Alloy Digest (1979) 28 (4): SA-358.
Published: 01 April 1979
.... This steel is capable of developing a minimum yield strength of 140,000 psi with an optimum combination of hardenability, temperability, weldability, formability, toughness and fatigue properties. It meets many special requirements for petrochemical applications. This datasheet provides information...
Journal Articles
Alloy Digest (1983) 32 (9): SA-393.
Published: 01 September 1983
... and toughness. This steel is capable of developing a minimum yield strength of 140,000 psi with an optimum combination of hardenability, temperability, weldability, formability, toughness and fatigue properties. It meets many special requirements for petrochemical applications. This datasheet provides...
Journal Articles
Alloy Digest (1989) 38 (8): CS-125.
Published: 01 August 1989
... BETHLEHEM RQ 100L is a low-carbon, low-sulfur, 100 ksi minimum yield strength quenched-and-tempered plate steel offering improved toughness and weldability over other quenched-and-tempered plate grades. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (2012) 61 (1): SA-640.
Published: 01 January 2012
... Superelso 890 (minimum yield strength of 890 MPa, or 130 ksi) is a high yield strength quenched and tempered steel alloy. This datasheet provides information on composition, tensile properties, and bend strength as well as fracture toughness. It also includes information on forming, machining...
Journal Articles
Alloy Digest (2012) 61 (2): SA-644.
Published: 01 February 2012
... Superelso 960 (minimum yield strength of 960 MPa, or 140 ksi) is a high yield strength quenched-and-tempered steel alloy. This datasheet provides information on composition and tensile properties as well as fracture toughness. It also includes information on forming, machining, and joining. Filing...
Journal Articles
Alloy Digest (2012) 61 (6): SA-654.
Published: 01 June 2012
... SuperElso 1100 is a high yield strength quenched and tempered steel alloy. For welded and weight-saving structures. This datasheet provides information on composition and tensile properties as well as fracture toughness. It also includes information on forming, machining, and joining. Filing Code...
Journal Articles
Alloy Digest (2013) 62 (7): SA-678.
Published: 01 July 2013
... Supralsim 690 QL1 is a high yield-strength quenched and tempered steel for welded and weight-saving structures. This datasheet provides information on composition and tensile properties as well as fracture toughness. It also includes information on forming, machining, and joining. Filing Code: SA...
Journal Articles
Alloy Digest (2006) 55 (12): Co-115.
Published: 01 December 2006
... Phynox is a high yield strength cobalt alloy with a range of physical, chemical, and technological properties that make it useful for a wide variety of applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also...
Journal Articles
Alloy Digest (2007) 56 (2): Fe-140.
Published: 01 February 2007
... Durimphy is a maraging steel with 1724 MPa (250 ksi) tensile strength and a very high yield strength due to precipitation hardening. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance...
Journal Articles
Alloy Digest (2007) 56 (3): Fe-141.
Published: 01 March 2007
... Phytime is a maraging steel with a 2068 MPa (300 ksi) strength and a very high yield strength due to precipitation hardening. The major improvement over Durimphy (see Alloy Digest Fe-140, February 2007) is cleanliness and improved fatigue performance. This datasheet provides information...
Journal Articles
Alloy Digest (1972) 21 (9): SA-280.
Published: 01 September 1972
... HY-130 and HY-140(T) comprise one steel composition capable of developing minimum yield strengths of 130,000 and 140,000 psi with an optimum combination of toughness, hardenability, temperability, weldability, formability and fatigue properties in thicknesses through 4 inches. This datasheet...
Journal Articles
Alloy Digest (1980) 29 (4): Ti-76.
Published: 01 April 1980
... RMI 25 is a grade of commercially pure titanium. It has a guaranteed minimum yield strength of 25,000 psi with good ductility and formability. Its yield strength is about the same as that of the annealed austenitic stainless steels of lowest yield strength. It has excellent resistance to corrosion...
Journal Articles
Alloy Digest (1990) 39 (8): CI-62.
Published: 01 August 1990
... 55-06 and 70-02 Ductile Dura-Bar are continuously cast ductile irons with about 50 and 75% pearlitic microstructures, respectively. 55-06 has about the same tensile strength as SAE 1045 as-hot-rolled steel. Its maximum yield strength and elongation are equivalent to a eutectoid carbon steel. 70-02...
Journal Articles
Alloy Digest (1980) 29 (2): Ti-75.
Published: 01 February 1980
... RMI 5A1-2.5Sn ELI (ELI = Extra Low Interstitials) is an alpha titanium alloy that was developed for use at cryogenic temperatures. It has a guaranteed minimum yield strength of 100,000 psi at room temperature with good ductility and formability; its yield strength and elongation increase...
Journal Articles
Alloy Digest (1963) 12 (11): SA-157.
Published: 01 November 1963
... USS T-1 Type-A is a high yield strength constructional alloy steel recommended where high levels of yield strength and toughness are required. It is furnished in the quenched and tempered condition. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (2016) 65 (1): SA-738.
Published: 01 January 2016
... SPARTAN II (HSLA-100) is one of the family of Spartan high strength (>690 MPa, or >100 ksi, minimum yield strength), high toughness, improved weldability steels, which are alternatives to traditional quenched and tempered alloy steels. The Spartan family of steels are low carbon, copper...
Journal Articles
Alloy Digest (2016) 65 (3): SA-743.
Published: 01 March 2016
... SPARTAN III (HSLA-100) is one of the family of Spartan high strength (>690 MPa, or >100 ksi, minimum yield strength), high toughness, improved weldability steels, which are alternatives to traditional quenched and tempered alloy steels. The Spartan family of steels are low carbon, copper...
Journal Articles
Alloy Digest (1971) 20 (12): SA-270.
Published: 01 December 1971
... REPUBLIC HP 9-4-20 is designed especially for applications requiring optimum combinations of relatively high yield strength and toughness with good weldability. This alloy is capable of providing 180,000 psi yield strength in combination with a Charpy V-notch value of 50 ft-lb at 75 F in plate...
Journal Articles
Alloy Digest (1980) 29 (7): Ti-78.
Published: 01 July 1980
... RMI 5A1-5Sn-2Zr-2Mo-Si is an alpha-type titanium alloy recommended for high-temperature applications in the 800-1000 F range. In the mill annealed condition it has a typical room-temperature yield strength of 126,000 psi and a typical yield strength (in short-time elevated-temperature tensile test...
Journal Articles
Alloy Digest (2019) 68 (12): SA-858.
Published: 01 December 2019
... Armstrong Ultra 690 is a high yield strength steel for welded and weight saving in structures. It has a minimum yield strength of 690 MPa (100 ksi) in thicknesses up to 50 mm (2 in.). This datasheet provides information on composition and tensile properties. It also includes information on forming...