The piping stress and thermal displacement corresponding to different types of riser rigid support and hanger devices in different installation directions have been calculated by means of finite element analysis, to further analyze the impact on cracking of adjacent steam tee welds exerted by the constraint effect of riser rigid hangers on angular displacement. It can be seen from the analysis that a riser rigid hanger has a constraint effect on angular displacement, and such a constraint effect, however, is weak and limited on the piping stress and thermal displacement, so the piping stress and supports and hangers are not the main reasons for the cracking of tee welds. In addition, the calculation results alert that for an axial limiting hanger of riser with a dynamic axial pipe clamp and rigid struts, its constraint effect on angular displacement has a significant impact on the piping stress and thermal displacement.