T24 tube material (7CrMoVTiB10-10), with its combination of high creep strength and potential to be welded without using preheat, is regarded as a candidate waterwall material for Ultra Supercritical (USC) boilers. However, its reputed sensitivity to hydrogen and potential for secondary hardening may have adverse impacts on construction of waterwall panels. Doosan Babcock Ltd have investigated the response of welds made in T24 tubing to secondary hardening via changing hardness in a series of ageing heat treatment trials. Also, the response of the material to hydrogen infusion has been investigated