Alloy Digest (1957) 6 (9): SS-61.
Published: 01 September 1957
... EMPIRE CF-3M is a superior stainless steel casting alloy recommended for welded fabrications because of freedom from carbide precipitation. It is equivalent to A. C. I. CF-4M (American Casting Institute designation). This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1964) 13 (10): SS-161.
Published: 01 October 1964
... EMPIRE CF-3 is an austenitic chromium-nickel stainless steel casting alloy recommended for welded fabrications because of freedom from carbide precipitation. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep...
Journal Articles
Alloy Digest (1993) 42 (5): Ni-432.
Published: 01 May 1993
... Hastelloy Alloy G-30 filler metal is used as matching composition filler metal for fabrication of Hastelloy G-30 wrought and cast products and as filler metal for fabrication of G/G-3 alloy wrought products. It is also used for weld repair of high chromium castings and for weld overlay cladding...
Journal Articles
Alloy Digest (1979) 28 (2): SA-355.
Published: 01 February 1979
... dioxide. Uniflux V90 is used widely in shipbuilding and other fabricating industries. It provides around 88,000 psi tensile strength and around 26 foot-pounds Charpy V-notch impact at -6OoF. Composition: Physical Constants: (Deposited Weld Metal+) Typical Deposited Weld Metal 75%A-q5q CO?* - L 100% co2...
Journal Articles
Alloy Digest (1979) 28 (7): SA-362.
Published: 01 July 1979
.... It is used to deposit typically 2.40% nickel steel weld metal with good low-temperature impact properties. Uniflux 90 is used widely in shipbuilding and other fabricating industries. It provides around 85,000 psi tensile strength and around 25 foot-pounds Charpy V-notch impact at -60 F. This datasheet...
Journal Articles
Alloy Digest (1978) 27 (6): CS-73.
Published: 01 June 1978
... Uniflux V70 is a continuous flux-cored welding electrode (wire) that is used to deposit carbon steel weld metal. Welding is protected by a shielding atmosphere of either 75% argon-25% carbon dioxide or 100% carbon dioxide. Uniflux V70 is used widely in shipbuilding and other fabricating industries...
Journal Articles
Alloy Digest (1978) 27 (9): CS-74.
Published: 01 September 1978
... UNIFLUX 70 is a continuous flux-cored welding electrode (wire) for welding in carbon dioxide shielding gas in the flat groove and horizontal fillet positions. It is used widely in shipbuilding and other fabricating industries to weld carbon steel and provides around 82,000 psi tensile strength...
Journal Articles
Alloy Digest (1999) 48 (7): Ni-557.
Published: 01 July 1999
... Haynes alloy 75 is an 80 nickel-20 chromium alloy with both good oxidation resistance and good mechanical properties at high temperatures. It is amenable to all forms of fabrication and welding. A typical application for sheet metal is fabrications in gas turbine engines. This datasheet provides...
Journal Articles
Alloy Digest (1973) 22 (11): Cb-20.
Published: 01 November 1973
... FANSTEEL 291 METAL is a columbium-base alloy that can be readily fabricated, machined and welded. It is used in the high-temperature range 2800-3500 F where excellent strength-to-weight ratio can be used to advantage. It is also used in the lower temperature range 2000-2700 F because of its...
Journal Articles
Alloy Digest (1981) 30 (11): Cb-10.
Published: 01 November 1981
... of fabrication associated with columbium. Fansteel 80 Metal can be fabricated easily at room temperature and high-quality ductile welds are possible. Its applications include nuclear, liquid metal loops and structures for high-temperature environments. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1984) 33 (3): SS-441.
Published: 01 March 1984
... and structures can be fabricated easily and it can be machined readily. It can be welded easily and gives strong, ductile welds. Some of its many applications are annealing boxes, boiler baffles, dryers, furnace parts, heat exchangers and oil-refining equipment. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1985) 34 (7): SS-460.
Published: 01 July 1985
... fabricated and welded. Applications include burners, muffles, heat exchangers, quenching fixtures, expansion bellows, guide plates and combustion nozzles. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness...
Journal Articles
Alloy Digest (2001) 50 (3): SS-820.
Published: 01 March 2001
... ALZ 309 is a high-silicon, austenitic stainless steel combining high resistance to oxidation with high tensile and creep strength at elevated temperatures. Corrosion resistance is excellent. The steel has good ductility and is readily welded so that difficult shapes and structures are easily...
Journal Articles
Alloy Digest (1997) 46 (8): SA-486.
Published: 01 August 1997
... Oregon Formalloy 400 (0.17C-1.50Mn maximum)combines through hardness and toughness with superior flame cutting, forming, and welding characteristics not found in typical abrasion resistant (AR) steels. This user-friendly grade permits more latitude in design and fabrication for such uses as dump...
Journal Articles
Alloy Digest (1997) 46 (9): SA-487.
Published: 01 September 1997
... Oregon Formalloy 500 (0.30C-1.15Mn maximum)combines through hardness and toughness with superior flame cutting, forming, and welding characteristics not found in typical abrasion-resistant (AR) steels. The user-friendly grade permits more latitude in design and fabrication for such uses as dump...
Journal Articles
Alloy Digest (1997) 46 (10): SA-488.
Published: 01 October 1997
... ASTM 514 covers quenched and tempered alloy steel grades of structural quality and primarily is intended for use in welded plate work in fabricated bridge and building members. This datasheet provides information on composition and tensile properties. It also includes information on heat treating...
Journal Articles
Alloy Digest (2000) 49 (2): Ni-558.
Published: 01 February 2000
... Haynes 230-W Filler Wire is a specially formulated welding filler metal designed for the fabrication of Haynes 230 alloy (see Alloy Digest Ni-320, August 1985). This datasheet provides information on composition, physical properties, elasticity, and bend strength. It also includes information...
Journal Articles
Alloy Digest (1970) 19 (12): Ta-1.
Published: 01 December 1970
... WC Ta-10W is a tantalum-base alloy having a combination of low-temperature ductility and fabricability in both the recrystalilzed and wrought conditions, as well as excellent weld ductility. Developed originally for structural applications at elevated temperatures, it is now available...
Journal Articles
Alloy Digest (1953) 2 (11): SA-12.
Published: 01 November 1953
... JALTEN is a high-strength low-alloy steel that is readily welded and easily fabricated. It offers an opportunity to incorporate many weight-saving features in design of new products. It is produced in three grades, namely, JALTEN, #1, JALTEN #2, JALTEN #3. This datasheet provides information...
Journal Articles
Alloy Digest (1972) 21 (4): Ni-171.
Published: 01 April 1972
... UDIMET 75 is a nickel-base high-temperature alloy developed for good resistance to oxidation and scaling to 2000 F. It can be fabricated and welded readily. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also...