AM-EPRI2019, 2019 Joint EPRI – 123HiMAT International Conference on Advances in High-Temperature Materials, 655-664, October 21–24, 2019,
... Abstract 18Cr-9Ni-3Cu-Nb-N steel is widely used for heat exchanger tubes such as super-heaters and reheaters of ultra-super critical power generation boilers. In this study, long-term creep rupture tests were carried out on 18Cr-9Ni-3Cu-Nb-N seamless steel tubes of 7 heat materials...
Proceedings Papers

AM-EPRI2013, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Seventh International Conference, 1047-1058, October 22–25, 2013,
... impact test. To select the annealing conditions for stress relief, stress relaxation tests and hardness tests were conducted on the weld joints after various heat treatments. The microstructure was also evaluated by SEM and TEM. Creep rupture tests are being performed for the weld joints with and without...
Proceedings Papers

AM-EPRI2013, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Seventh International Conference, 265-275, October 22–25, 2013,
... after creep-rupture test at 750°C, 800°C and 850°C were characterized in this paper by scanning electron microscopy, transmission electron microscopy and chemical phase analysis in details. The phase compositions of alloy 740H were also calculated by thermodynamic calculation. The research results...
Proceedings Papers

AM-EPRI2016, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Eighth International Conference, 429-439, October 11–14, 2016,
... Abstract The influence of holding time during tempering on the long-term creep rupture strength of mod.9Cr-1Mo steel was investigated in this study, so as to elucidate proper heat treatment for boiler applications. Tempering was conducted at 770°C for 0.5h, 1h, 3h, 10h and 100h for the test...
Proceedings Papers

AM-EPRI2019, 2019 Joint EPRI – 123HiMAT International Conference on Advances in High-Temperature Materials, 1169-1180, October 21–24, 2019,
... Abstract This paper presents results and analyses from long-term creep-rupture testing of alloy CCA617 (also known as alloy 617B) in wrought and welded forms at temperatures and stresses relevant to power generation under advanced steam conditions. The refined controlled chemical composition...
Proceedings Papers

AM-EPRI2016, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Eighth International Conference, 951-961, October 11–14, 2016,
... and final passes. Cross-weld tensile tests, side bend tests and impact tests of weld metals and heat-affected zones were carried out at ambient temperatures after two post-weld heat treatments (PWHT), each at 730°C for 12 hours. Creep rupture tests of cross-weld samples were performed at 625°C. This study...
Proceedings Papers

AM-EPRI2019, 2019 Joint EPRI – 123HiMAT International Conference on Advances in High-Temperature Materials, 185-196, October 21–24, 2019,
... Abstract Creep strength degradation behavior of normalized and tempered 2.25Cr-1.6W-V-Nb(Gr.23) steel was investigated by conducting extra long-term creep rupture tests. Creep strength drop was observed in long-term creep range at 600°C and above, while signs of a creep strength drop were...
Proceedings Papers

AM-EPRI2013, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Seventh International Conference, 903-913, October 22–25, 2013,
... as candidate materials for piping and superheater/reheater tubes in an A-USC boiler. Weldments of these alloys were manufactured by GTAW, after which long term creep rupture tests were conducted at 700°C, 750°C and 800°C. Weldments of HR6W, HR35 and Alloy617 showed similar creep strength as compared...
Proceedings Papers

AM-EPRI2019, 2019 Joint EPRI – 123HiMAT International Conference on Advances in High-Temperature Materials, 513-522, October 21–24, 2019,
... cracking. Stability of creep strength and microstructure has been confirmed by long-term creep rupture tests. The 100,000h average creep rupture strength of HR6W is 85MPa at 700C. That of HR35 is 126MPa at 700°C which is comparable with conventional Alloy617. Tubes of both alloys have been evaluated...
Proceedings Papers

AM-EPRI2019, 2019 Joint EPRI – 123HiMAT International Conference on Advances in High-Temperature Materials, 80-89, October 21–24, 2019,
... Abstract Long-term creep rupture tests up to 10 5 hours at 600℃ and 650℃ were carried out on mod.9Cr- 1Mo steel base metal and weldments from five different materials, consisting of various chemical compositions and heat treatments as well as welding conditions. As a result, positive...
Proceedings Papers

AM-EPRI2016, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Eighth International Conference, 446-457, October 11–14, 2016,
... the welded portions of the intrados and extrados of the elbow, and the number density of creep voids in fine-grained HAZ was measured in the wall-thickness direction. Then, creep rupture tests were performed to examine the remaining life of each portion of the base metal and welded joint. On the basis...
Proceedings Papers

AM-EPRI2010, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Sixth International Conference, 408-422, August 31–September 3, 2010,
... Abstract 10CrMoWVNbN (X 12 CrMoWVNbN 10 1 1) steel trial forgings has been manufactured to clarify the effect of austenitizing temperature on the creep rupture strength and microstructure. From the results of creep rupture tests up to 30,000 hours, higher austenitizing temperature improves...
Proceedings Papers

AM-EPRI2007, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Fifth International Conference, 185-196, October 3–5, 2007,
... Abstract SUPER304H (18Cr-9Ni-3Cu-Nb-N, ASME CC2328) and TP347HFG (18Cr-12Ni-Nb, ASME SA213) are advanced fine-grained microstructure steel tubes developed for high strength and superior steam oxidation resistance. Their exceptional performance is demonstrated by the longest creep rupture tests...
Proceedings Papers

AM-EPRI2013, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Seventh International Conference, 131-142, October 22–25, 2013,
... in A-USC boilers. Two alloys were considered to have potential for this application: Inconel 740 and Haynes 282 alloy. In support of this application, creep-rupture testing of several heats of Inconel 740 was conducted over a range of temperatures and stresses to develop confidence in qualitatively...
Proceedings Papers

AM-EPRI2013, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Seventh International Conference, 690-701, October 22–25, 2013,
...; the results indicated that the damage to the elbow was more severe in the fine-grain heat-affected zone near the inner surface. Furthermore, creep rupture tests were performed using specimens cut from the welded joint of the elbow, and from these results, the remaining life was evaluated using the time...
Proceedings Papers

AM-EPRI2016, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Eighth International Conference, 1149-1159, October 11–14, 2016,
... Abstract Large heat-to-heat variation of creep rupture strength in weldments of mod.9Cr-1Mo steels was observed in the creep rupture tests conducted for two different heats at 600°C and 650°C. One heat showed consistently lower time-to-rupture than the other for 130-60MPa at 600°C. Detailed...
Proceedings Papers

AM-EPRI2010, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Sixth International Conference, 1067-1076, August 31–September 3, 2010,
...-wall pipe. The integrity of the weldment was confirmed with metallurgical investigation, mechanical testing and long term creep rupture test. It is proved that the narrow gap HST welding procedure can meet the requirements for Ni based or Fe-Ni based alloys and provides excellent strength properties...
Proceedings Papers

AM-EPRI2007, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Fifth International Conference, 874-883, October 3–5, 2007,
... occurs in HAZ of the weldment. In the creep rupture test of these welded joints the rupture strength is lower than that of the parent metal, and sometimes this reduction of strength is caused by TypelV cracking. To develop an effective method to improve the rupture strength of welded joint, advanced...
Proceedings Papers

AM-EPRI2010, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Sixth International Conference, 916-932, August 31–September 3, 2010,
..., resulting in better strength and impact resistance at room-temperature, and about 20% higher yield-strength (YS) at 760°C, and similar or better ductility compared to the as-cast material. The initial creep-rupture testing at 700-800°C for up to 2000h also indicates similar or better rupture resistance...
Proceedings Papers

AM-EPRI2004, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Fourth International Conference, 987-998, October 25–28, 2004,
... ppm). Creep rupture tests were conducted at 923K for up to 10,000 hours. Despite their higher boron content, these steels exhibited good weldability. Welded joints of the boron steel displayed superior creep properties compared to conventional high-chromium ferritic steel welds like P92 and P122...