Skip Nav Destination
Close Modal
Search Results for
post-weld heat treatment
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Article Type
Volume Subject Area
Date
Availability
1-20 of 179
Search Results for post-weld heat treatment
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Proceedings Papers
AM-EPRI2019, 2019 Joint EPRI – 123HiMAT International Conference on Advances in High-Temperature Materials, 123-134, October 21–24, 2019,
... into the market. All CSEF steels require an accurate post-weld heat treatment after welding. This paper discusses the impact of chemical composition on Ac1 as well as the transformation behavior during post-weld heat treatment in a temperature range below and above Ac1. The Ac1 temperature of weld metals...
Abstract
View Papertitled, Transformation Behavior of <span class="search-highlight">Weld</span> Metal for CSEF Steels during Intercritical <span class="search-highlight">Post</span>-<span class="search-highlight">weld</span> <span class="search-highlight">Heat</span> <span class="search-highlight">Treatment</span> and the Impact on Mechanical Properties
View
PDF
for content titled, Transformation Behavior of <span class="search-highlight">Weld</span> Metal for CSEF Steels during Intercritical <span class="search-highlight">Post</span>-<span class="search-highlight">weld</span> <span class="search-highlight">Heat</span> <span class="search-highlight">Treatment</span> and the Impact on Mechanical Properties
Creep strength enhanced ferritic steels like T/P 91 and T/P 92 are widely used for the fabrication of pressure vessel components in the petro-chemical and thermal power industry. Today, a new generation of 9-12% Cr CSEF steels like MARBN, Save12AD, G115 and Super VM12 are entering into the market. All CSEF steels require an accurate post-weld heat treatment after welding. This paper discusses the impact of chemical composition on Ac1 as well as the transformation behavior during post-weld heat treatment in a temperature range below and above Ac1. The Ac1 temperature of weld metals with variations in chemical composition has been determined and thermodynamic calculations has been carried out. Simulations of heat treatment cycles with variations in temperature have been carried out in a quenching dilatometer. The dilatation curves have been analyzed in order to detect any phase transformation during heating or holding at post weld heat treatment. Creep rupture tests have been carried out on P91 and Super VM12 type weld metals in order to investigate the effect of sub- and intercritical post weld heat treatment on creep rupture strength.
Proceedings Papers
AM-EPRI2013, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Seventh International Conference, 615-626, October 22–25, 2013,
... to achieve sufficient toughness in the weld. To relieve the internal stress in the welds and to stabilise their microstructures, a post weld heat treatment (PWHT) is commonly applied. The heat treatment conditions used for the PWHT have a significant effect on both the resulting microstructure and the creep...
Abstract
View Papertitled, The Effect of <span class="search-highlight">Post</span> <span class="search-highlight">Weld</span> <span class="search-highlight">Heat</span> <span class="search-highlight">Treatment</span> on the Creep Behaviour and Microstructural Evolution in Grade 92 Steel <span class="search-highlight">Welds</span> for Steam Pipe Applications
View
PDF
for content titled, The Effect of <span class="search-highlight">Post</span> <span class="search-highlight">Weld</span> <span class="search-highlight">Heat</span> <span class="search-highlight">Treatment</span> on the Creep Behaviour and Microstructural Evolution in Grade 92 Steel <span class="search-highlight">Welds</span> for Steam Pipe Applications
Grade 92 steel has been widely applied in the power generation industry for use as steam pipes, headers, tubes, etc. owing to a good combination of creep and corrosion resistance. For the welding of thick section pipes, a multi-pass submerged arc welding process is typically used to achieve sufficient toughness in the weld. To relieve the internal stress in the welds and to stabilise their microstructures, a post weld heat treatment (PWHT) is commonly applied. The heat treatment conditions used for the PWHT have a significant effect on both the resulting microstructure and the creep behaviour of the welds. In this study, interrupted creep tests were carried out on two identical Grade 92 welds that had been given PWHTs at two different temperatures: 732°C and 760°C. It was found that the weld with the lower PWHT temperature had a significantly reduced stain rate during the creep test. In addition, microstructural examination of the welds revealed that the primary location of creep damage was in the heat affected zone in the sample with the lower PWHT temperature, whereas it was in the weld metal in the sample with the higher PWHT temperature. To understand the effect of the different PWHT temperatures on the microstructure, initially the microstructures in the head portions of the two creep test bars were compared. This comparison was performed quantitatively using a range of electron/ion microscopy based techniques. It was apparent that in the sample subjected to the higher PWHT temperature, larger Laves phase particles occurred and increased matrix recovery was observed compared with the sample subjected to the lower PWHT temperature.
Proceedings Papers
AM-EPRI2010, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Sixth International Conference, 787-799, August 31–September 3, 2010,
.... This research examines the effects of simulated post weld heat treatments (PWHT) on Grade 91 and 92 materials using dilatometer-controlled heating and cooling rates, with peak temperatures below Ac 1 , between Ac 1 and Ac 3 , and above Ac 3 , followed by heat treatment at 750°C for 2 hours. Hardness...
Abstract
View Papertitled, The Effect of Simulated <span class="search-highlight">Post</span> <span class="search-highlight">Weld</span> <span class="search-highlight">Heat</span> <span class="search-highlight">Treatment</span> Temperature Overshoot on Microstructural Evolution in P91 and P92 Power Plant Steels
View
PDF
for content titled, The Effect of Simulated <span class="search-highlight">Post</span> <span class="search-highlight">Weld</span> <span class="search-highlight">Heat</span> <span class="search-highlight">Treatment</span> Temperature Overshoot on Microstructural Evolution in P91 and P92 Power Plant Steels
Creep strength enhanced ferritic (CSEF) steels, particularly modified 9Cr steels Grade 91 and 92, are increasingly used in advanced coal-fired power plants for header and steam piping construction. While these materials typically enter service after receiving a standard high-temperature normalizing treatment followed by lower temperature tempering to achieve optimal microstructure, practical situations like welding operations may expose components to additional heat treatment exceeding the Ac 1 , and potentially the Ac 3 , temperature before returning to tempering temperature. This research examines the effects of simulated post weld heat treatments (PWHT) on Grade 91 and 92 materials using dilatometer-controlled heating and cooling rates, with peak temperatures below Ac 1 , between Ac 1 and Ac 3 , and above Ac 3 , followed by heat treatment at 750°C for 2 hours. Hardness measurements revealed significant reduction when exceeding the Ac 1 temperature, while advanced electron microscopy, including electron back scatter diffraction, was employed to analyze changes in martensite laths and grain structure, along with detailed carbide size distribution analysis using both scanning and transmission electron microscopy. The findings are discussed in terms of how such PWHT overshoots might affect mechanical properties during high-temperature service.
Proceedings Papers
AM-EPRI2024, Advances in Materials, Manufacturing, and Repair for Power Plants: Proceedings from the Tenth International Conference, 1195-1206, February 25–28, 2025,
...., HAZ of parent, fusion-line, and weld metal). The only variables that contribute to this observed behavior are the post weld heat treatment (PWHT) cycle and the applied stress (all tests performed at 650 °C). In this work detailed microstructural analysis was undertaken to precisely define...
Abstract
View Papertitled, The Effect of <span class="search-highlight">Post</span> <span class="search-highlight">Weld</span> <span class="search-highlight">Heat</span> <span class="search-highlight">Treatment</span> on the Microstructure and Creep Damage Susceptibility in Grade 92 Steel
View
PDF
for content titled, The Effect of <span class="search-highlight">Post</span> <span class="search-highlight">Weld</span> <span class="search-highlight">Heat</span> <span class="search-highlight">Treatment</span> on the Microstructure and Creep Damage Susceptibility in Grade 92 Steel
Creep strength enhanced ferritic (CSEF) steels have shown the potential for creep failure in the weld metal, heat affected zone (HAZ) or fusion line. Details for this behavior have been frequently linked to metallurgical risk factors present in each of these locations which may drive the evolution of damage and subsequent failure. This work is focused on three weld samples fabricated from a commercially sourced Grade 92 steel pipe section. These weld samples were extracted from the same welded section but were reported to exhibit failure in different time frames and failure locations (i.e., HAZ of parent, fusion-line, and weld metal). The only variables that contribute to this observed behavior are the post weld heat treatment (PWHT) cycle and the applied stress (all tests performed at 650 °C). In this work detailed microstructural analysis was undertaken to precisely define the locations of creep damage accumulation and relate them to microstructural features. As part of this an automated inclusion mapping process was developed to quantify the characteristics of the BN particles and other inclusions in the parent material of the samples. It was found that BN particles were only found in the sample that had been subjected to the subcritical PWHT, not those that had received a re-normalizing heat treatment. Such micron sized inclusions are a known potential nucleation site for creep cavities, and this is consistent with the observed failure location in the HAZ of the parent in the sample where these were present. In the absence of BN inclusions, the next most susceptible region to creep cavitation is the weld metal. This has an intrinsically high density of sub-micron sized spherical weld inclusions and this is where most of the creep damage was located, in all the renormalized samples.
Proceedings Papers
AM-EPRI2016, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Eighth International Conference, 1001-1009, October 11–14, 2016,
... 6.3 mm) should be enabled without preheating and post weld heat treatment (PWHT) due to the lower carbon content below 0.1%. High creep rupture strength (CRS) values are achieved by Ti, N and B elements alloyed to T24 steel. The original expectation that the welding small thickness without preheating...
Abstract
View Papertitled, Secondary Hardening of T24 Steel <span class="search-highlight">Weld</span> Joints Performed at Incorrect Interpass Temperature and Low Temperature <span class="search-highlight">Heat</span> <span class="search-highlight">Treatment</span>
View
PDF
for content titled, Secondary Hardening of T24 Steel <span class="search-highlight">Weld</span> Joints Performed at Incorrect Interpass Temperature and Low Temperature <span class="search-highlight">Heat</span> <span class="search-highlight">Treatment</span>
The efficiency of power plants is depending on the steam temperature and/or the steam pressure. Efficiency increasing from 35% to 42-45% require increasing of the steam temperature over 600°C and the pressure over 26 MPa. According to the designer opinion it is not profitable to use classical low alloy creep resistant steels 16Mo3, 13CrMo4-5 or 10CrMo9-10 for membrane waterwall construction for these service condition. New modified low alloy creep resistance T23 and T24 (7CrMoVTiB10-10) steels were developed for membrane waterwalls. Welding of these steels with small thickness (around 6.3 mm) should be enabled without preheating and post weld heat treatment (PWHT) due to the lower carbon content below 0.1%. High creep rupture strength (CRS) values are achieved by Ti, N and B elements alloyed to T24 steel. The original expectation that the welding small thickness without preheating was early overcome and was wrong. According to the present experience the T24 steel is welded with preheating at 150-250°C depending on the wall thickness and welded joint toughness in order to achieve required hardness and impact toughness values. Opinions on the T24 welded joints post weld heat treatment (PWHT) requirements are still inconsistent. Especially the membrane waterwalls of the supercritical power plants are still produced without PWHT.
Proceedings Papers
AM-EPRI2016, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Eighth International Conference, 1182-1193, October 11–14, 2016,
... grades. A key component for successful welds is optimised post weld heat treatment (PWHT). Under certain conditions premature failures of welds can occur when incorrect weld and heat treatment performance result in a reduction of specified mechanical properties and high temperature creep performance...
Abstract
View Papertitled, Investigating Effects of Variations in <span class="search-highlight">Heat</span> <span class="search-highlight">Treatment</span> Parameters on Performance of CSEF <span class="search-highlight">Welds</span>
View
PDF
for content titled, Investigating Effects of Variations in <span class="search-highlight">Heat</span> <span class="search-highlight">Treatment</span> Parameters on Performance of CSEF <span class="search-highlight">Welds</span>
There is a constant need for improved knowledge of the influence of non-standard processing on the expected performance of creep strength enhanced ferritic (CSEF) materials as the total installed tonnage of these materials is rapidly increasing across the power generation industry. Cr-Mo-V steel grades micro-alloyed with niobium and titanium designed for pressurized equipment operating in the supercritical steam range proved to be very sensitive to relative minor variations in the principal heat treatment parameters time and temperature, when compared to the traditional Cr-Mo-V grades. A key component for successful welds is optimised post weld heat treatment (PWHT). Under certain conditions premature failures of welds can occur when incorrect weld and heat treatment performance result in a reduction of specified mechanical properties and high temperature creep performance, it is therefore of significant importance to have a good understanding of actual material properties for effective operation and plant life studies. This study investigated the effect and impact variations of post weld heat treatment time and temperature on mechanical properties of tungsten inert gas (TIG) and manual metal arc (MMA) welds on Grade 91 pipes from a set of reference samples. This is in preparation of establishing a benchmark set of tests to determine the integrity and expected long-term performance of butt-welds from limited site sample volumes, providing a non-intrusive methodology to identify welds suspected to have received non-standard PWHT cycles on Grade 91 pipework systems.
Proceedings Papers
AM-EPRI2013, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Seventh International Conference, 973-981, October 22–25, 2013,
.... Selection of weld metals to match, under match or overmatch base material as well as direct and indirect consequences on the heat-affected zone also require evaluation. Application of post weld heat treatment and ramifications where dissimilar base materials are involved are discussed plus the necessity...
Abstract
View Papertitled, Qualifying <span class="search-highlight">Welding</span> Procedures for Repair of High Temperature Components
View
PDF
for content titled, Qualifying <span class="search-highlight">Welding</span> Procedures for Repair of High Temperature Components
Qualifying welding procedures for repair of components in high temperature service requires careful consideration of factors including identification of the materials involved, existing mechanical properties and service operating parameters such as temperature, pressure and environment. Selection of weld metals to match, under match or overmatch base material as well as direct and indirect consequences on the heat-affected zone also require evaluation. Application of post weld heat treatment and ramifications where dissimilar base materials are involved are discussed plus the necessity of conducting tests at the operating temperatures and conditions where information is not available from the literature. Each of these factors is discussed and examples provided.
Proceedings Papers
AM-EPRI2024, Advances in Materials, Manufacturing, and Repair for Power Plants: Proceedings from the Tenth International Conference, 409-417, February 25–28, 2025,
... plants cannot afford long downtimes, making on-site service essential. This paper presents an on-site technique for post-weld heat treatment (PWHT) of Stellite seats. By using a heating pad arrangement and an induction heater, the required PWHT temperature of 740°C, as specified in the welding...
Abstract
View Papertitled, Effect of Induction Coil Configuration for Localized Postweld <span class="search-highlight">Heat</span> <span class="search-highlight">Treatment</span> of 9% Cr Steel Control Valves
View
PDF
for content titled, Effect of Induction Coil Configuration for Localized Postweld <span class="search-highlight">Heat</span> <span class="search-highlight">Treatment</span> of 9% Cr Steel Control Valves
Main steam control valves are crucial components in power plants, as they are the final elements in the steam piping system before the steam enters the turbine. If any parts of these valves become damaged, they can severely harm the steam turbines. Recently, power plants have been required to operate under cyclical loading, which increases the risk of cracks in the control valve seats. This is due to the different rates of expansion between the Stellite surface and the underlying Grade 91 steel surface when exposed to high temperatures. To ensure a reliable power supply, power plants cannot afford long downtimes, making on-site service essential. This paper presents an on-site technique for post-weld heat treatment (PWHT) of Stellite seats. By using a heating pad arrangement and an induction heater, the required PWHT temperature of 740°C, as specified in the welding specification procedure (WPS), can be achieved. This method allows for on-site valve seat repair and can be applied to other power plants as well.
Proceedings Papers
AM-EPRI2007, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Fifth International Conference, 129-139, October 3–5, 2007,
... content and the Vickers hardness value in HAZ is less than 350Hv to allow the application without preheating and post weld heat treatment. The HCMA tube materials were prepared in commercial tube mills. It has been demonstrated that the allowable stress of the HCMA steel tube is 1.3 times higher than...
Abstract
View Papertitled, Development of High Strength HCMA (1.25Cr-0.4Mo-Nb-V) Steel Tube
View
PDF
for content titled, Development of High Strength HCMA (1.25Cr-0.4Mo-Nb-V) Steel Tube
Improvement of thermal efficiency of new power plants by increasing temperature and pressure of boilers has led us to the development of high creep strength steels in the last 10 years. HCMA is the new steel with base composition of 1.25Cr-0.4Mo-Nb-V-Nd, which has been developed by examining the effects of alloying elements on microstructures, creep strength, weldability, and ductility. The microstructure of the HCMA is controlled to tempered bainite with low carbon content and the Vickers hardness value in HAZ is less than 350Hv to allow the application without preheating and post weld heat treatment. The HCMA tube materials were prepared in commercial tube mills. It has been demonstrated that the allowable stress of the HCMA steel tube is 1.3 times higher than those of conventional 1%Cr boiler tubing steels in the temperatures range of 430 to 530°C. It is noted that creep ductility has been drastically improved by the suitable amount of Nd (Neodymium)-bearing. The steam oxidation resistance and hot corrosion resistance of the HCMA have been proved to be the same level of the conventional 1%Cr and 2%Cr steels. It is concluded that the HCMA has a practical capability to be used for steam generator tubing from the aspect of good fabricability and very high strength. This paper deals with the concept of material design and results on industrial products.
Proceedings Papers
AM-EPRI2019, 2019 Joint EPRI – 123HiMAT International Conference on Advances in High-Temperature Materials, 1123-1131, October 21–24, 2019,
... investigated within these projects. In order to reduce the welding residual stresses in thick-walled components a post weld heat treatment (PWHT) for Alloy 617B is recommended after welding. This PHWT reduces not only residual stresses but causes changes in the damage mechanisms and failure behavior of welded...
Abstract
View Papertitled, Creep and Failure Behavior of <span class="search-highlight">Welded</span> Joints Made of Alloy 617B
View
PDF
for content titled, Creep and Failure Behavior of <span class="search-highlight">Welded</span> Joints Made of Alloy 617B
Welded joints of Ni-base alloys are often the critical part of components operated under high temperature service conditions. Especially welds in thick-walled structures are susceptible to various crack phenomena. Creep rupture and deformation behavior of different similar welds of Alloy 617B, both circumferential and longitudinal, were determined in many research German projects with the aim to qualify the nickel alloys and its welded joints for the use in highly efficient Advanced Ultra Supercritical (AUSC) power plants. Damage mechanisms and failure behavior have also been investigated within these projects. In order to reduce the welding residual stresses in thick-walled components a post weld heat treatment (PWHT) for Alloy 617B is recommended after welding. This PHWT reduces not only residual stresses but causes changes in the damage mechanisms and failure behavior of welded joints of Alloy 617B. Improving effects of PWHT have been investigated in this study and results of microstructural investigations were correlated with the material behavior.
Proceedings Papers
AM-EPRI2013, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Seventh International Conference, 1016-1024, October 22–25, 2013,
... kinetics in the heat affected zone, it was hypothesized that M 23 C 6 carbides in the fine-grain heat-affected zone (FGHAZ) in the LTT sample were fully dissolved, resulting in re-precipitation of strengthening carbides during post weld heat treatment (PWHT). This was not the case in the HTT sample since...
Abstract
View Papertitled, Effect of Non-Standard <span class="search-highlight">Heat</span> <span class="search-highlight">Treatments</span> on Creep Performance of Creep-Strength Enhanced Ferritic (CSEF) Steel Weldments
View
PDF
for content titled, Effect of Non-Standard <span class="search-highlight">Heat</span> <span class="search-highlight">Treatments</span> on Creep Performance of Creep-Strength Enhanced Ferritic (CSEF) Steel Weldments
This paper summarizes recent efforts to improve creep performance in Grade 91 (Mod. 9Cr-1Mo, ASTM A387) steel weldments via non-standard heat treatments prior to welding. Such heat treatments offer a potential solution for minimizing Type IV failures in creep strength enhanced ferritic (CSEF) steels. A lower temperature tempering (LTT, 650°C) of the 9Cr steels prior to gas tungsten arc welding (GTAW) resulted in improved creep-rupture life at 650°C compared to the samples tempered at a standard condition (HTT, 760°C) before welding. From detailed characterization of precipitation kinetics in the heat affected zone, it was hypothesized that M 23 C 6 carbides in the fine-grain heat-affected zone (FGHAZ) in the LTT sample were fully dissolved, resulting in re-precipitation of strengthening carbides during post weld heat treatment (PWHT). This was not the case in the HTT sample since M 23 C 6 in the FGHAZ was only partially dissolved prior to welding, which caused coarsening of existing M 23 C 6 after PWHT and premature creep failure in the FGHAZ. However, it was also found that the LTT raised the ductile-brittle transition temperature above room temperature (RT). Two different thermo-mechanical treatments (TMTs); two-step tempering and aus-forging/aus-aging, of the modified 9Cr-1Mo steels were attempted, in order to control the balance between creep properties and RT ductility, through control of precipitation kinetics of the M 23 C 6 carbides and/or MX carbo-nitrides. The hardness map of the TMT samples after GTAW and PWHT were evaluated.
Proceedings Papers
AM-EPRI2019, 2019 Joint EPRI – 123HiMAT International Conference on Advances in High-Temperature Materials, 1069-1078, October 21–24, 2019,
... Abstract Nimonic 263 alloy was selected for gas turbine combustor transition piece due to its excellent high temperature mechanical performance. In present work, Nimonic 263 alloy plate with thickness of 5mm was welded using 263 filler metal by GTAW, then post weld heat treatment of 800℃/8h/air...
Abstract
View Papertitled, Study on GTAW <span class="search-highlight">Welded</span> Joint of Nimonic 263 Alloy after Aging at 750℃ for Gas Turbine Transition Pieces
View
PDF
for content titled, Study on GTAW <span class="search-highlight">Welded</span> Joint of Nimonic 263 Alloy after Aging at 750℃ for Gas Turbine Transition Pieces
Nimonic 263 alloy was selected for gas turbine combustor transition piece due to its excellent high temperature mechanical performance. In present work, Nimonic 263 alloy plate with thickness of 5mm was welded using 263 filler metal by GTAW, then post weld heat treatment of 800℃/8h/air cool was carried out. The hardness and impact toughness of welded joints were measured, and the microstructure evolution after aging at 750℃ for 3000h was investigated by scanning electron microscopy(SEM). The results show that, during the aging process, the hardness of weld metal increases firstly and then decreases. The impact toughness decreases significantly at first and then increase. Furthermore, some fluctuations can be detected in hardness and impact toughness after long-term thermal exposure. The significant decrease in the impact toughness of the aged welded joints mainly results from the precipitation of η phase around grain boundary and intergranular MC phase. The hardness of weld metal increases due to the precipitation of more carbides and γ′ phase after 1000h aging, then decreases owing to the growth of γ′ phase after 3000h aging.
Proceedings Papers
AM-EPRI2013, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Seventh International Conference, 276-280, October 22–25, 2013,
... be better from fabricating points. Whether re-solution for the bent tube is performed after bending depends on its bending radius, followed by welding and post weld heat treatment of component (this treatment can also be the aging treatment for annealed sector at the same time), this treating manner can...
Abstract
View Papertitled, Discussion of Delivered Condition Specified in ASME Code Case 2702 on Inconel 740H Used for A-USC Boiler
View
PDF
for content titled, Discussion of Delivered Condition Specified in ASME Code Case 2702 on Inconel 740H Used for A-USC Boiler
Delivered condition of Inconel740H specified in ASME Code Case 2702 is solution heat treated and aged condition, fabricating performances are also based on the condition, and a re-annealing and aging shall be performed if cold forming to strains is over 5%. These almost harsh requirements bring great inconvenience for its engineering practice and utilization. The comparative bending tests on 740H tubes in solution heat treated + aged condition and solution heat treated condition were performed, and the rules’ reasonability of the specification on delivered condition was discussed and analyzed from point view of deformability and weldability in the paper. The bending test results showed that tube bent was difficult because of its high strength and limited deforming capacity in solution heat treated + aged condition. Therefore, the material supplied in the solution condition may be better from fabricating points. Whether re-solution for the bent tube is performed after bending depends on its bending radius, followed by welding and post weld heat treatment of component (this treatment can also be the aging treatment for annealed sector at the same time), this treating manner can meet regulatory requirements. For solution tubes, however, there are some inconveniences to its engineering application because fewer research studies were carried out on its properties up to now, and no regulations on them were given for the material in the specification. Suggestions are: 1) deeply investigating the properties of tubes in solution condition, including mechanical and fabricating performances, 2) adding the mechanical properties, maximum allowable cold forming to stain without performing re-solution and weld strength reduction factor of solution material to the code case.
Proceedings Papers
AM-EPRI2016, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Eighth International Conference, 1075-1085, October 11–14, 2016,
... for such butt welds was initiated. According to the European standards butt welds of T24 boiler tubes with wall thickness < 10 mm (0.3937 in) do not require any post-weld heat treatment (PWHT) and no hardness limits are given. When looking at manufacturing related issues such as an imminent risk of cold...
Abstract
View Papertitled, Evaluation of Hardness Levels of T24 Boiler Tube Butt <span class="search-highlight">Welds</span> Regarding SCC Susceptibility in High Temperature Water
View
PDF
for content titled, Evaluation of Hardness Levels of T24 Boiler Tube Butt <span class="search-highlight">Welds</span> Regarding SCC Susceptibility in High Temperature Water
In Europe between 2006 and 2012 several ultra-super-critical (USC) coal-fired power plants were built employing T24 (7CrMoVTiB10-10 / DIN EN 10216-2:2014-03 / VdTÜV sheet 533/2) in membrane walls. During commissioning stress corrosion cracking (SCC) on the tube-to-tube butt welds appeared. The widespread damages required the development of a new patented commissioning procedure to avoid recurring damages. Although this commissioning procedure was employed successfully and the power plants are in operation since then, a debate about the implementation of a hardness limit for such butt welds was initiated. According to the European standards butt welds of T24 boiler tubes with wall thickness < 10 mm (0.3937 in) do not require any post-weld heat treatment (PWHT) and no hardness limits are given. When looking at manufacturing related issues such as an imminent risk of cold cracking after welding of micro-alloyed steels a widely applied but coarse hardness limit is 350 HV. Based on laboratory tests, some authors reallocated this 350 HV hardness limit for addressing SCC susceptibility of low-alloyed steels. This article describes typical hardness levels of T24 boiler tube TIG butt welds and the SCC behavior in high temperature water. Further the effect of the stress relief heat treatment (SRHT) of the boiler membrane walls between 450 °C and 550 °C (842 °F and 1022 °F) on its hardness values and on the SCC behavior is discussed, showing that the hardness values should not be used as an indicator for SCC susceptibility of T24 boiler tube butt welds.
Proceedings Papers
AM-EPRI2024, Advances in Materials, Manufacturing, and Repair for Power Plants: Proceedings from the Tenth International Conference, 1249-1256, February 25–28, 2025,
... Abstract A compositional modification has been proposed to validate an alloy design which potentially eliminates the requirement of post-weld heat treatment (PWHT) while preserving the advantage of mechanical properties in a reduced activation bainitic ferritic steel based on Fe-3Cr-3W-0.2V...
Abstract
View Papertitled, Development of PWHT-Free, Reduced Activation Creep-Strength Enhanced Bainitic Ferritic Steel for Large-Scale Fusion Reactor Components
View
PDF
for content titled, Development of PWHT-Free, Reduced Activation Creep-Strength Enhanced Bainitic Ferritic Steel for Large-Scale Fusion Reactor Components
A compositional modification has been proposed to validate an alloy design which potentially eliminates the requirement of post-weld heat treatment (PWHT) while preserving the advantage of mechanical properties in a reduced activation bainitic ferritic steel based on Fe-3Cr-3W-0.2V- 0.1Ta-Mn-Si-C, in weight percent, developed at Oak Ridge National Laboratory in 2007. The alloy design includes reducing the hardness in the as-welded condition for improving toughness, while increasing the hardenability for preserving the high-temperature mechanical performance such as creep-rupture resistance in the original steel. To achieve such a design, a composition range with a reduced C content combining with an increased Mn content has been proposed and investigated. Newly proposed “modified” steel successfully achieved an improved impact toughness in the as- welded condition, while the creep-rupture performance across the weldments without PWHT demonstrated ~50% improvement of the creep strength compared to that of the original steel weldment after PWHT. The obtained results strongly support the validity of the proposed alloy design.
Proceedings Papers
AM-EPRI2024, Advances in Materials, Manufacturing, and Repair for Power Plants: Proceedings from the Tenth International Conference, 735-749, February 25–28, 2025,
... comprehensive properties of the AM-built weld metal after post-weld heat treatment (PWHT), examines factors influencing deposit quality and performance, and explores the practical benefits for procurement and field construction, supported by in-service data and application cases. chromium-molybdenum steel...
Abstract
View Papertitled, <span class="search-highlight">Weld</span> Metal Additive Manufacturing for Grade 91
View
PDF
for content titled, <span class="search-highlight">Weld</span> Metal Additive Manufacturing for Grade 91
This study investigates a novel approach to addressing the persistent Type IV cracking issue in Grade 91 steel weldments, which has remained problematic despite decades of service history and various mitigation attempts through chemical composition and procedural modifications. Rather than further attempting to prevent heat-affected zone (HAZ) softening, we propose eliminating the vulnerable base metal entirely by replacing critical sections with additively manufactured (AM) weld metal deposits using ASME SFA “B91” consumables. The approach employs weld metal designed for stress-relieved conditions rather than traditional normalizing and tempering treatments. Our findings demonstrate that the reheat cycles during AM buildup do not produce the substantial softening characteristic of Type IV zones, thereby reducing the risk of premature creep failure. The study presents comprehensive properties of the AM-built weld metal after post-weld heat treatment (PWHT), examines factors influencing deposit quality and performance, and explores the practical benefits for procurement and field construction, supported by in-service data and application cases.
Proceedings Papers
AM-EPRI2019, 2019 Joint EPRI – 123HiMAT International Conference on Advances in High-Temperature Materials, 315-326, October 21–24, 2019,
... hardness martensitic stainless steel nondestructive evaluation post-weld heat treatment thick wall piping Joint EPRI 123HiMAT International Conference on Advances in High Temperature Materials October 21 24, 2019, Nagasaki, Japan J. Shingledecker, M. Takeyama, editors httpsdoi.org/10.31399...
Abstract
View Papertitled, The Development of Nondestructive Evaluation Coupons in Full Grade 91 Cross-<span class="search-highlight">welds</span> with Various Levels of Creep Damage
View
PDF
for content titled, The Development of Nondestructive Evaluation Coupons in Full Grade 91 Cross-<span class="search-highlight">welds</span> with Various Levels of Creep Damage
The global electric power production is largely dependent on the operation of fossil-fired generation units. Many coal-fired units are exceeding 300,000 hours, which is beyond the expected design life. This has caused a continuous need to inspect steam touched components operating at high temperature and pressure. State-of-the-art coal and combined cycle gas units are specifying ever-greater amounts of the Creep Strength Enhanced Ferritic (CSEF) steels such as Grade 91 or Grade 92. The martensitic 9%Cr CSEF steels were developed to provide greater strength than traditional low alloy power plant steels, such as Grades 11, 12 and 22. The enhanced strength allows for a reduction in overall wall thickness in new or replacement components. Extensive research in both service failures and laboratory testing has shown that time-dependent creep damage can develop differently in Grade 91 steel when compared to low alloy steels. Furthermore, the creep strength in Grade 91 can vary by more than a factor of 10 between different heats. This wide variation of creep strength has led to extensive research in understanding the damage mechanisms and progression of damage in this steel. In this study, large cross weld samples were fabricated from thick wall piping in Grade 91 steel using two different heats of material. One weld was fabricated in a ‘damage tolerant’ heat and another weld was fabricated in a ‘damage intolerant’ heat of material. The samples were subjected to a post-weld heat treatment (PWHT) at a temperature of 745°C (1375°F) for 1.50 hours. Hardness maps were collected on the cross-welds in the as-welded and PWHT condition for both weldments. Cross-weld creep test conditions were selected to develop accelerated damage representative of in-service behavior. The test samples were interrupted at multiple stages and nondestructively evaluated (NDE) with advanced phased-array ultrasonic techniques. Samples were developed to variable levels of damage (50% to 100% life fraction) in both weldments. Metallographic sections were extracted at specific locations to validate the NDE findings using light emitting diode, laser and scanning electron microscopy. This research is being used to help validate the level of damage that can be reliably detected using conventional and advanced NDE techniques.
Proceedings Papers
AM-EPRI2016, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Eighth International Conference, 951-961, October 11–14, 2016,
... and final passes. Cross-weld tensile tests, side bend tests and impact tests of weld metals and heat-affected zones were carried out at ambient temperatures after two post-weld heat treatments (PWHT), each at 730°C for 12 hours. Creep rupture tests of cross-weld samples were performed at 625°C. This study...
Abstract
View Papertitled, Creep Rupture Strength of Dissimilar CB2-P92 FCW Joint <span class="search-highlight">Welds</span>
View
PDF
for content titled, Creep Rupture Strength of Dissimilar CB2-P92 FCW Joint <span class="search-highlight">Welds</span>
As flux cored wires for gas metal arc welding offer several technical and economic advantages they are becoming more and more popular. Matching flux cored wires for welding P92 have already been available for several years. A matching flux cored wire for welding the Co-alloyed cast steel CB2, which is used for turbine and valve casings operating at steam temperatures of up to 620°C, was developed recently. To connect casings with P92 pipes, dissimilar welding of CB2 to P92 is necessary. This can be done with filler metal that matches either CB2 or P92. Pre-tests have confirmed that flux cored arc welding (FCAW) can generally be used for dissimilar joint welding of CB2 to P92. To evaluate creep rupture strength dissimilar welds were performed with filler metal matching CB2 and P92, respectively. TIG welding was used for the root and the second pass and FCAW for the intermediate and final passes. Cross-weld tensile tests, side bend tests and impact tests of weld metals and heat-affected zones were carried out at ambient temperatures after two post-weld heat treatments (PWHT), each at 730°C for 12 hours. Creep rupture tests of cross-weld samples were performed at 625°C. This study compares the results of the mechanical tests at ambient temperature and the creep rupture tests, and discusses why P92 filler metals are preferred for such welds.
Proceedings Papers
Effect of Reheated CGHAZ Microstructure on Hydrogen-Induced Cracking Susceptibility in SA-508 Steel
Free
AM-EPRI2024, Advances in Materials, Manufacturing, and Repair for Power Plants: Proceedings from the Tenth International Conference, 933-944, February 25–28, 2025,
.... The purpose of the 48 hr hold is to confirm the absence of hydrogen-induced cracking in the temper bead heat-affected zone. In previous research, the effect of post-weld heat treatment (PWHT) and temper bead welding (TBW) on the hydrogen-induced cracking (HIC) susceptibility in the coarse-grained heat...
Abstract
View Papertitled, Effect of Reheated CGHAZ Microstructure on Hydrogen-Induced Cracking Susceptibility in SA-508 Steel
View
PDF
for content titled, Effect of Reheated CGHAZ Microstructure on Hydrogen-Induced Cracking Susceptibility in SA-508 Steel
According to ASME Case N-888-3, Similar and Dissimilar Metal Welding Using Ambient Temperature SMAW or Machine GTAW Temper Bead Technique, a 48 hr waiting period before conducting the final nondestructive examination (NDE) is required when ferritic filler weld metal is used. The purpose of the 48 hr hold is to confirm the absence of hydrogen-induced cracking in the temper bead heat-affected zone. In previous research, the effect of post-weld heat treatment (PWHT) and temper bead welding (TBW) on the hydrogen-induced cracking (HIC) susceptibility in the coarse-grained heat-affected zone (CGHAZ) in welds of SA-508, P-No. 3 Group 3, pressure vessel steel was investigated using the Delayed Hydrogen Cracking Test (DHCT). In that previous study, the Gleeble thermomechanical simulator was used to generate six CGHAZ microstructural conditions: as-welded (AW), PWHT, and AW with single a TBW reheat at 675, 700, 725, and 735°C. Hydrogen was introduced to the specimen through cathodic charging under in situ constant tensile stress. The HIC susceptibility for these microstructures was ranked by the DHCT at a diffusible hydrogen level significantly exceeding typical GTAW and SMAW processes. The work described in this paper investigates the susceptibility to HIC of these same CGHAZ microstructures with DHCT at variable current densities, further ranking each condition. Test results were analyzed by fracture surface examination of failed tests, and cross-section microstructural analysis under a scanning electron microscope (SEM). Future steps include evaluating critical hydrogen content levels using gas chromatography for each condition. The results from this study will be used to consider potential elimination of the NDE hold time requirement in Case N-888-3 when ferritic weld metal is used.
Proceedings Papers
AM-EPRI2007, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Fifth International Conference, 818-829, October 3–5, 2007,
.... While derived from Nimonic alloy 263, alloy 740's unique chemistry necessitates comprehensive weldability studies to address potential challenges including heat-affected zone liquation cracking, ductility-dip cracking, and post-weld heat treatment cracking. This ongoing investigation examines...
Abstract
View Papertitled, Weldability Investigation of Inconel Alloy 740 for Ultrasupercritical Boiler Applications
View
PDF
for content titled, Weldability Investigation of Inconel Alloy 740 for Ultrasupercritical Boiler Applications
Inconel alloy 740, a precipitation-hardenable nickel-chromium-cobalt alloy with niobium addition, has emerged as a leading candidate material for ultra-supercritical (USC) boilers due to its superior stress rupture strength and corrosion resistance at operating temperatures near 760°C. While derived from Nimonic alloy 263, alloy 740's unique chemistry necessitates comprehensive weldability studies to address potential challenges including heat-affected zone liquation cracking, ductility-dip cracking, and post-weld heat treatment cracking. This ongoing investigation examines the alloy's weldability characteristics through material characterization studies comparing its cracking sensitivity to established aerospace alloys like Waspalloy and Inconel alloy 718. The research applies aerospace industry expertise to boiler applications requiring sections up to three inches thick, with gas tungsten arc welding and pulsed gas metal arc welding identified as the most promising processes for producing sound, crack-free welds.
1