Diffusion bonded compact heat exchangers have exceptionally high heat transfer efficiency and might significantly improve the performance and reduce the cost of supercritical carbon-dioxide Brayton cycle power plants using high temperature heat sources, like high temperature nuclear reactors and concentrating solar power plants. While these heat exchangers have an excellent service history for lower temperature applications, considerable uncertainty remains on the performance of diffusion bonded material operating in the creep regime. This paper describes a microstructural modeling framework to explore the plausible mechanisms that may explain the reduced creep ductility and strength of diffusion bonded material, compared to wrought material. The crystal plasticity finite element method (CPFEM) is used to study factors affecting bond strength in polycrystals mimicking diffusion bonded microstructures. Additionally, the phase field method is also employed to simulate the grain growth and recrystallization at the bond line to model the bonding process and CPFEM is used to predict the resulting material performance to connect processing parameters to the expected creep life and ductility of the material, and to study potential means to improve the structural reliability of the material and the resulting components by optimizing the material processing parameters.

This content is only available as a PDF.