Journal Articles
Publisher: Journals Gateway
Alloy Digest (1985) 34 (10): Cu-502.
Published: 01 October 1985
... to that of Copper Alloy No. C26000 (Cartridge brass or 70-30 brass). Among its many uses are wiring devices, springs and switches. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1978) 27 (4): Cu-351.
Published: 01 April 1978
...: Sheet and strip. Applications: Bellows connectors, circuit breakers, clips, wiring devices, relays, springs, switches, high-strength shells, and many other electrical and electronic devices. Manufacturer: Chase Brass & Copper Company, Inc. Sheet Division Cleveland, Ohio 44132. ...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2009) 58 (1): Cu-764.
Published: 01 January 2009
... terminals, springs, and connectors in the transportation field, especially automotive, as well as in electronic and electrical wiring devices. The alloy fills an important gap in properties between 260 and 510 and is used where an engineer previously had to overdesign with 510 or underdesign with 260. Where...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1966) 15 (1): Cu-160.
Published: 01 January 1966
..., springs, fuse clips, fasteners, wiring device components. Manufacturer: Bridgeport Rolling Mills Cornpan) Bridgeport, Connecricuc ...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2000) 49 (2): Cu-647.
Published: 01 February 2000
... with good stress re- laxation resistance. Specific uses include contact springs, con- nectors, and wiring devices. Producer: Olin Brass 427 N. Shamrock Street East Alton, IL 62024-1174 (618) 258-2000 (618) 258-3084 (fax) ISSN: 002-614X Cu-647B Fig. 2 Stress relaxation comparison Fig. 1 Formability...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2003) 52 (8): Cu-708.
Published: 01 August 2003
... for artillery shell and electrical wiring devices, especially for residential and commercial construction, often fab- ricated with hot dip tin coatings. The alloy has a design limitation because cold worked 260 alloy shapes may be susceptible to stress-corrosion cracking in media such as ammonia or its...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2014) 63 (10): Pt-6.
Published: 01 October 2014
... depending on the post-processing requirements. For medical use, these wires are delivered with the highest surface finish (medical class) in order to maximize the fatigue strength that is critical in implant devices such as lead wires for cochlear implants and implant electrodes. Stress-relieved conditioned...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2006) 55 (7): Ti-139.
Published: 01 July 2006
... sensitivity and forming characteristics. Product Forms Available: Bar and billet Applications: This alloy was developed for medical devices and surgical implants such as total hip replacement systems, fracture fixation plates, intermedullary rods and nails, spinal devices, screws, and wires. Producer: ATI...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1969) 18 (3): Co-58.
Published: 01 March 1969
... and tape, by drastic cold-reduction after initial hot-working of cast bars. There is no high temperature treatment, only a baking at about 1 lOOoF after final cold-working. Forms Available: Tape and wire. Applications: Electromechanical devices, recorders, speedometers, hysteresis motors, permanent memory...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2010) 59 (10): Cu-791.
Published: 01 October 2010
... and sizes. When using this alloy for low voltage measuring devices its relatively large thermoelectric force in contact with copper wire should be taken into consideration. Producer: In Germany ThyssenKrupp VDM GmbH Werdohl, Grmany Phone: +49-2392 55-0 Fax: +49-2392 55-2217 Web: www.thyssenkruppvdm.com ISSN...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1971) 20 (7): Ni-165.
Published: 01 July 1971
... HYTEMCO is a nickel-iron alloy with a high temperature coefficient of electrical resistance. It is recommended for electrical instruments and controls, such as ballistic devices and resistance thermometers, operating in air up to 1100 F. This datasheet provides information on composition, physical...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2007) 56 (11): Ag-13.
Published: 01 November 2007
... of DFT wire, cable, or ribbon. See Fig. 1. One of the more common uses of DFT wire is found in the medical device industry where designers have integrated the strength and Table 2 Typical Tensile Vales for MP-DFT Wire with a Silver Core Ultimate tensile strength 25% Ag 28% Ag 33% Ag 41% Ag % Cold work...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1979) 28 (11): Ag-9.
Published: 01 November 1979
... on the heat treatment. Forms Available: Rod, wire, sheet and strip. Applications: Light and medium-duty electrical-contact devices, slip-ring assemblies and rotor stock for rotary switches. Manufacturer: Handy & Harman New York. N.Y. 10022. ...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1965) 14 (10): Ni-106.
Published: 01 October 1965
... Tophet-C is a nickel-base alloy recommended for electrical appliances and other devices whose operating temperatures do not exceed 1850 F. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2011) 60 (12): Ni-693.
Published: 01 December 2011
.... For medical use, Sandvik delivers F562 with the highest surface finish (Medical class) in order to maximize the fatigue strength, which is critical in implant devices such as lead wires for pacemakers and heart value supports. Product Availability: Wire form: Sandvik Bioline F562 can be supplied in round...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1984) 33 (2): Cu-472.
Published: 01 February 1984
... production in tonnage quantities using conventional melting, casting and fabricating equipment. Forms Availabte: Cast cakes in various sizes up to I I tons, sheet, strip, wire rod and wire. Applications: CR 155 is an ideal material for electric motor commutators and heat-sink washers in electronic devices...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1979) 28 (9): Bi-13.
Published: 01 September 1979
... to check pouring temperature which should be about 150-212oF after melting in a double boiler, (4) Preheat parts surrounding cavity into which Cerrolow-136 is to be poured, (5) Make certain that cavity is completely filled by puddling the alloy with a fine wire before it solidifies, and (6) Allow up to 10...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1977) 26 (7): Ni-247.
Published: 01 July 1977
... of Techalloy Nickel 205 are high enough to minimize vibrational and microphonic effects. This alloy has a high Curie temperature (6800F). It also has a high magnetostriction coefficient; therefore, it is frequently used in devices employing this phenomenon. Forms Available: Rod, wire, flat wire and strip...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1968) 17 (3): Cu-186.
Published: 01 March 1968
... Hard Tensile strength, psi 75000 135000 Yield strength, psi (0.2%) 40000 115000 Elongation, % in 10 25-35 10-5 Reduction of area, % 60 20 Rockwell hardness B50 B85 *Mechanical properties vary greatly as wire is drawn to finer sizes. Table 2 - AVERAGE INCREASE IN RESISTANCE U ITH TEMPER.ATURE...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2013) 62 (6): Fe-160.
Published: 01 June 2013
... properties. Product Availability: Forms of supply. Safeni 48 can be delivered as round wire, shaped wire (profile), and strip according to the notes below. Other sizes can be offered upon request to the producer. Round Wire. Round wire is supplied cold drawn or an- nealed, with a bright or ground surface...