In Europe and Japan, great efforts are currently being invested in the development of materials designed to increase the steam temperature in fossil power plants. In the steel segment, the COST program is concentrating on 10% Cr steels with the addition of boron with the aim of achieving a steam temperature of 650°C. With nickel-based materials, the goal is to achieve steam temperatures of 700°C and higher. Alloy 617 has proved to be a very promising candidate in this field and a modified version is currently being developed in Japan. Materials of this type are used in both the turbine and in parts of the boiler.