1-20 of 92 Search Results for

water supply systems

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2001) 50 (3): Cu-662.
Published: 01 March 2001
... EnviroBrass III is one of a series of alloys pursued by an industry consortium to develop alloys that meet the National Sanitation Foundation’s standard on low lead pickup in water supply systems. The research showed that a combination of bismuth and selenium provides the same beneficial effect...
Journal Articles
Alloy Digest (1962) 11 (2): Cu-113.
Published: 01 February 1962
... NDZ-BRONZE is a copper-base alloy recommended as a high-strength dezincification and dealuminization resistant valve stem material in water supply systems. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information...
Journal Articles
Alloy Digest (1965) 14 (5): Cu-151.
Published: 01 May 1965
... LAVIN NDZ-S BRONZE is a copper-base alloy recommended as a high-strength dezincification and dealuminization resistant valve stem material in water supply systems. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes...
Journal Articles
Alloy Digest (1996) 45 (6): Cu-605.
Published: 01 June 1996
... SeBiLOY I (UNS C89510) is a selenium/bismuth-modified cast red brass alloy. Its low lead content helps meet the National Sanitation Foundation’s standard on low lead pickup in water supply systems. The Se/Bi modification permits machining similar to some of the red brasses it is replacing...
Journal Articles
Alloy Digest (1996) 45 (7): Cu-606.
Published: 01 July 1996
... SeBiLOY II (UNS C89520) is a selenium/bismuth-modified cast red brass alloy. Its low lead content helps meet the National Sanitation Foundation’s standard on low lead pickup in water supply systems. The Se/Bi modification permits machining exactly like the leaded red brasses it is replacing...
Journal Articles
Alloy Digest (2011) 60 (5): SA-625.
Published: 01 May 2011
... DIWA 373 can be used for temperatures up to 500 C and is suitable for use in boilers and piping systems. It is available in thicknesses up to 250 mm (9.84 in.). Up to a thickness of 180 millimeter, it is supplied in normalized and tempered state, and above this thickness, water-quenched...
Journal Articles
Alloy Digest (1958) 7 (1): Cu-58.
Published: 01 January 1958
... Forms Available: Sand castings, centrifugal castings, sheet, strip, rods and bars, extrusions, and forgings. Applications: Ship propellers, rudders and suuts for boats; large valves and water way castings for water supply systems, hydroelectric power plants and irrigation control; valve stems, housings...
Journal Articles
Alloy Digest (2008) 57 (9): Ni-665.
Published: 01 September 2008
...) Outgoing 50 ± 5.5 (120 ± 10) Some modifications may be needed to compensate for longer hoses. Supply pressure System pressure(a) Spray parameters kPa psi Flow kPa psi Oxygen 1450 210 1925 scfh 965 ± 70 140 ± 10 Fuel (K1 kerosene) 1170 170 6.0 gph 835 ± 70 121 ± 10 Powder (nitrogen carrier) 345 50 19 20...
Journal Articles
Alloy Digest (1995) 44 (6): Cu-601.
Published: 01 June 1995
... submarines); Valve Spindles: Fasteners at off- shore platforms and submarines; Flanges; Hose couplings for batrages; Gears: Fhwneten; Mechanical Seals; Control elements in &ma&eat Valve connectors; Sutanarine weapons handling (launch systems); So- nar quipnent components; Diverless deep water oil produaion...
Journal Articles
Alloy Digest (1983) 32 (7): Ti-85.
Published: 01 July 1983
... CABOT Ti-3A1-2.5V alloy is both lightweight and strong. It has a high strength-to-weight ratio which provides a major design advantage saving weight. It can be formed readily and it has good weldability. Seamless tubing of CABOT Ti-3A1-2.5V was developed for aircraft hydraulic and fuel systems...
Journal Articles
Alloy Digest (1987) 36 (7): Be-5.
Published: 01 July 1987
... in. Tensile Strength psi, min. Yield Strength (0.2% Offset) psi, min. Elongation (I in.) 932m, in. Typical Available Sizes, in. 0.02 l-0.03 I 0.03 1-O. I25 0.126-0.250 70000 70000 70000 50000 50000 50000 IO 24 by 72 10 24 by 84 IO 24 by 66 Heat Treatment: Brush Wellman SR-2OOEis supplied normally in the form...
Journal Articles
Alloy Digest (1976) 25 (3): SS-326.
Published: 01 March 1976
... of elasticity, psi (Tension) Modulus of rigidity, psi (Torsion) Magnetic properties 0.284 7.87 28.5 x 106 105 x 106 Magnetic Table 1 - MECHANICAL PROPERTIES Table 2 - hfACHINlNC SUGGESTIONS (In condition supplied by manufacturer for use in shafting) On condition supplied by manufacturer for use in shafting...
Journal Articles
Alloy Digest (2015) 64 (7): SS-1216.
Published: 01 July 2015
.... See Fig. 3 for available size. Applications: The alloy is used as automotive exhaust systems, high- temperature heated locations, and hot water supply parts. Producer: Nippon Steel and Sumitomo Metal Chicago, IL 60611, USA Tel: (312) 751-0800 Fax: (312) 751-0345 In Japan: Chiyoda-ku, Tokyo 100-871...
Journal Articles
Alloy Digest (2000) 49 (11): Ti-115.
Published: 01 November 2000
...- ter, brackish water, or polluted water. Titanium condensers, sheet and tube heat exchangers, and plate and frame heat exchangers are used extensively in power plants, refineries, air conditioning systems, chemical plants, offshore platforms, surface ships, and submarines. Millions of feet of welded...
Journal Articles
Alloy Digest (2015) 64 (1): SS-1195.
Published: 01 January 2015
... Sandvik Pressurfect is an austenitic chromium-nickel stainless steel with low carbon content used for high-pressure gasoline direct injection (GDI) fuel system. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and bend strength...
Journal Articles
Alloy Digest (1981) 30 (2): SS-381.
Published: 01 February 1981
....) Composition: Carbon Manganese Phosphorus SUlftlI Silicon Chromium Nickel Nitrogen 0.28-0.38 1.50-3.50 0.040 max. 0.015 max. 0.60-0.90 22.00-24.00 7.00-9.00 0.28-0.40 Physical Constants: Density, lb/cu in. glcu cm Specific gravity Magnetic permeability Hot rolled Hot rolled + 2150°F (1177OC), water quenched...
Journal Articles
Alloy Digest (1992) 41 (8): Ni-409.
Published: 01 August 1992
... Yield strength, 0.2% offset, Min., MPa 379 Elongation in 2 (or 4D), Min. 30% DOI: 10.31399/asm.ad.ni0409 Copyright © ASM International® 1996 Heat Treatment: Alloy C625 is normally supplied in the as-annealed at 1925°F (1052°C) temperature, followed by rapid cool- ing. Other temperature anneals...
Journal Articles
Alloy Digest (1987) 36 (5): Be-4.
Published: 01 May 1987
...&) 47000 (325) 35000 (240) 2.0 3000-4000 (20-30) 9-10 (IO-II) Heat Treatment: Brush Wellman S-2OOF is supplied in the hot-isostatic-pressed condition. Stress Relieving: S-2OOF is stress relieved by heating to 1450°F(7900C) in vacuum or Inert gas and cooling at lOOoF per hour. Hardening: S-2OOFcannot...
Journal Articles
Alloy Digest (1983) 32 (10): Ni-293.
Published: 01 October 1983
... supply of cutting fluid. Use heavy- duty, rigid cutting equipment; tools must be sharp and have the proper geometry. High-speed-steel or carbide-tipped tools can be used successfully. A sulfurized cutting oil is recommended for high-speed- steel cutters and a water-soluble oil is recommended for carbide...
Journal Articles
Alloy Digest (2011) 60 (11): SA-636.
Published: 01 November 2011
... Dillidur 400V is a wear-resistant steel with surface hardness at room temperature of 370–430 HB. The steel is easy to weld, bend, and machine. Because of its high wear resistance and good welding performance, 400V is used in the production of agricultural machinery and industrial truck systems...