 9Cr-3W-3Co-Nd-B heat-resistant steel SAVE12AD (Recently designated as ASME Grade 93) pipes and tubes have higher creep strength in both base metal and welded joints than conventional high Cr ferritic steels such as ASME Grades 91, 92 and 122. The welded joints of SAVE12AD...
Proceedings Papers

AM-EPRI2016, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Eighth International Conference, 1001-1009, October 11–14, 2016,
... was early overcome and was wrong. According to the present experience the T24 steel is welded with preheating at 150-250°C depending on the wall thickness and welded joint toughness in order to achieve required hardness and impact toughness values. Opinions on the T24 welded joints post weld heat treatment...
Proceedings Papers

AM-EPRI2013, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Seventh International Conference, 607-614, October 22–25, 2013,
... Abstract In order to clarify the effect of stress state on microstructural changes during creep, the microstructure was observed in the central part of the cross section of the fine-grained heat-affected zone (FGHAZ) and in the surface region of the FGHAZ in Gr.92 steel welded joint. Creep...
Proceedings Papers

AM-EPRI2004, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Fourth International Conference, 987-998, October 25–28, 2004,
... Abstract This study investigated the creep rupture strength and microstructure evolution in welded joints of high-boron, low-nitrogen 9Cr steels developed by NIMS. The welds were fabricated using the GTAW process and Inconel-type filler metal on steel plates with varying boron content (47-180...
Proceedings Papers

AM-EPRI2019, 2019 Joint EPRI – 123HiMAT International Conference on Advances in High-Temperature Materials, 162-173, October 21–24, 2019,
... Abstract Two materials with different purity of 2.25Cr-1Mo steel thick weld joint were prepared and creep rupture behavior was investigated by large sized specimens. For high purity material, two types of challenging heat treatment was tried to modify the original microstructural conditions...
Proceedings Papers

AM-EPRI2019, 2019 Joint EPRI – 123HiMAT International Conference on Advances in High-Temperature Materials, 405-415, October 21–24, 2019,
... Abstract In the present study, the Inconel 617B superalloy welded trial rotor was fabricated by narrow gap tungsten inert gas (NG-TIG) welding and the effects of temperature on fracture toughness of its welded joint were investigated at 650 ℃ and 730 ℃. Fracture toughness (J0.2) of the base...