Skip Nav Destination
Close Modal
Search Results for
workability
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 4571
Search Results for workability
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Journal Articles
MAGIVAL MG1: Workable Ferritic Stainless Steel
Available to Purchase
Alloy Digest (2013) 62 (10): SS-1159.
Published: 01 October 2013
... MAGIVAL MG1 is the best known ferritic free machining stainless steel grade, developed for magnetic applications, and it has high machinability and corrosion resistance similar to type 430F. Magival steels are easily workable ferritic stainless steels developed for magnetic applications where high...
Abstract
View articletitled, MAGIVAL MG1: <span class="search-highlight">Workable</span> Ferritic Stainless Steel
View
PDF
for article titled, MAGIVAL MG1: <span class="search-highlight">Workable</span> Ferritic Stainless Steel
MAGIVAL MG1 is the best known ferritic free machining stainless steel grade, developed for magnetic applications, and it has high machinability and corrosion resistance similar to type 430F. Magival steels are easily workable ferritic stainless steels developed for magnetic applications where high permeability and low coercive force are required. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-1159. Producer or source: Valbruna Stainless Steel.
Journal Articles
MAGIVAL MG2: Workable Ferritic Stainless Steel
Available to Purchase
Alloy Digest (2013) 62 (11): SS-1161.
Published: 01 November 2013
... MAGIVAL MG2 is a free machining ferritic stainless steel grade with the same high machinability and corrosion resistance as type 430F, but offering a higher magnetic permeability and lower coercive force than MG1 (Alloy Digest SS-1159, October 2013). Magival is a group of easily workable ferritic...
Abstract
View articletitled, MAGIVAL MG2: <span class="search-highlight">Workable</span> Ferritic Stainless Steel
View
PDF
for article titled, MAGIVAL MG2: <span class="search-highlight">Workable</span> Ferritic Stainless Steel
MAGIVAL MG2 is a free machining ferritic stainless steel grade with the same high machinability and corrosion resistance as type 430F, but offering a higher magnetic permeability and lower coercive force than MG1 (Alloy Digest SS-1159, October 2013). Magival is a group of easily workable ferritic stainless steels developed for magnetic applications where high permeability and low coercive force are required. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-1161. Producer or source: Valbruna Stainless Steel.
Journal Articles
MAGIVAL MG4: Workable Ferritic Stainless Steel
Available to Purchase
Alloy Digest (2014) 63 (1): SS-1165.
Published: 01 January 2014
...-resistant alloys elasticity hardness heat treatability joinability machinability MAGIVAL MG4 magnetic permeability physical properties workability DATA ON WORLDWIDE METALS AND ALLOYS Copyright © 2014, ASM International®. All rights reserved. Data shown are typical, not to be used...
Abstract
View articletitled, MAGIVAL MG4: <span class="search-highlight">Workable</span> Ferritic Stainless Steel
View
PDF
for article titled, MAGIVAL MG4: <span class="search-highlight">Workable</span> Ferritic Stainless Steel
MAGIVAL MG4 is a free machining ferritic stainless steel grade with the machinability and corrosion resistance as MG3 (Alloy Digest SS-1164, December 2013), and offering a higher magnetic permeability and lower coercive force than MG1 (Alloy Digest SS-1159, October 2013). Its higher silicon content allows it to reduce the eddy currents losses in components working in AC, and its molybdenum content allows applications in mild chloride corrosive environments. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-1165. Producer or source: Valbruna Stainless Steel.
Journal Articles
MUELLER ALLOY 3300: Low Leaded Brass
Available to Purchase
Alloy Digest (1981) 30 (11): Cu-425.
Published: 01 November 1981
... MUELLER Alloy 3300 is a brass containing 0.5% lead for improving machinability. The lead detracts somewhat from its cold workability; however, despite the lead, cold workability is rated as excellent. Overall, the alloy has a good to excellent combination of machinability and cold workability...
Abstract
View articletitled, MUELLER ALLOY 3300: Low Leaded Brass
View
PDF
for article titled, MUELLER ALLOY 3300: Low Leaded Brass
MUELLER Alloy 3300 is a brass containing 0.5% lead for improving machinability. The lead detracts somewhat from its cold workability; however, despite the lead, cold workability is rated as excellent. Overall, the alloy has a good to excellent combination of machinability and cold workability. It has good resistance to corrosion by various atmospheres, saline waters and mild organic chemicals. Its uses include pump and power cylinders and liners, plumbing brass goods and plumbing accessories. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-425. Producer or source: Mueller Brass Company.
Journal Articles
CARTECH Ti-3Al-8V-6Cr-4Mo-4Zr (BETA C): Ti-3Al-8V-6Cr-4Mo-4Zr Alloy
Available to Purchase
Alloy Digest (2020) 69 (11): Ti-172.
Published: 01 November 2020
...-3Al-8V-6Cr-4Mo-4Zr has gained in popularity among beta alloys because it is easier to melt and process, exhibiting low segregation, good workability, and good heat-treating properties. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also...
Abstract
View articletitled, CARTECH Ti-3Al-8V-6Cr-4Mo-4Zr (BETA C): Ti-3Al-8V-6Cr-4Mo-4Zr Alloy
View
PDF
for article titled, CARTECH Ti-3Al-8V-6Cr-4Mo-4Zr (BETA C): Ti-3Al-8V-6Cr-4Mo-4Zr Alloy
CarTech Ti-3Al-8V-6Cr-4Mo-4Zr, also known as Ti-3-8-6-4-4 and Beta C, is a metastable beta alloy used in the solution heat treated or solution heat treated and aged condition. It is appropriate for applications where very high strength, minimum weight, and corrosion resistance are important. Ti-3Al-8V-6Cr-4Mo-4Zr has gained in popularity among beta alloys because it is easier to melt and process, exhibiting low segregation, good workability, and good heat-treating properties. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ti-172. Producer or source: Carpenter Technology Corporation.
Journal Articles
CARLSON ALLOY C600 and C600 ESR: Corrosion and Heat Resistant Nickel-Base Alloy
Available to Purchase
Alloy Digest (1994) 43 (11): Ni-470.
Published: 01 November 1994
... workability. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, and machining. Filing Code: Ni-470. Producer or source: G.O. Carlson...
Abstract
View articletitled, CARLSON ALLOY C600 and C600 ESR: Corrosion and Heat Resistant Nickel-Base Alloy
View
PDF
for article titled, CARLSON ALLOY C600 and C600 ESR: Corrosion and Heat Resistant Nickel-Base Alloy
CARLSON ALLOYS C600 AND C600 ESR have excellent mechanical properties from sub-zero to elevated temperatures with excellent resistance to oxidation at high temperatures. It is a solid-solution alloy that can be hardened only by cold working. High strength at temperature is combined with good workability. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, and machining. Filing Code: Ni-470. Producer or source: G.O. Carlson Inc.
Journal Articles
SP 700: Beta Rich Alpha-Beta Titanium Alloy
Available to Purchase
Alloy Digest (1995) 44 (6): Ti-107.
Published: 01 June 1995
... SP 700 is a high strength, beta-rich alpha-beta titanium alloy. It was developed with the following attributes: (1) excellent hot- and cold-workability; (2) enhanced hardenability with a wide range of mechanical properties that can be obtained by heat treatment; and (3) superior superplastic...
Abstract
View articletitled, SP 700: Beta Rich Alpha-Beta Titanium Alloy
View
PDF
for article titled, SP 700: Beta Rich Alpha-Beta Titanium Alloy
SP 700 is a high strength, beta-rich alpha-beta titanium alloy. It was developed with the following attributes: (1) excellent hot- and cold-workability; (2) enhanced hardenability with a wide range of mechanical properties that can be obtained by heat treatment; and (3) superior superplastic behavior at low temperature (around 1050 K). This datasheet provides information on composition, physical properties, microstructure, elasticity, tensile properties, and bend strength. It also includes information on high temperature performance as well as heat treating. Filing Code: TI-107. Producer or source: NKK Corporation.
Journal Articles
REMANIT 4003: Ferritic Stainless Steel
Available to Purchase
Alloy Digest (1995) 44 (10): SS-615.
Published: 01 October 1995
... REMANIT 4003 possesses good workability, weldability and is mainly used in the transportation industry. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on high temperature performance as well as forming, heat...
Abstract
View articletitled, REMANIT 4003: Ferritic Stainless Steel
View
PDF
for article titled, REMANIT 4003: Ferritic Stainless Steel
REMANIT 4003 possesses good workability, weldability and is mainly used in the transportation industry. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on high temperature performance as well as forming, heat treating, machining, and joining. Filing Code: SS-615. Producer or source: Thyssen Stahl AG.
Journal Articles
REMANIT 4589: Corrosion-Resistant Stainless Steel
Available to Purchase
Alloy Digest (1996) 45 (6): SS-647.
Published: 01 June 1996
... Remanit 4589 was developed specifically for structual parts exposed to loads demanding higher yield points. Due to its composition, this steel exhibits a compromise of high loadability, good wear, and good workability. This datasheet provides information on composition, physical properties...
Abstract
View articletitled, REMANIT 4589: Corrosion-Resistant Stainless Steel
View
PDF
for article titled, REMANIT 4589: Corrosion-Resistant Stainless Steel
Remanit 4589 was developed specifically for structual parts exposed to loads demanding higher yield points. Due to its composition, this steel exhibits a compromise of high loadability, good wear, and good workability. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-647. Producer or source: Thyssen Stahl AG.
Journal Articles
AVESTA SHEFFIELD SAF 2304: Austenitic/Ferritic Duplex Stainless Steel
Available to Purchase
Alloy Digest (1996) 45 (8): SS-649.
Published: 01 August 1996
... Avesta Sheffield SAF 2304 is an austenitic/ferritic duplex stainless steel with high tensile strength, impact toughness with good workability and weldability. The alloy has high resistance to chloride stress-corrosion cracking and good resistance to pitting, crevice, and general corrosion. It has...
Abstract
View articletitled, AVESTA SHEFFIELD SAF 2304: Austenitic/Ferritic Duplex Stainless Steel
View
PDF
for article titled, AVESTA SHEFFIELD SAF 2304: Austenitic/Ferritic Duplex Stainless Steel
Avesta Sheffield SAF 2304 is an austenitic/ferritic duplex stainless steel with high tensile strength, impact toughness with good workability and weldability. The alloy has high resistance to chloride stress-corrosion cracking and good resistance to pitting, crevice, and general corrosion. It has higher thermal conductivity and a lower coefficient of thermal expansion than austenitic stainless steel. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-649. Producer or source: Avesta Sheffield Inc.
Journal Articles
RAONEL 600: Heat Resisting Alloy
Available to Purchase
Alloy Digest (1962) 11 (12): Ni-77.
Published: 01 December 1962
... RAonel 600 is a corrosion and heat resisting nickel-base alloy having a combination of high strength and oxidation resistance along with hot and cold workability. It is recommended for component parts in the aircraft, chemical, petroleum and paper pulp industries. This datasheet provides...
Abstract
View articletitled, RAONEL 600: Heat Resisting Alloy
View
PDF
for article titled, RAONEL 600: Heat Resisting Alloy
RAonel 600 is a corrosion and heat resisting nickel-base alloy having a combination of high strength and oxidation resistance along with hot and cold workability. It is recommended for component parts in the aircraft, chemical, petroleum and paper pulp industries. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ni-77. Producer or source: Rolled Alloys Inc..
Journal Articles
AMPHOS: Phosphorized Copper
Available to Purchase
Alloy Digest (1963) 12 (11): Cu-135.
Published: 01 November 1963
... Amphos is a phosphorized oxygen-free copper having free-scaling properties, freedom from hydrogen embrittlement, improved cold workability, and desirable high softening temperature. This datasheet provides information on composition, physical properties, and tensile properties. It also includes...
Abstract
View articletitled, AMPHOS: Phosphorized Copper
View
PDF
for article titled, AMPHOS: Phosphorized Copper
Amphos is a phosphorized oxygen-free copper having free-scaling properties, freedom from hydrogen embrittlement, improved cold workability, and desirable high softening temperature. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on forming, heat treating, and joining. Filing Code: Cu-135. Producer or source: American Metal Climax Inc..
Journal Articles
ALUMINUM 7076: Heat Treatable Aluminum Alloy
Available to Purchase
Alloy Digest (1965) 14 (2): Al-143.
Published: 01 February 1965
... Aluminum 7076 is an ultra-strength aluminum forging alloy exhibiting exceptional mechanical properties, workability, and response to age-hardening heat treatment. It is suitable for highly stressed structural parts. This datasheet provides information on composition, physical properties, hardness...
Abstract
View articletitled, ALUMINUM 7076: Heat Treatable Aluminum Alloy
View
PDF
for article titled, ALUMINUM 7076: Heat Treatable Aluminum Alloy
Aluminum 7076 is an ultra-strength aluminum forging alloy exhibiting exceptional mechanical properties, workability, and response to age-hardening heat treatment. It is suitable for highly stressed structural parts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as heat treating, machining, and joining. Filing Code: Al-143. Producer or source: Aluminum Company of America.
Journal Articles
PHOSNIC BRONZE: High Strength and High Conductivity Bronze
Available to Purchase
Alloy Digest (1965) 14 (2): Cu-12.
Published: 01 February 1965
... CHASE PHOSNIC BRONZE is a high copper alloy combining high strength and high conductivity, both electrical and thermal, in an unusual degree. It has high workability and excellent corrosion resistance. The additions of nickel and phosphorus to the copper render the alloy capable of being hardened...
Abstract
View articletitled, PHOSNIC BRONZE: High Strength and High Conductivity Bronze
View
PDF
for article titled, PHOSNIC BRONZE: High Strength and High Conductivity Bronze
CHASE PHOSNIC BRONZE is a high copper alloy combining high strength and high conductivity, both electrical and thermal, in an unusual degree. It has high workability and excellent corrosion resistance. The additions of nickel and phosphorus to the copper render the alloy capable of being hardened and strengthened by age-hardening heat treatment. The alloy has also high endurance strength in the harder drawn tempers of wire, and excellent resistance to creep or flow under the influence of prolonged stress. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep and fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-12. Producer or source: Chase Brass & Copper Company Inc.. Originally published November 1953, revised February 1965.
Journal Articles
TRI-STEEL: High Strength Low Alloy Steel
Available to Purchase
Alloy Digest (1966) 15 (1): SA-189.
Published: 01 January 1966
... Tri-Steel is a high strength low-alloy steel which is resistant to shock, atmospheric corrosion, abrasion, and fatigue and has good workability and welding properties. It is intended for applications requiring high strength for which a carbon steel is not adequate. This datasheet provides...
Abstract
View articletitled, TRI-STEEL: High Strength Low Alloy Steel
View
PDF
for article titled, TRI-STEEL: High Strength Low Alloy Steel
Tri-Steel is a high strength low-alloy steel which is resistant to shock, atmospheric corrosion, abrasion, and fatigue and has good workability and welding properties. It is intended for applications requiring high strength for which a carbon steel is not adequate. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and compressive and shear strength as well as fatigue. It also includes information on corrosion resistance as well as forming, machining, and joining. Filing Code: SA-189. Producer or source: Inland Steel Company.
Journal Articles
EVERDUR-655: High Strength Titanium Alloy
Available to Purchase
Alloy Digest (1966) 15 (2): Cu-161.
Published: 01 February 1966
... EVERDUR-655 is a copper-silicon-manganese alloy having the desired combination of high strength, good workability, weldability and machinability along with high corrosion resistance. It is recommended for fasteners, springs pressure vessels and general hardware. This datasheet provides information...
Abstract
View articletitled, EVERDUR-655: High Strength Titanium Alloy
View
PDF
for article titled, EVERDUR-655: High Strength Titanium Alloy
EVERDUR-655 is a copper-silicon-manganese alloy having the desired combination of high strength, good workability, weldability and machinability along with high corrosion resistance. It is recommended for fasteners, springs pressure vessels and general hardware. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength. It also includes information on corrosion resistance as well as forming, machining, and joining. Filing Code: Cu-161. Producer or source: Anaconda American Brass Company.
Journal Articles
KAISER ALLOY 1100: Commercially Pure Aluminum
Available to Purchase
Alloy Digest (2019) 68 (11): Al-459.
Published: 01 November 2019
... Kaiser Alloy 1100 is in the commercially pure wrought family (1000 or 1xxx series) of aluminum alloys. It is typically used in applications requiring maximum ductility and relatively low strength. It has good corrosion resistance, workability, and weldability. This datasheet provides information...
Abstract
View articletitled, KAISER ALLOY 1100: Commercially Pure Aluminum
View
PDF
for article titled, KAISER ALLOY 1100: Commercially Pure Aluminum
Kaiser Alloy 1100 is in the commercially pure wrought family (1000 or 1xxx series) of aluminum alloys. It is typically used in applications requiring maximum ductility and relatively low strength. It has good corrosion resistance, workability, and weldability. This datasheet provides information on composition, physical properties, hardness, elasticity, and shear strength as well as fatigue. It also includes information on high temperature performance and corrosion resistance as well as machining and joining. Filing Code: Al-459. Producer or source: Kaiser Aluminum Corporation.
Journal Articles
VDM 33: High-Chromium Austenitic Alloy
Available to Purchase
Alloy Digest (2023) 72 (9): Ni-786.
Published: 01 September 2023
... VDM 33 (Nicrofer 3033) is an austenitic alloy that has an excellent resistance against common corrosion and pitting corrosion in media containing chloride due to its well-balanced analysis and extraordinarily high chromium content. Also because of its very high strength and good workability, VDM...
Abstract
View articletitled, VDM 33: High-Chromium Austenitic Alloy
View
PDF
for article titled, VDM 33: High-Chromium Austenitic Alloy
VDM 33 (Nicrofer 3033) is an austenitic alloy that has an excellent resistance against common corrosion and pitting corrosion in media containing chloride due to its well-balanced analysis and extraordinarily high chromium content. Also because of its very high strength and good workability, VDM 33 is a material that can be used for many applications in the chemical processing industry. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-786. Producer or source: VDM Metals GmbH (a subsidiary of Acerinox, S.A.).
Journal Articles
ALUMINUM 75S: Heat Treatable Wrought Aluminum Alloy
Available to Purchase
Alloy Digest (1953) 2 (2): Al-5.
Published: 01 February 1953
... ALUMINUM 75S is an ultra-strength aluminum alloy exhibiting exceptional mechanical properties, workability, and response to various degrees of heat treatment and refrigeration. It is suitable for highly stressed primary structures. This datasheet provides information on composition, physical...
Abstract
View articletitled, ALUMINUM 75S: Heat Treatable Wrought Aluminum Alloy
View
PDF
for article titled, ALUMINUM 75S: Heat Treatable Wrought Aluminum Alloy
ALUMINUM 75S is an ultra-strength aluminum alloy exhibiting exceptional mechanical properties, workability, and response to various degrees of heat treatment and refrigeration. It is suitable for highly stressed primary structures. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fatigue. It also includes information on low temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Al-5. Producer or source: Aluminum Company of America.
Journal Articles
ALUMINUM 50S: Low Cost, Moderate Strength Aluminum Alloy
Available to Purchase
Alloy Digest (1953) 2 (3): Al-6.
Published: 01 March 1953
... ALUMINUM ALLOY 50S is a wrought, non-heat treatable aluminum alloy of excellent workability and high corrosion resistance. (See update, Aluminum 5050, Alloy Digest Al-206, March 1973.) This datasheet provides information on composition, physical properties, hardness, tensile properties, and shear...
Abstract
View articletitled, ALUMINUM 50S: Low Cost, Moderate Strength Aluminum Alloy
View
PDF
for article titled, ALUMINUM 50S: Low Cost, Moderate Strength Aluminum Alloy
ALUMINUM ALLOY 50S is a wrought, non-heat treatable aluminum alloy of excellent workability and high corrosion resistance. (See update, Aluminum 5050, Alloy Digest Al-206, March 1973.) This datasheet provides information on composition, physical properties, hardness, tensile properties, and shear and bearing strength as well as fatigue. It also includes information on as well as heat treating, machining, and joining. Filing Code: Al-6. Producer or source: Aluminum Company of America.