AM-EPRI2024, Advances in Materials, Manufacturing, and Repair for Power Plants: Proceedings from the Tenth International Conference, 1331-1337, October 15–18, 2024,
... Abstract A thorough understanding of interactions between graphite and fluoride fuel salts is crucial, as graphite is a promising candidate for the moderator of molten salt reactors. This study investigates the infiltration of fluoride fuel salts into graphite and the fluorination of graphite...