Abstract
In this paper, the performance of T23 and 12Cr1MoVG water wall tubes as well as their welded joints in engineering applications is reported. It was found that the T23 water wall tube may have water leak problems during its operation. In order to make sure the safe operation, leakage reasons of T23 water wall tube were analyzed and improvement measures were taken. Recommendations on the choice of water wall material of 1000MW USC tower boiler are given.