AM-EPRI2016, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Eighth International Conference, 283-294, October 11–14, 2016,
... Abstract For raising thermal efficiency and decreasing CO 2 emission, China had constructed the first 600°C ultra-supercritical(USC) fossil power plant in 2006. Now more than a hundred 600°C, 1000MW USC electric power units have been put in service. Recently, China has also developed 620°C USC...
Proceedings Papers

AM-EPRI2019, 2019 Joint EPRI – 123HiMAT International Conference on Advances in High-Temperature Materials, 647-654, October 21–24, 2019,
... up to 20 000 hours. The morphology of the oxide scale and the microstructure of the bulk material were investigated. In addition, the effect of surface finish and pressure on the steam oxidation were also studied. advanced ultra-supercritical fossil power plants austenitic stainless steel...
Proceedings Papers

AM-EPRI2007, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Fifth International Conference, 46-58, October 3–5, 2007,
... with high pollution and high energy consumption and encourages to make supercritical and ultra supercritical units of above 600MW and large circulation fluidized bed units and to push forward the application of IGCC technology. Chinese government has required to shut down the small fossil fired power plants...
Proceedings Papers

AM-EPRI2019, 2019 Joint EPRI – 123HiMAT International Conference on Advances in High-Temperature Materials, 1215-1223, October 21–24, 2019,
... W, Hua F, Ming Y, et al, Materials Used for High-temperature Components of 600°C/620°C Ultra-supercritical Double-reheat Unit, Dongfang Turbine, No.1(2016), pp. 50-55. (In Chinese) [14] Fukuda, Yuji, Development of advanced ultra supercritical fossil power plants in Japan: materials and high...
Proceedings Papers

AM-EPRI2004, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Fourth International Conference, 35-50, October 25–28, 2004,
... in the properties of fabricated metal. For further improvement in the thermal efficiency of fossil-fired power plants with ultra supercritical steam parameter conditions aiming at temperatures above 700°C, alloy development concepts and material issues with increasing steam temperature must be reviewed...
Proceedings Papers

AM-EPRI2013, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Seventh International Conference, 448-458, October 22–25, 2013,
.... and DiGianfrancesco, A., The European Effort in Development of New High Temperature Rotor Materials Cost 536, Proc. 8th Liege Conference, Liege, Belgium, September 2006, pp 843-854 [3] Blaes, N., Donth, B., Diwo, A., Bokelmann, D., Rotor Forgings for Supercritical and Ultra supercritical Fossil Power Plants, Proc...
Proceedings Papers

AM-EPRI2007, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Fifth International Conference, 520-530, October 3–5, 2007,
... Abstract Reducing emissions and increasing economic competitiveness require more efficient steam power plants that utilize fossil fuels. One of the major challenges in designing these plants is the availability of materials that can stand the supercritical and ultra-supercritical steam...
Proceedings Papers

AM-EPRI2019, 2019 Joint EPRI – 123HiMAT International Conference on Advances in High-Temperature Materials, 1250-1261, October 21–24, 2019,
... in the development of new materials, were made to establish the technology for the ultra-supercritical power plants, which are the standard of today’s power generation. For decades voestalpine Boehler Special Steel has been a full package supplier of customized high quality special steels and forgings with close...
Proceedings Papers

AM-EPRI2013, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Seventh International Conference, 143-154, October 22–25, 2013,
.... Currently, steels used in power plants operating up to 600°C achieve efficiencies of 38-40%. Advanced Ultra Supercritical (A-USC) designs aim for a significant leap, targeting steam temperatures of 700°C and pressures of 35 MPa with a lifespan exceeding 100,000 hours. Ni-based superalloys are leading...
Proceedings Papers

AM-EPRI2013, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Seventh International Conference, 832-846, October 22–25, 2013,
... Abstract Nickel-based alloys and stainless steel Super304H, along with various coatings, are undergoing testing in a steam loop at Alabama Power’s Plant Barry. These materials are being evaluated for use in advanced ultra-supercritical (A-USC) fossil-fired power plants at temperatures ranging...
Proceedings Papers

AM-EPRI2019, 2019 Joint EPRI – 123HiMAT International Conference on Advances in High-Temperature Materials, 580-591, October 21–24, 2019,
... Abstract The harsh operating conditions of Advanced Ultra-Supercritical (A-USC) power plants, i.e., steam operation conditions up to 760°C (1400°F)/35 MPa (5000 psi), require the use of Ni-based alloys with high temperature performance. Currently, the U.S. Department of Energy Fossil Energy...
Proceedings Papers

AM-EPRI2016, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Eighth International Conference, 1010-1017, October 11–14, 2016,
.... advanced ultra-supercritical fossil fuel power plants aging chemical composition creep rupture time creep testing G115 steel mechanical properties microstructure oxidation resistance strengthening Advances in Materials Technology for Fossil Power Plants Proceedings from the Eighth International...
Proceedings Papers

AM-EPRI2019, 2019 Joint EPRI – 123HiMAT International Conference on Advances in High-Temperature Materials, 217-226, October 21–24, 2019,
... Abstract 9-10%Cr-3%Co martensitic steels are the prospective materials for elements of boilers, tubes and pipes for fossil power plants which are able to work at ultra-supercritical parameters of steam (T=620-650°C, P=25-30 MPa). The effect of creep on the microstructure of the 10 wt.%Cr-3Co...
Proceedings Papers

AM-EPRI2016, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Eighth International Conference, 1-11, October 11–14, 2016,
... advanced ultra-supercritical (A-USC) coal-fired power plants to be operated at steam temperatures up to 760°C, a United States-based consortium has started on a project to build an A-USC component test facility, (A-USC ComTest). Among the goals of the facility are to validate that components made from...
Proceedings Papers

AM-EPRI2010, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Sixth International Conference, 53-64, August 31–September 3, 2010,
... future coal power plants. advanced ultra-supercritical pulverized coal power plants CO 2 capture CO 2 emission CO 2 storage economic analysis power plant design Advances in Materials Technology for Fossil Power Plants Proceedings from the Sixth International Conference August 31...
Proceedings Papers

AM-EPRI2013, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Seventh International Conference, 1182-1189, October 22–25, 2013,
... Abstract Addressing the growing concern of supercritical and ultra-supercritical boilers as potential safety hazards in power plants, a new Boiler Risk Management and Life Prediction System (BRMLPS) has been developed. This system leverages risk-based inspection and assessment techniques...
Proceedings Papers

AM-EPRI2013, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Seventh International Conference, 86-97, October 22–25, 2013,
...) is a goal of the U.S. Program on Materials Technology for Ultrasupercritical Coal-Fired Boilers sponsored by the United States (U.S.) Department of Energy and the Ohio Coal Development Office (OCDO). As part of the development of advanced ultra-supercritical power plants in this program and internally...
Proceedings Papers

AM-EPRI2016, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Eighth International Conference, 190-201, October 11–14, 2016,
... superalloy GH750 to be used as the candidate boiler tube materials of A-USC power plants in the future. boiler tube fabrication chemical composition microstructure nickel-based superalloys process performance stress rupture strength tensile properties thermal stability ultra-supercritical power...
Proceedings Papers

AM-EPRI2019, 2019 Joint EPRI – 123HiMAT International Conference on Advances in High-Temperature Materials, 1060-1068, October 21–24, 2019,
... on Advance in Materials Technology for Fossil Power Plants, Waikoloa, Hawaii, October 22-25, 2013, pp. 491-503. [8] Patel, S. J., Introduction to Inconel Alloy 740H: An Alloy Designed for Superheater Tubing in Coal-Fired Ultra Supercritical Boilers, Acta Metallurgical Sinica, Vol. 18, No. 4 (2005), pp. 479...
Proceedings Papers

AM-EPRI2007, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Fifth International Conference, 1-15, October 3–5, 2007,
... International Conference on Advances in Materials Technology for Fossil Power Plants, Hilton Head Island, SC, October 2004, ASM International, in press. [5] G. Booras, Task 1 C, Economic Analysis , Boiler Materials for Ultra-supercritical Coal Power Plants, DOE Grant DE-FG26-01NT41175, OCDO Grant D-00-20...