Alloy Digest (1996) 45 (11): Co-101.
Published: 01 November 1996
... The Stellite 700 series are wear-resistant alloys in which molybdenum replaces the tungsten used in traditional Stellite alloys. Both corrosion and wear resistance result. This datasheet provides information on composition, hardness, tensile properties, and compressive strength. It also includes...
Journal Articles
Alloy Digest (1975) 24 (2): Ni-215.
Published: 01 February 1975
... Nickel-Copper Alloys 505 and 506 are strong castings alloys. Both alloys combine high strength with good wear resistance. Alloy 505 (4% silicon) is employed where exceptional resistance to galling is needed. Alloy 506 (3% silicon) is recommended where good (but not exceptional) galling resistance...
Journal Articles
Alloy Digest (1988) 37 (6): Ni-356.
Published: 01 June 1988
... CARPENTER Wear Resistant HY MU 800A is a nickel-iron-molybdenum soft magnetic alloy containing fine aluminum oxide particles for increased wear resistance as encountered in tape recorder heads. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (1996) 45 (9): Co-99.
Published: 01 September 1996
... TRIBALOY ALLOY T-800 wear resistance m D/GEST - DATA ON WORLD WIDE METALS AND ALLOYS TRIBALOY@ ALLOY T-800 (Wear-Resistant Alloy with Laves Phase) Ttibaloy alloy T3ClO was derived from an alloy family developed by DuPont Excessive amounts of molybdenum and silicon included the formation during...
Journal Articles
Alloy Digest (1996) 45 (10): Co-100.
Published: 01 October 1996
... crack resistance and a lower preheat temperature compared with Tribaloy T-800 (Alloy Digest Co-99, September 1996). This datasheet provides information on composition, microstructure, and hardness. It also includes information on corrosion and wear resistance. Filing Code: CO-100. Producer or source...
Journal Articles
Alloy Digest (1961) 10 (8): Co-29.
Published: 01 August 1961
... HAYNES STELLITE alloy No. 3 is a cobalt-base alloy having high hardness and compressive strength, high heat and corrosion resistance, along with excellent abrasion and wear resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties...
Journal Articles
Alloy Digest (1962) 11 (2): Co-30.
Published: 01 February 1962
... HAYNES STELLITE Alloy No. 12 is a cobalt-base alloy having high heat and corrosion resistance with excellent wear and abrasion resistance. It will withstand moderate shock and impact. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties...
Journal Articles
Alloy Digest (1964) 13 (6): SA-165.
Published: 01 June 1964
..., New Jerk HAYNES Alloy No. 90 (Abrasion & Wear Resisting Alloy) HAINES .4lloy No. 90 is a high-chromium high-carbon iron-base alloy recommended for handling extreme condi- tions of wear, abrasion, and heat. Composition: Physical Constants: Carbon Chromium Silicon Manganese Nominal Specific gravity...
Journal Articles
Alloy Digest (1969) 18 (11): Co-59.
Published: 01 November 1969
... No. 4 (High Temperature Corrosion &Wear Resistant Alloy) Engineering Alloys Digest. Inc. Upper Monrclair, New Jersey Haynes Stellite No. 4 is a cobalt-base cast alloy recommended for handlmg severe conditions of abrasion. heat and corrosion. It is especially recommended to resist the severe abrasive...
Journal Articles
Alloy Digest (1978) 27 (7): Co-20.
Published: 01 July 1978
... HAYNES STELLITE alloy No. 6K is a cobalt-base alloy with outstanding resistance to most types of wear. Its wear resistance is a built-in characteristic and not the result of heat-treatment, plating, nitriding, or other methods used to produce a superficial hardness on metal parts. Among its many...
Journal Articles
Alloy Digest (1979) 28 (7): Co-23.
Published: 01 July 1979
... HAYNES STELLITE Alloy No. 6B is a cobalt-base alloy that is highly resistant to most types of wear. It has long service life even under constant erosive conditions, and it exhibits high resistance to seizure and galling even without lubricants. Its corrosion resistance is good in a wide variety...
Journal Articles
Alloy Digest (1962) 11 (1): Co-6.
Published: 01 January 1962
... REXALLOY 33 is a cast nonferrous cobalt-base alloy of chromium, tungsten and carbon which is recommended for cutting tools and wear-resistant parts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information...
Journal Articles
Alloy Digest (1962) 11 (5): Co-31.
Published: 01 May 1962
... tensile properties Filing Code: Co-31 HAYNES STELLITE Star J-Metal Cobo tA oy MAY 1962 -DATA ON WORLD WIDE METALS AND ALLOYS HAYNES STELLITE Star J-Metal Pmblisbed by Engineering Alloys Digest, Inc. (Wear Resistant Alloy) Upper Montclair, New Jersey HAYNES STELLITE . Star J-Metal is a cobalt-base...
Journal Articles
Alloy Digest (1955) 4 (6): Cr-1.
Published: 01 June 1955
... alloys hardness joinability physical properties workability Filing Code: Cr-1 CHROMIUM CARBIDE GRADE 608 Chromium Alloy JUNE 1955 - DATA ON WORLD WIDE METALS AND ALLOYS PubliJhed 67 Engineering Alloys Digest, Inc. Upper hfontclair, New Jersey CHROMIUM CARBIDE GRADE 608 (tieaf and Wear Resistant...
Journal Articles
Alloy Digest (2010) 59 (11): Ni-683.
Published: 01 November 2010
... Deloro 50 EXV is also called Deloro 53. It is a self-fluxing alloy for abrasion and corrosion resistance. This datasheet provides information on composition, physical properties, microstructure, hardness, and tensile properties as well as fracture toughness. It also includes information on wear...
Journal Articles
Alloy Digest (1980) 29 (8): TS-368.
Published: 01 August 1980
... WIDE METALS AND ALLOYS Q Copyright 1980. Engineering Publications. Inc. AtI rights resewed. Pubhhetl by ISSN:OO2-614X Eagineaing AIIoys Dig- Inc POStofficeBOX823 Upper MontcIair. New Jersey CARPENTER* No. 408 Punch Steel (High-Strength, Tough, Wear-Resistant Alloy) CARPENTER No. 408 Punch Steel...
Journal Articles
Alloy Digest (1993) 42 (2): Co-88.
Published: 01 February 1993
... chemical composition hardness heat treatability joinability machinability physical properties powder metal products STELLITE 98M2 PM tensile properties wear resistance thermal properties - DIGEST- DATA ON WORLD WIDE METALS AND ALLOYS STELLITE 98M2 PM Flllng Code: Cobalt Alloy co-88 FEBRUARY...
Journal Articles
Alloy Digest (1992) 41 (11): Co-86.
Published: 01 November 1992
... STELLITE 12 PM (High Temperature Wear and Corrosion Resistant Alloy) STELLITE 12 PM is a cobalt-base alloy recommended for handling severe conditions of abrasion, heat and corrosion. The PM designation indicates prealloyed atomized powders and parts made from the powder. STELLITE@ is a registered...
Journal Articles
Alloy Digest (1993) 42 (3): Co-90.
Published: 01 March 1993
... chemical composition hardness heat treatability joinability machinability physical properties powder metal products STELLITE 3PM tensile properties wear resistance thermal properties P ID1 itif Filing Code: co-90 STELLITE 3 PM Cobalt Alloy d - DIGEST- DATA ON WORLD WIDE METALS AND ALL0...
Journal Articles
Alloy Digest (1993) 42 (6): Co-92.
Published: 01 June 1993
...-9161 27 Canlllld SImU. Orange. N.J. 07050 I USA STELLITE 31 PM (High Temperature Wear and Corrosion Resistant Alloy) STELLITI? 31 PM is a cobalt-base alloy recommended for handling severe conditions of abrasion, heat and comsion. The PM designation indicates prealloyed atomized powders and parts made...