Abstract
This paper addresses the limitations of P92 steel used in ultra-supercritical power plants, particularly ferrite formation in thick components and its impact on short- and long-term properties. A guideline for determining ferritic content in P92 steel is presented. Furthermore, a novel 12% Cr boiler steel grade, VM12-SHC, is introduced. This new material offers good creep properties and oxidation resistance, overcoming the limitations of P92 steel. Finally, the development of matching filler metals for welding P92 and VM12-SHC steels is presented, ensuring optimal weld compatibility and performance in power plant applications.