... joinability physical properties tensile properties workability wrought copper alloys UNS C72700 COPPER ALLOY No. C727 Y u-s6 NOVEMBER 1991 .LOYS cc@y@hf 1991.AlbyDgasr..AIlr#fsrarerved. PcMshedby; [email protected] Dafa8flownue!jpfmf,m7ftobeusedfof 2? Canfeld SIreel. Orange, NJ. 070!50 I USA...
Journal Articles
Alloy Digest (1989) 38 (11): Cu-549.
Published: 01 November 1989
... Copper alloy no. C72500 corrosion-resistant alloys elasticity hardness heat treatability joinability machinability physical properties tensile properties workability wrought copper alloys UNS C72500 COPPER ALLOY NO, C725 I:~ cu-54g NOVEMBER 1989 -DIGEST - DATA ON WORLD WIDE METALS...
Journal Articles
Alloy Digest (1990) 39 (6): Cu-553.
Published: 01 June 1990
... Copper alloy No. C76390 is a wrought (rod) leaded nickel silver with nominally 24.5% nickel and 1% lead. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on forming, heat treating, machining, and joining. Filing Code: Cu-553...
Journal Articles
Alloy Digest (1980) 29 (11): Cu-406.
Published: 01 November 1980
... heat treatability joinability machinability munitions novelties physical properties tensile properties workability wrought copper alloys UNS C21000 I I Filing Code: Cu-406 1 ANACONDA Alloy 210 1 copper Alloy NOVEMBER 1980 - DATA ON WORLD WIDE METALS AND ALLOYS P- bu 0 Copyright 1980...
Journal Articles
Alloy Digest (1972) 21 (5): Cu-255.
Published: 01 May 1972
... - DATA ON WORLD WIDE METALS AND ALLOYS Pnblisbed by Engineering Alloys Digest, Inc. Upper Monrclair, New Jersey COPPER ALLOY No. 210 (Wrought Brass Alloy) COPPER ALLOY No. 210 is a 5% zinc brass having excellent cold working properties. Composition: Copper 94.0-96.0 Lead* 0.05 max Iron 0.05 max Total...
Journal Articles
Alloy Digest (1963) 12 (4): Cu-20.
Published: 01 April 1963
... hardness heat treatability joinability machinability physical properties tensile properties thermal conductivity wear resistance BERYLCO 165 Filing Code: Cu-20 Copper Alloy Revised: 4/l/63 NOVEMgER, 1954 DATA ON WORLD WIDE METALS AND ALLOYS *BERYLCO 165 (Heat Treatable Beryllium Copper Wrought...
Journal Articles
Alloy Digest (1953) 2 (4): Cu-6.
Published: 01 April 1953
... BERYLCO 10 is a heat treatable, wrought, beryllium-copper alloy having high elastic and endurance strength, high ductility and impact strength, and high electrical and thermal conductivity. Since this material has good formability and machinability when heat treated, it is generally supplied...
Journal Articles
Alloy Digest (1977) 26 (5): Cu-333.
Published: 01 May 1977
... Copper Alloy No. 175 is a wrought copper alloy that combines high strength with good electrical and thermal conductivities. It can be hardened by aging after a solution treatment. It is used for a variety of electrical hardware components and for industrial welding equipment. This datasheet...
Journal Articles
Alloy Digest (1991) 40 (8): Cu-563.
Published: 01 August 1991
... Copper Alloy No. C72600 is a wrought copper-nickel alloy. It has excellent capacity for cold work and may be readily joined by soldering, brazing, arc and resistance welding. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well...
Journal Articles
Alloy Digest (1974) 23 (5): Cu-278.
Published: 01 May 1974
... joinability low-temperature alloys machinability oxygen-free copper physical properties shear strength tensile properties workability wrought copper alloys Copper No. 101 Filing Code: Cu-278 Copper MAY 1974 DIGEST d - DATA ON WORLD WIDE METALS AND ALLOYS Prblisbd by Engineering Alloys D&t, Inc...
Journal Articles
Alloy Digest (1987) 36 (10): Cu-529.
Published: 01 October 1987
... Copper Alloy No. C68800 is a wrought copper-base alloy (modified brass) containing nominally 22.7% zinc, 3.4% aluminum and 0.40% cobalt. It has high strength and fairly good ductility. It can be hardened and strengthened further by heating temper-rolled material to 425 F where an ordering reaction...
Journal Articles
Alloy Digest (1980) 29 (3): Cu-391.
Published: 01 March 1980
... ANACONDA Alloy 706 (also known as Cupro Nickel, 10% 706) is a wrought 90% copper-10% nickel alloy developed to provide a material less costly than the copper-nickel alloys containing 20 or 30% nickel, but yet offering much of their excellent reliability. This was achieved by adding 1.25% iron...
Journal Articles
Alloy Digest (1988) 37 (5): Cu-538.
Published: 01 May 1988
... composition corrosion-resistant alloys elasticity electrical applications fatigue properties hardness heat treatability joinability machinability oxygen free copper physical properties shear strength tensile properties UNS C10100 workability wrought copper alloys UNS C10100 UNS No. Cl0100...
Journal Articles
Alloy Digest (1979) 28 (3): Cu-368.
Published: 01 March 1979
... machinability oxygen free copper physical properties shear strength tensile properties workability wrought copper alloys UNS C10200 Copper No. 102 Filing Code: Cu-368 Copper MARCH 1979 - DATA ON WORLD WIDE METALS AND ALLOYS Publiahd by Enghering Alloys Digest. Inc. Post office Box 823 Copper No. 102...
Journal Articles
Alloy Digest (1978) 27 (12): Cu-363.
Published: 01 December 1978
... AMPCOLOY 522 is a wrought copper-nickel-iron alloy characterized by high strength and ductility, and by its excellent resistance to corrosion, especially in saline waters. It is well suited for temperatures up to 700 F. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1975) 24 (5): Cu-297.
Published: 01 May 1975
... IN-838 is a wrought copper-15% nickel alloy with a controlled chromium addition for improved corrosion resistance in flowing sea water. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance...
Journal Articles
Alloy Digest (1983) 32 (11): Cu-467.
Published: 01 November 1983
... PFINODAL C72900 is a copper-base alloy that derives its strength from spinodal hardening. It is produced by the manufacturer's wrought powder-metallurgy process for strip metal. This process provides the homogeneity and uniformity needed to achieve fully the available properties of the alloy...
Journal Articles
Alloy Digest (1976) 25 (3): Cu-310.
Published: 01 March 1976
... AMPCOLOY 83 is a wrought copper-base alloy containing nominally 1.8% beryllium. It offers good formability in the unhardened condition and can be strengthened by precipitation hardening. It has a combination of high strength and hardness, good ductility, good electrical and thermal conductivity...
Journal Articles
Alloy Digest (1991) 40 (6): Cu-561.
Published: 01 June 1991
... conductivity fabricability hardness heat treatability joinability machinability physical properties shear strength tensile properties workability wrought copper alloys - DIGEST- DATA ON WORLD WIDE METALS AND ALLOYS Filing Code: Copper Alloy CU-561 JUNE 1991 Publlshedby: uoy Digest k I201477-9161...
Journal Articles
Alloy Digest (1980) 29 (12): Cu-407.
Published: 01 December 1980
... alloys SOMERS LTA Copper Filing Code: cu-407 Wwer DECEMBER 1980 - DATA ON WORLD WIDE METAL!5 AND ALLOYS @ Copyright 1980, Engineering Publications, Inc. AN rights reserved. MN : 002-614X SOMERS LTA* Copper (Wrought Copper Foil; CDA No. Cl 1000) SOMERS LTA@ Copper is a wrought copper foil that can...