Abstract
The fall-off of oxide scale with poor adhesion inside superheater/reheater tubes in boilers for (ultra) supercritical power unit is the main cause of accidents such as superheater/reheater blockage, tube explosion and solid particle erosion in the steam turbine which cause serious economic losses. However, there is still no method for testing and assessing the adhesion of oxide scale inside the tube. A method for testing the adhesion of corrosion products in tubes by spiral lines is proposed in this paper, and the accuracy of adhesion evaluation is improved by adopting the image recognition method.