Abstract
In order to reduce CO2 emissions and improve power generation efficiency, a development project involving an advanced USC (A-USC) plant has been carried out in Japan since 2008. Nibased alloys are candidate materials for boiler components with high temperature steam conditions, which are much stronger than conventional heat resistant steel. However, Ni-based alloys have never been applied with respect to the high pressure parts and thick walled components of USC coal-fired power plants. In this study, therefore, fabrication and characteristic properties, such as weldability, the weld joint and bent part properties, and weld cracking susceptibilities of Ni-based alloys such as HR6W, HR35 and two types of Alloy617 (High B and Low B) pipes were evaluated. Additionally, two types of HR6W header mock-ups and a HR6W tube element mock-up were fabricated. With the exception of Alloy617 (High B), the fabrication trials of Ni-based alloy pipes were conducted successfully, and the long-term creep strength of weldments and bends of Ni-based alloy pipes were found to be nearly equivalent to those of base metal. In the case of Alloy617 (High B), hot cracking was observed.