Alloy Digest (1956) 5 (4): Cu-37.
Published: 01 April 1956
... LUMEN 15 and 15A are deoxidized tin-bronze casting alloys recommended for worm gears and heavy duty bearings. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness and fatigue...
Journal Articles
Alloy Digest (1958) 7 (4): Cu-62.
Published: 01 April 1958
... NICUITE is an age-hardenable copper base alloy recommended for worm gears and bearings. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as deformation. It also includes information on corrosion...
Journal Articles
Alloy Digest (2005) 54 (4): Cu-733.
Published: 01 April 2005
... and is available in continuous tube, round rod, and rec- tangular bar. These characteristics make the alloy ideal for bush- ings, tie bar nuts, bearings, gears, worm gears, and similar application. MoldStar 21 is a wrought (UNS C62500) or cast (UNS C95900) Al-Fe-Cu alloy recommended for heavier-duty applications...
Journal Articles
Alloy Digest (1986) 35 (12): Cu-519.
Published: 01 December 1986
... in the as-cast condition. Typical applications include gears and worm wheels. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining...
Journal Articles
Alloy Digest (1968) 17 (6): Cu-188.
Published: 01 June 1968
... PROMET 104AB is a polyphase aluminum bronze, offering a combination of high strength, hardness, wear resistance, fatigue strength and good corrosion resistance. It is recommended for gears, bearing races, worm wheels, slides, etc. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (2019) 68 (11): Cu-900.
Published: 01 November 2019
... fluid ends, glands, worms, worm gears, hot mill guides, sewage treatment applications, valve components, bearing gears, bushings, landing gear parts, and handgun recoil mechanism. Producer Concast Metal Products Co. Wakeman, OH 44889, USA Tel: +1-440-965-4455 Fax: +1-440-204-1316 www.concast.com ISSN...
Journal Articles
Alloy Digest (2010) 59 (12): Cu-793.
Published: 01 December 2010
... of its high physical properties. Applications: Ampco 18.23 gives a successful performance under heavy loads and impact conditions and makes it a preferred material for heavy-duty worm gears and similar applications. Products Available: Centrifugal castings Producer: Ampco Engineered Alloys...
Journal Articles
Alloy Digest (1969) 18 (3): Cu-197.
Published: 01 March 1969
...: Extruded bars. Applications: Bushings, gears, cams, shafts, connecting rods, propeller shafts, bearing pins, worm gears, thrust washers, marine hardware, pumps, valve scats, sealing rings. Manufacturer: Ampco Metal, Inc. Milwaukee, Wiionsin ...
Journal Articles
Alloy Digest (2017) 66 (8): SA-795.
Published: 01 August 2017
... carbonitriding. Product Forms Available: Ingots and continuously cast products are formed to bars as required. Applications: Plastic processing for cylinders in pressing, pistons, worm gears, and injection nozzles; gear manufacture for rolls, gears, and pinions; engine construction for crankshafts, connecting...
Journal Articles
Alloy Digest (1964) 13 (4): Cu-140.
Published: 01 April 1964
... coefficient of friction. It has very good non- seizing and non-galling characteristics. Forms Available: Extrusions (solid and hollow bar forms). Applications: Bushings, bearings, gears, rams, nuts, connecting rods, shafting, idler shaft, valve stems, worm gears, feed fingers, lead screw nuts. Manufacturer...
Journal Articles
Alloy Digest (2017) 66 (5): SA-785.
Published: 01 May 2017
... Product Forms Available: Ingots and continuously cast products are formed to bars as required. Applications: Plastic processing for cylinders in pressing, pistons, worm gears, and injection nozzles Gear manufacture for rolls, gears, and pinions Engine construction for crankshafts, connecting rods...
Journal Articles
Alloy Digest (2017) 66 (7): SA-791.
Published: 01 July 2017
... carbonitriding. Product Forms Available: Ingots and continuously cast products are formed to bars as required. Applications: Plastic processing for cylinders in pressing, pistons, worm gears, and injection nozzles; gear manufacture for rolls, gears, and pinions; engine construction for crankshafts, connecting...
Journal Articles
Alloy Digest (2017) 66 (10): SA-802.
Published: 01 October 2017
... carbonitriding. Product Forms Available: Ingots and continuously cast products are formed to bars as required. Applications: Plastic processing for cylinders in pressing, pistons, worm gears, and injection nozzles; gear manufacture for rolls, gears, and pinions; engine construction for crankshafts, connecting...
Journal Articles
Alloy Digest (2017) 66 (11): SA-806.
Published: 01 November 2017
... carbonitriding Product Forms Available: Ingots and continuously cast products are formed to bars as required. Applications: Plastic processing for cylinders in pressing, pistons, worm gears, and injection nozzles; gear manufacture for rolls, gears, and pinions; engine construction for crankshafts, connecting...
Journal Articles
Alloy Digest (1962) 11 (8): SA-133.
Published: 01 August 1962
... bars. Applications: .4rbors, worms, gears, pinions, bolts, studs, callender rolls, sprockets, knitting cylinders, racks, boring bars, sleeve shafts, drill and reamer shanks, chuck screws, lathe spindles, motor shafts. Manufacturer: Theelock, Lovejoy and Company, Inc. Cambridge, hfassacbusetts ...
Journal Articles
Alloy Digest (2017) 66 (9): SA-797.
Published: 01 September 2017
... Forms Available: Ingots and continuously cast products are formed to bars as required. Applications: Plastic processing for cylinders in pressing, pistons, worm gears, and injection nozzles; gear manufacture for rolls, gears, and pinions; engine construction for crankshafts, connecting rods...
Journal Articles
Alloy Digest (1998) 47 (7): Al-350.
Published: 01 July 1998
.... OF machine 300 sfm IS suggesesred rmmmum Applications: Aircraft fittings, gears and shafts. fuse parts, meter shafts, gears, missile parts, regulating valves, worm gears, keys, aerospace connectors and fittings, and defense parts bility and anodizing response. The T73 and T7351 tern Producer: ALCOA Wire, Rod...
Journal Articles
Alloy Digest (1998) 47 (3): Al-346.
Published: 01 March 1998
... 2024-T4 - 2024~T851 - I Fig. I rvopmy comparisoos P varioos rmlpers corrosion cracking resistance over the T4 and T351 tempers. Other applications include clock parts, gears and shafts, COU- plings, fuse parts, rectifier parts, worm gears, veterinary and or- thopedic equipment. Table 4 Machining...
Journal Articles
Alloy Digest (1965) 14 (2): Cu-148.
Published: 01 February 1965
... shouid not be used in proloaged wo&g temperacures in excess of 450 deg. F. Forms Available: Extrusions and forgings Applications: Propeller shafts, gears, spindles, bearing pins, worm gears, cwnmiag rods, cams, drive shah, chrusr washers, marine hardware, pumps, piston heads, bushings, sleeve and thrust...
Journal Articles
Alloy Digest (2017) 66 (6): SA-787.
Published: 01 June 2017
... are formed to bars as required. Applications: Plastic processing for cylinders in pressing, pistons, worm gears, and injection nozzles; gear manufacture for rolls, gears, and pinions; engine construction for crankshafts, connecting rods, and cylinders; toolmaking; and machine tool construction. Producer...