Abstract
This paper presents an overview of China’s electric power development and the National 700°C Ultra-Supercritical (USC) Coal-Fired Power Generation Technology Innovation Consortium. Besides, the R&D plan and latest progress of China 700°C USC coal-fired power generation technology is also introduced in this paper.