Alloy Digest (1992) 41 (3): P-33.
Published: 01 March 1992
... ULTEM 4001 is an unreinforced polyetherimide resin with an internal lubricant. It is wear resistant and it has a reduced coefficient of friction. See also ULTEM 4000 (Alloy Digest CP-21, March 1992) for reinforced resin properties. ULTEM 4001 is available in opaque colors only. This datasheet...
Journal Articles
Alloy Digest (1992) 41 (3): Cp-21.
Published: 01 March 1992
... ULTEM 4000 is a reinforced polyetherimide resin with an internal lubricant. It is wear resistant and has a reduced coefficient of friction. See also ULTEM 4001 for unreinforced resin properties (Filing code P-33, 3/92). This datasheet provides information on physical properties, hardness, tensile...
Journal Articles
Alloy Digest (1988) 37 (6): Ni-356.
Published: 01 June 1988
... CARPENTER Wear Resistant HY MU 800A is a nickel-iron-molybdenum soft magnetic alloy containing fine aluminum oxide particles for increased wear resistance as encountered in tape recorder heads. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (2003) 52 (4): CS-135.
Published: 01 April 2003
... Domex Wear is a wear-resistant, very-high-strength steel that can be cold formed. It is used in the construction and mining industries. This datasheet provides information on composition, physical properties, hardness, tensile properties, and bend strength as well as fracture toughness. It also...
Journal Articles
Alloy Digest (1969) 18 (3): TS-216.
Published: 01 March 1969
... Dargraph is an oil-hardening, graphitic steel having excellent resistance to abrasive wear, galling, scuffing and scoring. It is recommended for drawing and forming dies, bushings, pneumatic hammers, wear plates, etc. This datasheet provides information on composition, hardness, and tensile...
Journal Articles
Alloy Digest (1969) 18 (11): Co-59.
Published: 01 November 1969
... No. 4 (High Temperature Corrosion &Wear Resistant Alloy) Engineering Alloys Digest. Inc. Upper Monrclair, New Jersey Haynes Stellite No. 4 is a cobalt-base cast alloy recommended for handlmg severe conditions of abrasion. heat and corrosion. It is especially recommended to resist the severe abrasive...
Journal Articles
Alloy Digest (1970) 19 (10): CI-36.
Published: 01 October 1970
... MEEHANITE AQ is a wear and abrasion resisting iron that is readily machinable as cast but may be air hardened after machining with minimum distortion. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear...
Journal Articles
Alloy Digest (1961) 10 (8): Co-29.
Published: 01 August 1961
... HAYNES STELLITE alloy No. 3 is a cobalt-base alloy having high hardness and compressive strength, high heat and corrosion resistance, along with excellent abrasion and wear resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties...
Journal Articles
Alloy Digest (1962) 11 (1): Co-6.
Published: 01 January 1962
... REXALLOY 33 is a cast nonferrous cobalt-base alloy of chromium, tungsten and carbon which is recommended for cutting tools and wear-resistant parts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information...
Journal Articles
Alloy Digest (1962) 11 (2): Co-30.
Published: 01 February 1962
... HAYNES STELLITE Alloy No. 12 is a cobalt-base alloy having high heat and corrosion resistance with excellent wear and abrasion resistance. It will withstand moderate shock and impact. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties...
Journal Articles
Alloy Digest (1962) 11 (5): Co-31.
Published: 01 May 1962
... tensile properties Filing Code: Co-31 HAYNES STELLITE Star J-Metal Cobo tA oy MAY 1962 -DATA ON WORLD WIDE METALS AND ALLOYS HAYNES STELLITE Star J-Metal Pmblisbed by Engineering Alloys Digest, Inc. (Wear Resistant Alloy) Upper Montclair, New Jersey HAYNES STELLITE . Star J-Metal is a cobalt-base...
Journal Articles
Alloy Digest (1963) 12 (4): TS-132.
Published: 01 April 1963
... HYCC is a high-carbon high-chromium tool steel having high wear and abrasion resistance combined with non-deforming characteristics. It is particularly adaptable for blanking dies and punches. This datasheet provides information on composition, physical properties, hardness, and elasticity...
Journal Articles
Alloy Digest (1963) 12 (12): SA-158.
Published: 01 December 1963
... Jessop No. 9 is a non-magnetic super high tensile steel having exceptionally high toughness and wear resistance. It is recommended for heavy earth moving equipment subject to severe battering. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (1964) 13 (6): SA-165.
Published: 01 June 1964
..., New Jerk HAYNES Alloy No. 90 (Abrasion & Wear Resisting Alloy) HAINES .4lloy No. 90 is a high-chromium high-carbon iron-base alloy recommended for handling extreme condi- tions of wear, abrasion, and heat. Composition: Physical Constants: Carbon Chromium Silicon Manganese Nominal Specific gravity...
Journal Articles
Alloy Digest (1955) 4 (6): Cr-1.
Published: 01 June 1955
... CHROMIUM CARBIDE Grade 608 is a bonded chromium carbide having extremely high resistance to corrosion, erosion, wear and oxidation. This datasheet provides information on composition, physical properties, and hardness. It also includes information on corrosion resistance as well as forming...
Journal Articles
Alloy Digest (1975) 24 (10): TS-291.
Published: 01 October 1975
... UHB Regin 3 is a chromium-tungsten-vanadium tool steel characterized by good toughness (especially when exposed to impact stresses), high red hardness, good wear resistance and good machinability. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (2018) 67 (12): sa-833.
Published: 01 December 2018
... XAR 450 Premium is a special wear-resistant structural steel as thick plate that is water quenched and tempered. These wear resistant materials last at least five times longer than conventional steels due to their extreme hardness and toughness. This datasheet provides information on composition...
Journal Articles
Alloy Digest (2019) 68 (1): SA-836.
Published: 01 January 2019
... XAR 400W is a special wear-resistant structural steel as thick plate that is water quenched and tempered. These wear-resistant materials last at least five times longer than conventional steels due to their extreme hardness and toughness. It is heat resistant up to 400 deg C. This datasheet...
Journal Articles
Alloy Digest (1992) 41 (11): Fe-5.
Published: 01 November 1992
... Canfield Slmel. Orange. N.J. 0705O/U.S.A (Corrosion and Wear Resistant iron Alloy) DURIRON is a high-silicon corrosion resistant iron alloy useful in the handling and carrying of corrosive liquids, wastes, and gases. Composition, Wt. W: Siiicon Manganese Carbon Chromium Copper Molybdenum Iron 14.20-14.75 1...
Journal Articles
Alloy Digest (1994) 43 (5): SA-475.
Published: 01 May 1994
... on composition, hardness, and tensile properties. It also includes information on wear resistance as well as forming and joining. Filing Code: SA-475. Producer or source: Lukens Steel Company. Producer or Source: Lukens Steel Company Copyright © ASM International® 1996 1996 ASM International...