Proceedings Papers

AM-EPRI2019, 2019 Joint EPRI – 123HiMAT International Conference on Advances in High-Temperature Materials, 348-359, October 21–24, 2019,
... 11,727 hours operation and 397 starts. This paper reports microstructural and oxidation analysis, that has been undertaken by Loughborough University as part of IMPULSE project, and outlines future work to be carried out. boiler tubing martensitic stainless steel MarBN steels microstructural...
Proceedings Papers

AM-EPRI2007, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Fifth International Conference, 366-376, October 3–5, 2007,
.... chromium steel creep resistance creep-rupture test ductility ladle furnace microstructural analysis vacuum degassing Advances in Materials Technology for Fossil Power Plants Proceedings from the Fifth International Conference R. Viswanathan, D. Gandy, K. Coleman, editors, p 366-376 Copyright ©...
Proceedings Papers

AM-EPRI2024, Advances in Materials, Manufacturing, and Repair for Power Plants: Proceedings from the Tenth International Conference, 507-516, February 25–28, 2025,
... Abstract The microstructure of MoSiBTiC alloys is very complex, with three to four constituent phases and characteristic structures such as fine precipitates and lamellar structures. To perform the microstructural analysis efficiently, image segmentation was first performed for each phase...
Proceedings Papers

AM-EPRI2019, 2019 Joint EPRI – 123HiMAT International Conference on Advances in High-Temperature Materials, 715-725, October 21–24, 2019,
... degradation. (4) There are no obvious corrosion elements in the oxide layers of the cracks. (5) Metallographic microstructure analysis shows that there are many intergranular cracks and carbides such as Cr-rich phase and Fe-Cr are precipitated at the grain boundaries, ultimately resulting in strain-induced...
Proceedings Papers

AM-EPRI2024, Advances in Materials, Manufacturing, and Repair for Power Plants: Proceedings from the Tenth International Conference, 1195-1206, February 25–28, 2025,
...., HAZ of parent, fusion-line, and weld metal). The only variables that contribute to this observed behavior are the post weld heat treatment (PWHT) cycle and the applied stress (all tests performed at 650 °C). In this work detailed microstructural analysis was undertaken to precisely define...
Proceedings Papers

AM-EPRI2024, Advances in Materials, Manufacturing, and Repair for Power Plants: Proceedings from the Tenth International Conference, 296-303, February 25–28, 2025,
... steam pipe within a heat recovery steam generator(HRSG) of J-class gas turbine, occurring in the P92 base material and repair welds. This pipe has been used at the power plant for about 10 years. Microstructural analysis of the cross-section indicated that the cracks were primarily due to thermal...
Proceedings Papers

AM-EPRI2013, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Seventh International Conference, 586-595, October 22–25, 2013,
... Abstract In order to study the effect of precipitation strengthening by MX precipitates on the restriction of microstructure degradation in 9 mass% Cr ferritic heat-resistant steels, V, Nb additioned model steels were evaluated by microstructure analysis through TEM and EBSD with reference...
Proceedings Papers

AM-EPRI2004, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Fourth International Conference, 1042-1063, October 25–28, 2004,
... of creep and damage kinetics, weldability, microstructure analysis during creep, modeling of precipitation and coarsening kinetics, and deformation behavior under creep loading. The individual projects are briefly described, outlining the conceptual approach towards quantitatively describing the creep...
Proceedings Papers

AM-EPRI2019, 2019 Joint EPRI – 123HiMAT International Conference on Advances in High-Temperature Materials, 1446-1456, October 21–24, 2019,
... to more than 1% as the volume fraction of γ phase increases to 80%. However, γ single phase alloys show very limited ductility of less than 0.2%. Microstructure analysis have revealed that intragranular fracture along γ/γ grain boundary occurred in γ single phase alloy whereas it does not along β/γ...
Proceedings Papers

AM-EPRI2024, Advances in Materials, Manufacturing, and Repair for Power Plants: Proceedings from the Tenth International Conference, 573-581, February 25–28, 2025,
... of the root. Thus, a special GMAW-Pulsed version was applied to achieve good wettability and defect-free joints. ASTM G48 tests were performed to evaluate the corrosion resistance through Critical Pitting Testing (CPT) analysis on the root pass, microstructural analysis via optical microscopy, and impact...
Proceedings Papers

AM-EPRI2007, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Fifth International Conference, 168-184, October 3–5, 2007,
... calculations and microstructural analysis revealed that the Laves phase in HR6W gradually decreases with increasing temperature, whereas the γ' phase in Alloy 617 rapidly diminishes and almost completely dissolves at 800°C, potentially causing an abrupt drop in creep strength above 750°C. After comprehensive...
Proceedings Papers

AM-EPRI2024, Advances in Materials, Manufacturing, and Repair for Power Plants: Proceedings from the Tenth International Conference, 933-944, February 25–28, 2025,
... metal is used. coarse-grained heat-affected zone delayed hydrogen cracking test fracture surface examination hydrogen-induced cracking susceptibility low alloy steel microstructural analysis microstructure nondestructive examination post-weld heat treatment pressure vessels temper bead...
Proceedings Papers

AM-EPRI2010, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Sixth International Conference, 140-152, August 31–September 3, 2010,
... in China during the past few years. This paper presents the evaluation results of S30432 tubes manufactured by four steel plants in China as well as Sumitomo super304H tubes for comparison. A detailed microstructural analysis of the tubes has been performed by using optical and electron microscope...
Proceedings Papers

AM-EPRI2024, Advances in Materials, Manufacturing, and Repair for Power Plants: Proceedings from the Tenth International Conference, 712-722, February 25–28, 2025,
... and the heat affected zone (HAZ). This was the apparent primary cause of the failure. However, chloride-induced SCC of such materials typically results in transgranular crack propagation, whereas the observed cracks were indicative of intergranular stress corrosion cracking (IGSCC). Microstructural analysis...
Proceedings Papers

AM-EPRI2004, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Fourth International Conference, 1198-1212, October 25–28, 2004,
... focused on specific specimen configurations for evaluating the high temperature behavior of weldments. Creep testing on INCONEL alloy 740 has shown good strengths (higher than 230 or CCA617) that may meet the target steam conditions. Microstructural analysis by electron microscopy on aged and tested...
Proceedings Papers

AM-EPRI2019, 2019 Joint EPRI – 123HiMAT International Conference on Advances in High-Temperature Materials, 1395-1401, October 21–24, 2019,
.... Conversely, Eγα 2 and FLγ displayed a slight acceleration and the longest rupture strain, albeit with the shortest rupture time compared to Eγ. Upon microstructural analysis of of the creep-test specimens, it was observed that numerous dynamic recrystallized grains (DXGs) and sub-grains formed along grain...
Proceedings Papers

AM-EPRI2013, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Seventh International Conference, 1151-1162, October 22–25, 2013,
... and effective when used for microstructural analysis purposes during R&D, manufacturing and operating processes. austenitic stainless steel boiler tubes electron probe X-ray microanalysis failure analysis martensitic stainless steel microstructural analysis nickel-base superalloys phase...
Proceedings Papers

AM-EPRI2024, Advances in Materials, Manufacturing, and Repair for Power Plants: Proceedings from the Tenth International Conference, 678-689, February 25–28, 2025,
... properties of the 45° orientation predictably fell between those of 0° and 90° orientations, creep behavior over 100-10,000 hours revealed unexpected results: the 45° orientation demonstrated significantly shorter rupture times and faster creep rates compared to other orientations. Microstructural analysis...
Proceedings Papers

AM-EPRI2004, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Fourth International Conference, 1213-1226, October 25–28, 2004,
... accident simulation heating tests were conducted to assess the integrity of P92 beyond 650°C (relevant for short-term creep) and compare it to stainless steel 1.4404 (potential building material). Finally, microstructural analysis was performed on tested samples, revealing that the martensitic structure...
Proceedings Papers

AM-EPRI2016, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Eighth International Conference, 832-843, October 11–14, 2016,
... and industrial practices that has long term implications on scale growth kinetics and morphological development. Microstructural analysis of both virgin and ex-service tubing reveals the presence of a pre-existing oxide structure that is incorporated into the inwardly growing scale and is implicated...