Local vacuum electron beam welding is an advanced manufacturing technology which has been investigated at Sheffield Forgemasters to develop as part of a cost-effective, reliable, agile, and robust manufacturing route for the next generation of civil nuclear reactors in the UK. A dedicated electron beam welding facility at Sheffield Forgemasters has been installed. This includes an x-ray enclosure, 100kW diode electron gun, 100T turntable, and weld parameter development vacuum chamber. A small modular reactor demonstrator vessel has successfully been manufactured with a wall thickness of 180 mm, including indication-free slope-in, steady- state and slope-out welding parameters. Electroslag strip cladding has also been investigated to demonstrate its viability in reactor pressure vessel manufacture. The electro-slag strip cladding method has been shown to produce high quality 60 mm strips on a 2600 mm inner diameter ring.