Alloy Digest (1995) 44 (3): Co-96.
Published: 01 March 1995
... implant industry physical properties tensile properties workability wrought cobalt alloys thermal properties m DIGEST- DATA ON WORLD WIDE METALS AND ALL0 YS - zzP- Fwdbhafw AIoyupl.Inc/201477-0161 27c;mfirN.J.QlOSOlU.S& BIO-DURm CARPENTER CCM@ ALLOY (Cobait-chromiummolybdenum alloy) BIG-DUR...
Journal Articles
Alloy Digest (2010) 59 (4): Co-119.
Published: 01 April 2010
.... Producer or Source: Carpenter Specialty Alloys Copyright © ASM International® 2010 2010 ASM International BioBlu 27 chemical composition elasticity hardness heat treatability machinability physical properties powder metal products tensile properties workability wrought cobalt alloys...
Journal Articles
Alloy Digest (2021) 70 (11): Co-142.
Published: 01 November 2021
... Deloro Stellite 25 is a cobalt-chromium-tungsten-nickel alloy. This tungsten strengthened cobalt-chromium alloy is the cast version of the wrought cobalt-base alloy L605. Deloro Stellite 25 is resistant to wear, galling, and corrosion and retains this resistance at high temperatures. Its...
Journal Articles
Alloy Digest (1993) 42 (3): Co-89.
Published: 01 March 1993
... ULTIMET alloy is a cobalt-base corrosion-wear alloy that compares with HASTELLOY alloys in corrosion and resistance to STELLITE alloys in its wear resistance. It is available as both wrought and cast products. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1959) 8 (3): Co-17.
Published: 01 March 1959
... HAYNES Alloy No. 36 is a cobalt-base alloy having excellent strength at temperatures up to 1800 deg. F. It is the cast modification of wrought HAYNES Alloy No. 25 and has been used successfully in jet engine blading and nozzle vanes. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1991) 40 (5): Ni-66.
Published: 01 May 1991
... NIMONIC ALLOY 105 is a wrought nickel-cobalt-chromium-base alloy strengthened by additions of molybdenum, aluminum and titanium. It has been developed for service up to 950 C (1742 F). This datasheet provides information on composition, physical properties, and elasticity as well as creep. It also...
Journal Articles
Alloy Digest (1987) 36 (10): Cu-529.
Published: 01 October 1987
... Copper Alloy No. C68800 is a wrought copper-base alloy (modified brass) containing nominally 22.7% zinc, 3.4% aluminum and 0.40% cobalt. It has high strength and fairly good ductility. It can be hardened and strengthened further by heating temper-rolled material to 425 F where an ordering reaction...
Journal Articles
Alloy Digest (1961) 10 (12): SS-28.
Published: 01 December 1961
... MULTIMET alloy is cobalt-nickel-chromium-iron austenitic alloy having high oxidation and scaling resistance along with good high-temperature properties. It tends to work harden but does not respond significantly to age-hardening. It is made in a wrought grade (0.08-0.16% carbon) and a casting...
Journal Articles
Alloy Digest (1961) 10 (12): Co-5.
Published: 01 December 1961
... HAYNES# Alloy No. 25 is a wrought, high temperature, cobalt-base alloy that has exceptional mechanical properties at temperatures up to 1800 deg. F. in the fully annealed condition without subsequent aging. It is easy to fabricate because it has excellent ductility at room temperature...
Journal Articles
Alloy Digest (2023) 72 (7): Ni-784.
Published: 01 July 2023
... Böhler L090 is a wrought, precipitation-hardenable, nickel-chromium-cobalt alloy that is strengthened by additions of titanium and aluminum. It has been developed as an age-hardenable creep resisting alloy for service at temperatures up to 900 °C (1650 °F). This datasheet provides information...
Journal Articles
Alloy Digest (2022) 71 (4): Co-144.
Published: 01 April 2022
... CarTech GADS Vitallium is a non-magnetic, cobalt-chromium-molybdenum alloy possessing a unique combination of high strength, excellent corrosion resistance, high wear resistance, and improved fatigue strength over its counterparts R31537 and R31538. This alloy is a dispersion-strengthened variant...
Journal Articles
Alloy Digest (2021) 70 (12): Co-143.
Published: 01 December 2021
... Ugitech UGI HT605 (UNS R30605) is a solid solution strengthened, wrought cobalt-chromium-tungsten-nickel alloy with excellent high-temperature strength and excellent oxidation resistance up to 1095 °C (2000 °F). This datasheet provides information on composition, physical properties, and tensile...
Journal Articles
Alloy Digest (2017) 66 (5): Co-127.
Published: 01 May 2017
... level of high-temperature alloy performance at temperatures up to 1204 °C (2200 °F). This alloy is a wrought cobalt-base alloy (Co-28Cr-21Fe- 9Ni-1.25Ti-1Nb) for use in sheet and wire forms. Not only is this alloy fully fabricable and weldable, it achieves a level of stress-rupture strength...
Journal Articles
Alloy Digest (1956) 5 (6): SA-44.
Published: 01 June 1956
... Cobalt magnet steels have high coercive force which makes it possible to maintain strong magnetic fields with relatively short magnets. These alloys must be hardened by drastic quenching in oil to obtain the maximum magnetic properties. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1990) 39 (6): Cu-553.
Published: 01 June 1990
... Copper alloy No. C76390 is a wrought (rod) leaded nickel silver with nominally 24.5% nickel and 1% lead. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on forming, heat treating, machining, and joining. Filing Code: Cu-553...
Journal Articles
Alloy Digest (1988) 37 (11): Co-84.
Published: 01 November 1988
... HAYNES ALLOY No. 150 is a cobalt-base alloy with excellent thermal shock resistance. It has a higher melting point than other cobalt-and nickel-base high-temperature alloys and resists high-temperature corrosion in air and air-sulfur dioxide atmospheres. This datasheet provides information...
Journal Articles
Alloy Digest (1955) 4 (8): Co-7.
Published: 01 August 1955
... REFRACTALOY 80 is a super heat and oxidation resistant alloy containing high percentages of cobalt, chromium nickel and molybdenum. It has an exceedingly low creep rate at elevated temperatures and shows marked high temperature stability. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1968) 17 (9): SA-231.
Published: 01 September 1968
... NM-100 STEEL is a wrought, highly alloyed martensitic steel having excellent wear and corrosion resistance at temperatures up to 1100 F. It is recommended for high temperature bearings and bushings. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (1990) 39 (5): Ni-383.
Published: 01 May 1990
... International Carpenter Nickel 205 alloy chemical composition elasticity electrical resistance heat treatability oxidation resistance physical properties tensile properties wrought nickel alloys UNS N02205 CARPENTER NICKEL 205 ALLOY Filing Code: Nickel Alloy Ni-383 - DIGEST- MAY 1990 DATA...
Journal Articles
Alloy Digest (1978) 27 (7): Co-20.
Published: 01 July 1978
... - DATA ON WORLD WIDE METALS AND ALLOYS HAYNES STELLITE* Alloy No. 6K =ay=$ici~~ Iant (Wrought Wear-Resistant Alloy) Upper Maudair, New Jay HAYNES STELLITE alloy No. 6K is a cobalt-base alloy with outstanding resistance to most types of wear. Its wear resistance is a built-in characteristic...