Abstract
The A286 is one of the earliest superalloys developed. It has been used for manufacturing different components of turbo machineries because of its balanced high temperature properties. These components include shafts, discs, spacers, blades and fasteners. This paper reviews some of the issues and recent field experiences related to metallurgy, fabrication, in-service evaluation and failure of some of these components. The fabrication aspects including the effects of alloy melting processes, forging parameters and different types of heat treatments on the processed parts are discussed. The importance of these factors on the microstructure and properties of A286 are highlighted. The effects of service exposure on some of these parts are also discussed. In service evaluation involves checking for service induced damage or changes in microstructures and properties so that the suitability of the part for continued service can be determined. The failure analysis section of the paper briefly discusses failures of two expander wheels and an expander disc made out of A286 to pinpoint some of the salient features of damage accumulation and fracture during service.