1-20 of 155

Search Results for weld repairs

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Proceedings Papers

AM-EPRI2013, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Seventh International Conference, 1206-1219, October 22–25, 2013,
... will also be discussed and how they will influence the life or operation of the component. Application of weld repairs to critical components such as rotors and steam chest casings will be highlighted and how defect tolerant design concept is applied for the repair procedure and the acceptance standard...
Proceedings Papers

AM-EPRI2016, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Eighth International Conference, 556-567, October 11–14, 2016,
... Abstract The application of cold weld repair techniques in the power industry has been well documented. This type of repair is only considered when a conventional repair (involving post-weld heat treatment) is impracticable or the penalties of time and cost for conventional repair...
Proceedings Papers

AM-EPRI2024, Advances in Materials, Manufacturing, and Repair for Power Plants: Proceedings from the Tenth International Conference, 247-258, February 25–28, 2025,
... electric power generation gas tungsten arc welding generator rotors plasma arc welding steam turbines surface hardness welding repair X-ray fluorescence analysis Advances in Materials, Manufacturing, and Repair for Power Plants: Proceedings from the Tenth International Conference October 15 18...
Proceedings Papers

AM-EPRI2019, 2019 Joint EPRI – 123HiMAT International Conference on Advances in High-Temperature Materials, 1079-1089, October 21–24, 2019,
... because of flexible operation. Therefore, there is a growing need for weld repair techniques including those which do not mandate post weld heat treatment (PWHT), e.g. so-called ‘temper bead’ weld repair. In this study, a simulated weld repair was performed using a temper bead technique. The maximum...
Proceedings Papers

AM-EPRI2013, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Seventh International Conference, 973-981, October 22–25, 2013,
... Abstract Qualifying welding procedures for repair of components in high temperature service requires careful consideration of factors including identification of the materials involved, existing mechanical properties and service operating parameters such as temperature, pressure and environment...
Proceedings Papers

AM-EPRI2024, Advances in Materials, Manufacturing, and Repair for Power Plants: Proceedings from the Tenth International Conference, 50-61, February 25–28, 2025,
... Abstract There is a growing need to automate the gas tungsten arc welding process for fabrication and repair of nuclear components due to an increasing shortage of experienced welders. Therefore, a collaborative effort has been performed in this study to develop a fully autonomous gas tungsten...
Proceedings Papers

AM-EPRI2024, Advances in Materials, Manufacturing, and Repair for Power Plants: Proceedings from the Tenth International Conference, 855-860, February 25–28, 2025,
... and where it is applied in Coke drum repair welding. Comparative test results of the different weld processes for fatigue performance, HAZ tempering, and toughness will also be presented. chromium-molybdenum alloy steel coke drums fatigue performance gas tungsten arc welding heat-affected zone...
Proceedings Papers

AM-EPRI2024, Advances in Materials, Manufacturing, and Repair for Power Plants: Proceedings from the Tenth International Conference, 135-146, February 25–28, 2025,
... of nickel and tramp boron in austenitic materials commonly used in reactor internals can lead to the generation of trapped helium and the associated risk of helium-induced cracking (HeIC) during weld repairs. In the weld heat affected zone, where temperatures are insufficient to allow the helium to diffuse...
Proceedings Papers

AM-EPRI2024, Advances in Materials, Manufacturing, and Repair for Power Plants: Proceedings from the Tenth International Conference, 397-408, February 25–28, 2025,
... of the degradation. Welding repair of reactor components may input excessive heat into these irradiated materials resulting in diffusion of trace amounts of helium within the grain boundaries of the weld heat-affected zone (HAZ). Intergranular HAZ cracking can then result from the combination of this helium...
Proceedings Papers

AM-EPRI2024, Advances in Materials, Manufacturing, and Repair for Power Plants: Proceedings from the Tenth International Conference, 88-98, February 25–28, 2025,
... the mechanical properties of 1CrMoV, highlighting the need for service- exposed property data to perform mechanical integrity assessments. Finally, the consequences for repair of damage will be discussed, illustrating how analysis can guide volume of material for excavation and selection of weld filler metal...
Proceedings Papers

AM-EPRI2013, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Seventh International Conference, 714-731, October 22–25, 2013,
... densities of voids further complicates in-service assessment of condition and weld repair of these steels. The present paper examines background on the nucleation and development of creep voids in 9 to 12%Cr martensitic steels and discusses factors affecting brittle behavior. brittle behaviour creep...
Proceedings Papers

AM-EPRI2013, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Seventh International Conference, 513-524, October 22–25, 2013,
.... In addition to these identified issues, 516 fabrication-related difficulties have been highlighted such as flame heating/straightening, excessive grinding, weld repair, brittle fracture and ferritic dissimilar metal welds. Examples for each of these difficulties will be briefly detailed in subsequent sections...
Proceedings Papers

AM-EPRI2024, Advances in Materials, Manufacturing, and Repair for Power Plants: Proceedings from the Tenth International Conference, iii-v, February 25–28, 2025,
... EPRI Advanced Nuclear Technology Elizabeth Benton EPRI (Conference Secretariat) Alex Bridges EPRI Materials Michael Gagliano EPRI Materials David Gandy EPRI Nuclear Materials Horst Hack EPRI Advanced Generation & Bulk Energy Storage Tapasvi Lolla EPRI Materials Nick Mohr EPRI Welding Repair Technology...
Proceedings Papers

AM-EPRI2024, Advances in Materials, Manufacturing, and Repair for Power Plants: Proceedings from the Tenth International Conference, 924-932, February 25–28, 2025,
... of Materials Science Engineering, The Ohio State University, Columbus, Ohio, USA Steve McCracken, Jonathan Tatman Welding and Repair Technology Center, Electric Power Research Institute, Charlotte, NC, USA ABSTRACT Solidification cracking (SC) is a defect that occurs in the weld metal at the end...
Proceedings Papers

AM-EPRI2024, Advances in Materials, Manufacturing, and Repair for Power Plants: Proceedings from the Tenth International Conference, 933-944, February 25–28, 2025,
... welding Advances in Materials, Manufacturing, and Repair for Power Plants: Proceedings from the Tenth International Conference October 15 18, 2024, Bonita Springs Florida, USA httpsdoi.org/10.31399/asm.cp.am-epri-2024p0933 Copyright © 2024 ASM International® All rights reserved...
Proceedings Papers

AM-EPRI2016, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Eighth International Conference, 983-988, October 11–14, 2016,
... of header suffered from leakage due to cracks during the hydrostatic test conducted by the manufacturer.This paper introduces inspection and evaluation of the header tube and welds repaired. 2 ON-SITE TEST Circumferential welds on 8 tube sections of 3 headers have been tested on site by means of hardness...
Proceedings Papers

AM-EPRI2024, Advances in Materials, Manufacturing, and Repair for Power Plants: Proceedings from the Tenth International Conference, 650-661, February 25–28, 2025,
... components manufactured from EA and DS superalloys was successfully resolved by modification of welding materials with boron and silicon to provide a sufficient amount of eutectic at terminal solidification to promote self-healing of liquation cracks along the weld - base material interface. For crack repair...
Proceedings Papers

AM-EPRI2016, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Eighth International Conference, 35-46, October 11–14, 2016,
... work with the IMPACT project (3), the UK INMAP project (4) demonstrated manufacturability of a full scale industrial size MarBN steel component, validated non destructive testing techniques, and established weld repair procedures. An 8,640kg net weight turbine valve casting was manufactured with a pour...
Proceedings Papers

AM-EPRI2007, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Fifth International Conference, 590-600, October 3–5, 2007,
... of development, it was found possible to grind them out and return to service without the need for weld repair. For stub cracks, where it was calculated that early recracking would be most likely, finite element analysis was used to define ground profiles which left the surface Type IV zones subjected...
Proceedings Papers

AM-EPRI2013, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Seventh International Conference, 525-536, October 22–25, 2013,
... occurred within both shop welds and field repair welds of the T23 material, originally performed without post weld heat treatment (PWHT). The original weld procedure for the T23/T23 butt welds utilized 100% gas tungsten arc welding-GTAW, with matching ER90S-G filler metal (chemistry similar to Grade 23...