Journal Articles
Alloy Digest (2003) 52 (6): SA-515.
Published: 01 June 2003
... Domex 100W is a weather-resistant, very high strength steel that is used for civil engineering structural components. The alloy has a good combination of corrosion resistance, strength, toughness, formability, and weldability. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (2003) 52 (7): SA-516.
Published: 01 July 2003
... DOCOL® 100W Filing Code: SA-516 Alloy Steel July 2003 DOCOL® 100W (Extra-High-Strength Weather-Resistant Steel) Docol 100W is a very-high-strength steel that is used for transportation products. Docol is a registered trademark of SSAB Swedish Steel, Inc. Table 1 Recommended Filler Metals Producer Manual...
Journal Articles
Alloy Digest (2003) 52 (3): SA-511.
Published: 01 March 2003
... Domex 80W is a weather resistant very high-strength steel that is used for civil engineering structural components. This datasheet provides information on composition, physical properties, tensile properties, and bend strength as well as fracture toughness. It also includes information on heat...
Journal Articles
Alloy Digest (2014) 63 (8): SA-705.
Published: 01 August 2014
..., and containers. The "W" signifies a weather-resistant steel. This datasheet provides information on composition, physical properties, tensile properties, and bend strength as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing...
Journal Articles
Alloy Digest (2013) 62 (12): SA-688.
Published: 01 December 2013
... the weight of heavy vehicles, trailers, cranes, and containers. The "W" signifies a weather resistant steel. This datasheet provides information on composition, physical properties, tensile properties, and bend strength as well as fracture toughness. It also includes information on forming, heat treating...
Journal Articles
Alloy Digest (2010) 59 (4): SA-616.
Published: 01 April 2010
... Docol W steels are weather resistant during outdoor use. These steels are designated according to their lowest yield strength. In addition to its weather-resistance properties, Docol W steels are characterized by high resistance to impact and wear, good formability, and weldability. This datasheet...
Journal Articles
Alloy Digest (2017) 66 (11): SA-805.
Published: 01 November 2017
... Patinax 355P is a weathering steel that due to its chemical composition, when utilized unprotected, exhibits resistance to atmospheric corrosion over unalloyed steels. Patinax 355P has increased phosphorus content for improved weather resistance compared with Patinax 355 (Alloy Digest SA-803...
Journal Articles
Alloy Digest (2017) 66 (10): SA-803.
Published: 01 October 2017
... Patinax 355 is a weathering steel that due to its chemical composition, when utilized unprotected, exhibits resistance to atmospheric corrosion over unalloyed steels. This datasheet provides information on composition and tensile properties as well as fracture toughness. It also includes...
Journal Articles
Alloy Digest (2015) 64 (4): SA-724.
Published: 01 April 2015
...)/5 + (Ni+Cu)/15; CET + C + (Mn+Mo)/10 + (Cr+Cu)/20 + Ni/40 In addition, the weather resistance index of I > 6.0 in accordance with ASTM G101-01 is valid. I = 26.01 (% Cu) + 3.88 (% Ni) + 1.2 (% Cr) + 1.49 (% Si) + 17.28 (% P) 7.29 (% Cu) (% Ni) 9.10 (% Ni) (% P) 33.39 (% Cu...
Journal Articles
Alloy Digest (2016) 65 (6): SA-754.
Published: 01 June 2016
... the classification requirements but that the JIS Mark system is not applicable to the classification.) Corrosion Resistance: Weather Resistance. S-TEN surpasses ordinary steel in weather resistance. S-TEN2 about 4 to 6 times (similar to COR-TEN 490). Specifications Equivalents: Hot-rolled sheets and plates (all...
Journal Articles
Alloy Digest (1992) 41 (4): P-34.
Published: 01 April 1992
...: Molded parts of polystyrene are not affected by changes in relative humidity but the material is not considered a weather- resistant plastic. Continuous long-time outdoor exposure re- sults in discoloration and reduction in strength and toughness. Finely dispersed carbon black or ultraviolet stabilizers...
Journal Articles
Alloy Digest (2022) 71 (11): Cu-935.
Published: 01 November 2022
... Austral Wright Copper Alloy 220 (UNS C22000), also known as 90/10 gilding metal, is a wrought copper-zinc alloy. It combines a rich golden color with the best combination of strength, ductility, and corrosion resistance of the plain copper-zinc alloys. It weathers to a rich bronze color and can...
Journal Articles
Alloy Digest (1990) 39 (6): Cp-8.
Published: 01 June 1990
... finish and weather resistance. It is heat stabilized for high- temperature performance and resistance to ultraviolet radiation. Forms Available: Free-flowing pellets packaged in multi-wall. foil-lined, moisture-proof 25 kg bags. Gaylords can also be made available. It is produced in standard and custom...
Journal Articles
Alloy Digest (1997) 46 (5): SS-680.
Published: 01 May 1997
... Duracorr is low-cost, utilitarian 11% Cr stainless steel with more corrosion resistance and life-cycle cost advantages than weathering steels. The steel may be used where a combination of abrasion and corrosion resistance is required. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (2004) 53 (10): SS-912.
Published: 01 October 2004
... Duracorr 300 is low-cost, utilitarian 12% Cr stainless steel with more corrosion resistance and life-cycle cost advantages than weathering steels. The steel may be used where a combination of abrasion and corrosion resistance is required. The nominal hardness is 300 HB. This datasheet provides...
Journal Articles
Alloy Digest (1969) 18 (8): Cu-205.
Published: 01 August 1969
... OREIDE 5% is a tin-modified Commercial Bronze alloy having good formability weldability and corrosion resistance. It is recommended for jewelry, weather stripping, and stamped hardware. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Journal Articles
Alloy Digest (1971) 20 (11): SA-20.
Published: 01 November 1971
... MAYARI R is a low-alloy, high-strength steel having excellent resistance to atmospheric corrosion, high yield point and superior weldability. It may be fabricated with regular shop equipment used for structural-grade carbon steel. It is used widely as a weathering steel in architectural work...
Journal Articles
Alloy Digest (1981) 30 (12): Cu-427.
Published: 01 December 1981
... ANACONDA Alloy 226 nominally contains 87.5% copper and remainder zinc. This composition gives it a pleasing, rich color, hence the old name Jewelry Bronze. It possesses a resistance to dezincification and to stress-corrosion cracking that makes it ideal for all-weather usage as well...
Journal Articles
Alloy Digest (1982) 31 (2): Cu-431.
Published: 01 February 1982
... AMBRONZE 430 is a copper-zinc-tin alloy with excellent to good corrosion resistance in most environments. It has good mechanical properties and can be cold worked readily by conventional processes. Its many applications include springs, weather strip, sash chains and platers' bars and cores...
Journal Articles
Alloy Digest (1988) 37 (8): Cu-539.
Published: 01 August 1988
... UNS C42500 is a copper-zinc-tin alloy suitable for electrical switches and springs, fuse and pen clips, and weather stripping. It can be cold worked readily by conventional processes. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...