Alloy Digest (1956) 5 (6): Zn-3.
Published: 01 June 1956
... DI-METAL 3 is a zinc-base alloy of high fluidity capable of producing fine detail in die castings. It is the most stable of the zinc die casting alloys, but on aging loses about 20% of its tensile strength with practically no impact drop. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1966) 15 (11): TS-185.
Published: 01 November 1966
...). Its hardness is uniform within one or two Rockwell C points from surface to center in sections as heavy as eight inches thick. lr can be obtained in the un- hardened condition also. Forms Available: Forging billets, bars, forgings Applications: Zinc die casting dies, injection and compression molded...
Journal Articles
Alloy Digest (1957) 6 (4): Zn-4.
Published: 01 April 1957
... No. 2 DIE METAL is a zinc-base alloy recommended primarily for die castings and sand castings (stamping and drop-hammer dies). This datasheet provides information on composition, physical properties, hardness, tensile properties, and shear strength as well as fracture toughness and fatigue...
Journal Articles
Alloy Digest (1967) 16 (7): Zn-10.
Published: 01 July 1967
... ASARCO Z.D.C. No. 7 is a zinc die casting alloy which will be found particularly helpful in casting relatively large, complicated shapes and intricate parts which are not free to shrink in the dies because of cores, slides, etc. and require a hardware finish for subsequent plating or organic...
Journal Articles
Alloy Digest (1991) 40 (8): Zn-51.
Published: 01 August 1991
.... 07050 I USA apac#icatfon w fnal dss&m ZAMAK 2 (Zinc Die Casting Alloy) ZAMAK 2 is the strongest and hardest of the four Zamak alloys. While generally produced by die casting, ZAMAK 2 is occasionally gravity cast. It is not a widely used alloy. Composition (Principal Elements): AIuminum 3.943 Copper 2.6...
Journal Articles
Alloy Digest (1989) 38 (3): Zn-47.
Published: 01 March 1989
... 33521. Ten-year indoor aging tests on UNS Z 33522 show that it has the same degree of permanence of properties and di- mensional stability as UNS Z 33522. Forms Available: Ingots, die castings. Applications: Die Castings. Manufacturer: Virtually all companies making zinc die casting alloys. ...
Journal Articles
Alloy Digest (1972) 21 (5): Zn-14.
Published: 01 May 1972
... ILZRO 16 is a zinc-base die-casting alloy which was developed to have superior creep resistance at both ambient and elevated temperatures for processing in cold-chamber die-casting machines. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Journal Articles
Alloy Digest (1986) 35 (10): TS-15.
Published: 01 October 1986
... CASCADE is a precipitation-hardening steel which is very popular as a mold steel for injection molding of thermoplastics. It is also an excellent choice for many zinc die-casting dies because of its resistance to heat checking and wash. A further wide usage for Cascade is as a holding-block...
Journal Articles
Alloy Digest (1975) 24 (10): TS-292.
Published: 01 October 1975
... ALMOLD 20 is a chromium-molybdenum tool steel of medium-carbon content. It was designed especially for zinc die casting dies and plastic molds. It is produced to high-quality tool-steels standards to permit a high luster to be achieved on polished die cavity surfaces. This datasheet provides...
Journal Articles
Alloy Digest (2009) 58 (11): TS-684.
Published: 01 November 2009
..., zinc die-casting dies, pressure plates, tool holders, rubber molds, composite olds, and stripper plates. Producer: Crucible Service Centers Divisional Headquarters Camillus, NY Tel: 315/487-0800 Fax: 315/487-4028 www.cruciblesservice.com ISSN: 002-614X TS-684 DOI: 10.31399/asm.ad.ts0684 ...
Journal Articles
Alloy Digest (1975) 24 (1): Zn-17.
Published: 01 January 1975
... to corrosion, chemically treat all finish-machined castings by a chromate conversion coating process. General Characteristics: FORMALOY is a high-strength zinc-base alloy which provides unsurpassed performance in dies to form sheet metal. Punch and die forms are easily cast and machined with this stronger...
Journal Articles
Alloy Digest (1981) 30 (8): Zn-37.
Published: 01 August 1981
... Tg-12 Zinc Alloy is the general-purpose, zinc-aluminum-copper foundry alloy. It can be sand, permanent-mold or die cast, has a modest cost and a tensile strength suitable for many applications where bronze and cast or malleable iron were traditionally used. Tg-12 is extremely resistant to galling...
Journal Articles
Alloy Digest (1988) 37 (3): Zn-42.
Published: 01 March 1988
... UNS No. Z35635 is a zinc-aluminum-copper-magnesium foundry alloy recommended for castings of moderate strength and low cost. It was designed for use in nonferrous permanent-mold foundries to compete with cast-iron, aluminum and bronze castings. The alloy can be sand cast and die cast. Its many...
Journal Articles
Alloy Digest (1982) 31 (8): Zn-38.
Published: 01 August 1982
... KIDD Alloy ZA-12 is the general-purpose, zinc-aluminum-copper foundry alloy. It can be sand, permanent-mold or die cast. Alloy ZA-12 has a modest cost and a tensile strength suitable for many applications where bronze and cast or malleable iron were traditionally used. Alloy ZA-12 is extremely...
Journal Articles
Alloy Digest (1968) 17 (8): Zn-11.
Published: 01 August 1968
... ILZRO-14 is a zinc-base die casting alloy developed with superior creep resistance at both ambient and elevated temperatures. It is recommended for carburetors, fuel pumps, valve bodies, etc. This datasheet provides information on composition, physical properties, hardness, and tensile properties...
Journal Articles
Alloy Digest (1977) 26 (6): Cu-335.
Published: 01 June 1977
... and lower speed than used for aluminum or zinc alloys. Also, the relatively high casting temperature can contribute to a die deterioration problem because of die cracking. This difficulty, however, has been minimized by the die producers who have developed special metals and processes for making the dies...
Journal Articles
Alloy Digest (1978) 27 (5): Cu-354.
Published: 01 May 1978
... Copper Alloy No. 858 is a copper-zinc-tin-lead (yellow brass) alloy for die castings. It is a low-cost, general-purpose alloy with good machinability and soldering characteristics. Its many uses include general and marine hardware, pump, impellers, plumbing parts and gears. This datasheet provides...
Journal Articles
Alloy Digest (1988) 37 (7): Zn-43.
Published: 01 July 1988
... plating or protective laquering. Plating: UNS NO. 235630 can be readily plated using the similar cleaning and preliminary copper strike procedures used for plating zinc die castings. A shorter or milder cleaning cycle is. however, recommended. Chromating: UNS NO. 235630 should be coated with zinc...
Journal Articles
Alloy Digest (1982) 31 (1): TS-393.
Published: 01 January 1982
.... It is produced to high-quality tool-steel standards to permit a high luster to be achieved on the surface of the polished die cavity. P20 is used for molds for plastics and for die-casting dies for zinc and other low-temperature casting alloys. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1977) 26 (9): Zn-31.
Published: 01 September 1977
...- sequent plating or protective laquering. Plating: ZA-12 can be readily plated using the same cleaning and preliminary copper strike procedures used for plating zinc die castings. A shorter or milder cleaning cycle is, however, recommended. A preliminary copper strike is recommended prior to plating...