The capacity of PC power plants in Japan rose to 35GW in 2004. The most current plants have a 600 deg-C class steam temperature and a net thermal efficiency of approximately 42% (HHV). Older plants, which were built in the ‘70s and early ‘80s, will reach the point where they will need to be rebuilt or refurbished in the near future. The steam temperatures of the older plants are 538 deg-C or 566 deg-C. We have done a case study on the refurbishment of one of these plants with the advanced USC technology that uses a 700 deg-C class steam temperature in order to increase the thermal efficiency and to reduce CO2 emissions. The model plant studied for refurbishing has a 24.1MPa/538 deg-C /538 deg-C steam condition. We studied three possible systems for the refurbishing. The first was a double reheat system with 35MPa/700 deg-C /720 deg-C /720 deg-C steam conditions, the second one was a single reheat 25MPa/700 deg-C/720 deg-C system, the last one was a single reheat 24.1MPa/610 deg-C/720 deg-C system. In addition to these, the most current technology system with 600 deg-C main and reheat temperatures was studied for comparison. The study showed that the advanced USC Technology is suitable for refurbishing old plants. It is economical and environmentally-friendly because it can reuse many of the parts from the old plants and the thermal efficiency is much higher than the current 600 deg-C plants. Therefore, CO2 reduction is achieved economically through refurbishment.

This content is only available as a PDF.