Alloy Digest (1990) 39 (5): Ni-383.
Published: 01 May 1990
... International Carpenter Nickel 205 alloy chemical composition elasticity electrical resistance heat treatability oxidation resistance physical properties tensile properties wrought nickel alloys UNS N02205 CARPENTER NICKEL 205 ALLOY Filing Code: Nickel Alloy Ni-383 - DIGEST- MAY 1990 DATA...
Journal Articles
Alloy Digest (1988) 37 (11): Ni-364.
Published: 01 November 1988
... AL 200 and AL 201 alloys are wrought commercially pure nickel. They differ, as to composition, in maximum specified carbon levels (0.15 for AL 200 and 0.02 for AL 201). Strengths of both alloys in the annealed condition are similar to that of mild steel. The lower carbon AL 201 alloy has higher...
Journal Articles
Alloy Digest (1989) 38 (11): Cu-549.
Published: 01 November 1989
... AND ALLOYS tZCq&ght 1589. Atby Digest. Inc. Ati tights msen.d P&M by: Alloy DiiesI,lnc./2O1-677-9161 Datashowlam~.notto&dfu 27Canfield Street, Orangs.N.J.070501U.S.A. sAxedationwhnat~n. COPPER ALLOY NO. C72500 (Copper-Nickel-Tin Wrought Alloy) COPPER ALLOY No. C72500 is a tin-bearing cupronickel. It has...
Journal Articles
Alloy Digest (1990) 39 (3): Ni-244.
Published: 01 March 1990
... Inconel alloy MA 754 is an oxide-dispersion-strengthened nickel-chromium alloy produced by mechanical alloying. It offers the advantages of a wrought high-temperature material in service environments where only cast alloys could be used in the past. Its strength in conjunction with its high...
Journal Articles
Alloy Digest (1991) 40 (11): Cu-566.
Published: 01 November 1991
... ~fkm or fmal cbs@l. COPPER ALLOY No. C72700 (Wrought Copper/Nicket/Tin Alloy) Copper Alloy No. C72700 is a copper/nickel/tin alloy which is responsive to spinodal decomposition hardening. Composition: Nominal Minimum Maximum Copper (including silver) 84.8 Remainder Lead - - 0.02* Iron - - 0.50 Zinc...
Journal Articles
Alloy Digest (1953) 2 (3): Ni-3.
Published: 01 March 1953
... INCONEL X is a high-strength, high-temperature nickel-base alloy responding to age hardening for maximum properties. It is highly resistant to chemical corrosion and oxidation. Its creep rate is low under high stresses at 1200-1500 F. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1990) 39 (6): Cu-553.
Published: 01 June 1990
... Copper alloy No. C76390 is a wrought (rod) leaded nickel silver with nominally 24.5% nickel and 1% lead. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on forming, heat treating, machining, and joining. Filing Code: Cu-553...
Journal Articles
Alloy Digest (2025) 74 (1): SA-879.
Published: 06 March 2025
... 8620, 8620H, 8620RH, 20NiCrMo2-2, 20NiCrMoS2-2, SNCM220, and SNCM220H are wrought, low-carbon, nickel-chromium-molybdenum, low alloy steels that are typically used in the carburized or carbonitrided, and subsequently quench hardened, and tempered condition. In general, these steels are intended...
Journal Articles
Alloy Digest (1987) 36 (2): Ni-345.
Published: 01 February 1987
... NIMONIC Alloy 81 is a wrought nickel alloy designed to provide enhanced resistance to high-temperature corrosion coupled with good high-temperature strength. It is particularly resistant to attack by deposits of alkali metal sulfates and chlorides resulting from combustion of impure fuels...
Journal Articles
Alloy Digest (1976) 25 (5): Ni-228.
Published: 01 May 1976
... NIMAG 105 is a wrought nickel alloy with a high magnetostriction coefficient. It is easily formed or drawn, has a high Curie temperature and has low oxidation at high temperatures. It is recommended for electronic and electrical applications. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1977) 26 (7): Ni-247.
Published: 01 July 1977
... TECHALLOY Nickel 205 is a wrought nickel-base alloy containing small additions of magnesium and titanium. It has a high Curie temperature and a high magnetostriction coefficient. It is used for many electrical and electronic components and for equipment employing magnetostrictive effects...
Journal Articles
Alloy Digest (1994) 43 (6): Ni-456.
Published: 01 June 1994
... Carlson Alloys C200 and C201 are wrought forms of nickel with carbon the only difference in composition. The metal has excellent resistance to dry chlorine and hydrogen chloride and caustic alkalis. The alloys combine good mechanical properties with excellent resistance to corrosive environments...
Journal Articles
Alloy Digest (2006) 55 (5): Ni-637.
Published: 01 May 2006
... International® 2006 2006 ASM International aircraft manufacturing applications chemical composition creep properties elasticity HAYNES 282 heat treatability high-temperature alloys physical properties tensile properties workability wrought nickel alloys thermal properties Chemical...
Journal Articles
Alloy Digest (2000) 49 (3): Ni-559.
Published: 01 March 2000
... AL-22 is a wrought 22Cr-13.5Mo-3W-4Fe high-nickel alloy with outstanding and versatile corrosion resistance. The alloy is available in plate and is used where excellent corrosion, pitting, or crevice corrosion resistance is needed. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1992) 41 (12): Ni-419.
Published: 01 December 1992
... Carlson alloy C825 is a wrought nickel-iron-chromium alloy with additions of molybdenum, copper, and titanium. It was developed to handle both reducing and oxidizing media. The alloy is resistant to chloride-ion stress-corrosion cracking, to pitting and crevice attack and many corrosive solutions...
Journal Articles
Alloy Digest (1977) 26 (6): Ni-246.
Published: 01 June 1977
... TECHALLOY Nickel 200 is commercially pure wrought nickel. It maintains good strength at elevated temperatures and is tough and ductile at low temperatures. It is a general-purpose material when the properties of nickel alloys are not needed. Its many uses include spun and cold-formed parts...
Journal Articles
Alloy Digest (1975) 24 (1): Ni-214.
Published: 01 January 1975
... Nickel-Copper Alloys 410 and 411 are strong and ductile casting alloys; they are generally used in conjunction with wrought counterparts. They can be cast readily into fittings such as elbows, tees, return bends, flanges and similar components. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1987) 36 (1): Ni-51.
Published: 01 January 1987
... UDIMET 700 is a wrought nickel-base alloy produced by vacuum-induction melting and further refined by vacuum-arc remelting. It has excellent mechanical properties at high temperatures. Among its applications are blades for aircraft, marine and land-based gas turbines and rotor discs...
Journal Articles
Alloy Digest (1995) 44 (7): Cu-602.
Published: 01 July 1995
... MARINEL alloy is a very high strength cupronickel exhibiting immunity to hydrogen embrittlement. It is a wrought precipitation hardened alloy containing about 18% nickel and 5% manganese, strengthened by additions of aluminum, iron, chromium, and niobium, and has been developed to provide...
Journal Articles
Alloy Digest (1998) 47 (6): Ni-539.
Published: 01 June 1998
... ASM International chemical composition corrosion-resistant alloys elasticity electronic applications machinability NICKEL 200 NICKEL 201 physical properties tensile properties wrought nickel alloys thermal properties UNS N02200 N02201 - DIGES 1 Filing code: Nl-539 Ini a Nickel...