Proceedings Papers

AM-EPRI2016, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Eighth International Conference, 202-212, October 11–14, 2016,
... development efforts were focused on that microstructure. High temperature tensile test and creep test results indicated that the performance of the new alloys was competitive with NIMONIC 263. SEM and TEM microscopy were utilized to determine the deformation mechanisms during creep. advanced ultra...
Proceedings Papers

AM-EPRI2013, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Seventh International Conference, 1432-1440, October 22–25, 2013,
... captured a significant difference in the local creep deformation between two Grade 91 steel welds with different pre-welding conditions (standard and non-standard). Strain contour plots exhibited inhomogeneous deformation in the weldments, especially at the heat-affected zone (HAZ). Standard heat-treated...
Proceedings Papers

AM-EPRI2004, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Fourth International Conference, 1124-1135, October 25–28, 2004,
... Abstract Creep deformation behavior of the T122 type steels with different matrix phases such as α’ (martensite) and α’+δ (martensite and delta-ferrite) at different stress levels has been studied comparing with those of the model steels with the initial microstructures consisting...
Proceedings Papers

AM-EPRI2004, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Fourth International Conference, 1213-1226, October 25–28, 2004,
... Abstract This study examines the deformation behavior of P92 steel (ferritic, 9% Cr) at high temperatures (600°C to 900°C) using isothermal hot tensile tests. Particular focus is placed on the stress-strain behavior around its alpha-gamma transition temperature (825°C). Additionally, fire...
Proceedings Papers

AM-EPRI2004, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Fourth International Conference, 1229-1241, October 25–28, 2004,
... suppresses coarsening of these carbides during creep deformation, leading to excellent microstructural stability and creep strength. Further improvement of creep strength is achieved by the addition of appropriate amount of nitrogen which enhances precipitation of fine MX. Excess addition of nitrogen...
Proceedings Papers

AM-EPRI2010, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Sixth International Conference, 620-639, August 31–September 3, 2010,
... resistance and long-term creep rupture strength, particularly in welded joints where resistance to Type IV cracking is critical for constructing thick-section boiler components. The current research aims to investigate the creep deformation behavior and microstructure evolution during creep for base metals...
Proceedings Papers

AM-EPRI2019, 2019 Joint EPRI – 123HiMAT International Conference on Advances in High-Temperature Materials, 360-369, October 21–24, 2019,
... Abstract This work deals with the potential of microstructurally based modeling of the creep deformation of martensitic steels. The motivation for the work stems from the ever increasing demand for higher efficiency and better reliability of modern thermal power plants. Service temperatures...
Proceedings Papers

AM-EPRI2019, 2019 Joint EPRI – 123HiMAT International Conference on Advances in High-Temperature Materials, 570-579, October 21–24, 2019,
... material was degraded, the resistance against crack propagation was reduced, while in the region where stress was relaxed, the crack driving force was lowered. creep deformation crystal nickel-base superalloys fatigue crack propagation gas turbines material degradation Joint EPRI 123HiMAT...
Proceedings Papers

AM-EPRI2019, 2019 Joint EPRI – 123HiMAT International Conference on Advances in High-Temperature Materials, 914-923, October 21–24, 2019,
... properties depended on the microstructure of the alloys. aging boron creep deformation creep properties creep test microstructure near-alpha-titanium alloys solution treatment Joint EPRI 123HiMAT International Conference on Advances in High Temperature Materials October 21 24, 2019...
Proceedings Papers

AM-EPRI2019, 2019 Joint EPRI – 123HiMAT International Conference on Advances in High-Temperature Materials, 1380-1388, October 21–24, 2019,
... Abstract Tensile deformation behavior of γ-TiAl based alloys consisting of α 2 -Ti 3 Al/γ lamellar colonies, β-Ti grains, and γ grains were investigated by in-situ scanning electron microscopy and digital image correlation technique, in order to identify the role of each microstructure...
Proceedings Papers

AM-EPRI2024, Advances in Materials, Manufacturing, and Repair for Power Plants: Proceedings from the Tenth International Conference, 99-110, February 25–28, 2025,
... while accounting for both stress and temperature effects. The model was implemented using a polycrystalline microstructure simulation framework based on elasto-viscoplastic Fast Fourier Transform (EVPFFT). It incorporates three key deformation mechanisms: thermally activated dislocation glide...
Proceedings Papers

AM-EPRI2024, Advances in Materials, Manufacturing, and Repair for Power Plants: Proceedings from the Tenth International Conference, 678-689, February 25–28, 2025,
... revealed distinct creep deformation mechanisms active within different build orientations, with the accelerated creep rate in 45° specimens attributed to multiple phenomena, particularly η-phase formation and twinning. These findings provide crucial insights into the orientation-dependent creep behavior...
Proceedings Papers

AM-EPRI2024, Advances in Materials, Manufacturing, and Repair for Power Plants: Proceedings from the Tenth International Conference, 1289-1299, February 25–28, 2025,
... Abstract Creep deformation and rupture properties of several long-term used Super 304H steel boiler tubes were presented in this paper. The aged superheater tubes that have been in service for about 140,000 hours at the approximate metal temperature ranged from 550°C to 640°C, were investigated...
Proceedings Papers

AM-EPRI2004, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Fourth International Conference, 1299-1312, October 25–28, 2004,
... Abstract The microstructures of two 9% chromium steels, P92 (30 ppm B) and B2 (100 ppm B), after heat treatment and after long-term creep deformation at 600°C were quantitatively investigated by means of transmission electron microscopy and boron trace autoradiography. The aim of the study...
Proceedings Papers

AM-EPRI2019, 2019 Joint EPRI – 123HiMAT International Conference on Advances in High-Temperature Materials, 470-478, October 21–24, 2019,
... tensile tests were conducted on CW and P/M processed alloy720Li in order to reveal the effect of temperature and strain rate on deformation behavior and to demonstrate the effect of microstructure derived from P/M process on deformability. The fracture mode of the P/M material changed from grain interior...
Proceedings Papers

AM-EPRI2004, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Fourth International Conference, 773-787, October 25–28, 2004,
... specimen testing reports on low-temperature behavior. However, cross-weld local material data at high service temperatures have not been reported yet. In the present study, MT tests are conducted across similar P22 and P91 steel welds at 550°C and 600°C, respectively. To study deformation mechanisms...
Proceedings Papers

AM-EPRI2019, 2019 Joint EPRI – 123HiMAT International Conference on Advances in High-Temperature Materials, 523-534, October 21–24, 2019,
... an alternative, more economical, 1-step aging treatment and compared microstructure, tensile properties at 750˚C and deformation behavior. Moreover, three cooling rates from the solution temperature were studied to simulate large-scale components conditions. We found that as much as about 20% of fine spherical...
Proceedings Papers

AM-EPRI2013, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Seventh International Conference, 1292-1303, October 22–25, 2013,
... to 10 mass% resulted in the creep life extension. However, the Cr content higher than 11 mass% decreased the creep life. In 9 mass% Cr-containing steel, the increase in W content decreased the creep deformation rate with creep time. However, it also shortened the time to reach the minimum creep rate...
Proceedings Papers

AM-EPRI2019, 2019 Joint EPRI – 123HiMAT International Conference on Advances in High-Temperature Materials, 1429-1435, October 21–24, 2019,
... stage, both show similar behavior with rupture time of about 50 h and rupture elongation of 60 %. At the low stress, on the other hand, reverse behavior occurs, that is, W α 2 shows creep rate higher than Nγ in transient stage. The regions near grain boundaries progressively deformed for both specimens...
Proceedings Papers

AM-EPRI2024, Advances in Materials, Manufacturing, and Repair for Power Plants: Proceedings from the Tenth International Conference, 1320-1330, February 25–28, 2025,
...) technique, the highly gradient creep properties across the HAZ of Grade 91 steel was quantitatively measured. A physical creep cavitation constitutive model was proposed to investigate the local creep deformation and damage accumulation within the heterogeneous HAZ, which takes into account the nucleation...