Alloy Digest (1959) 8 (9): Cu-81.
Published: 01 September 1959
... Revere No. 508 is a highly ductile, malleable and corrosion resistant copper-nickel alloy suitable for condenser and heat exchanger tubes and many engineering applications such as salt water piping aboard ship, many components of salt water and fresh water stills, feed water heater tubes...
Journal Articles
Alloy Digest (1966) 15 (9): Cu-168.
Published: 01 September 1966
... Copper Alloy 720 is a copper-nickel alloy having high corrosion resistance and retention of strength at moderately elevated temperatures. It is recommended for heat exchangers, salt water piping and relays. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1982) 31 (12): Cu-449.
Published: 01 December 1982
.... Its strength and other mechanical properties are similar to the older copper-nickel alloys (90-10 and 70-30). Alloy C72200 is used primarily for condenser and heat-exchanger tubing using seawater and for salt-water piping. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1983) 32 (3): Cu-455.
Published: 01 March 1983
... ANACONDA Alloy 230 is a single-phase brass containing nominally 85% copper and 15% zinc. It is the most widely used of the low-zinc brasses. It has excellent resistance to dezincification and season cracking. Generally it is considered to be the most durable of all alloys for commercial water pipe...
Journal Articles
Alloy Digest (1985) 34 (9): Cu-500.
Published: 01 September 1985
... uses are springs, switches, heat exchangers, salt-water piping and relays. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining...
Journal Articles
Alloy Digest (1980) 29 (3): Cu-391.
Published: 01 March 1980
... to Alloy 706 to increase its resistance to corrosion by salt water. Alloy 706 is recommended where good mechanical properties, weldability and corrosion resistance are needed. It is widely used for plates, tubing and piping that must resist seawater. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1995) 44 (5): Cu-600.
Published: 01 May 1995
..., plasma cut or machined rings and discs, heads, rolled and tack-welded cylinders, and special cut shapes. Applications: 90 10 Cu Ni is widely used in marine service, offshore platform sea water piping, tidewater power plants. desalina- tion plants, oil refineries. and in the chemical process in- dustry...
Journal Articles
Alloy Digest (1973) 22 (12): Ni-198.
Published: 01 December 1973
... water environments. Forms Available: Bar, billet, strip, wire, tubular products. Applications: Steam and gas turbine tubing and piping, rocket engine components, heat shields, furnace hardware, chemical plant hardware, marine hardware. Manufacturer: Carpenter Technology Corporation Reading, Pennsylvania...
Journal Articles
Alloy Digest (2011) 60 (5): SA-625.
Published: 01 May 2011
... DIWA 373 can be used for temperatures up to 500 C and is suitable for use in boilers and piping systems. It is available in thicknesses up to 250 mm (9.84 in.). Up to a thickness of 180 millimeter, it is supplied in normalized and tempered state, and above this thickness, water-quenched...
Journal Articles
Alloy Digest (1987) 36 (10): CS-115.
Published: 01 October 1987
... UNS No. G10450 is a plain carbon steel containing nominally 0.45% carbon. It may be used in four conditions: hot rolled, normalized, oil quenched and tempered or water quenched and tempered. It is a general-purpose construction and engineering steel and provides medium strength and medium...
Journal Articles
Alloy Digest (1987) 36 (4): TS-473.
Published: 01 April 1987
... SILICO ALLOY is a silicon-manganese shock-resisting tool steel; it has high toughness at relatively high operating hardnesses. It is primarily an oil-hardening steel because of its molybdenum content (0.45%); however, it may be water hardened. It is a low-cost, high-quality steel that combines...
Journal Articles
Alloy Digest (1968) 17 (1): Cu-184.
Published: 01 January 1968
... and characteristics. It is es- pecially recommended for sea water piping where impingement attack is encountered. Ic responds well to both hoc and cold working operations. Forms Available: Scrip, tube Applications: Heat exchangers, salt water piping, and relays. Manufacturer: Practically all copper alloy mills. ...
Journal Articles
Alloy Digest (1971) 20 (4): Pb-7.
Published: 01 April 1971
... was for water pipe by the Romans. Many of these pipes have been dug up in modem times in an almost perfect sfate of preservation, thus demonstrating the outstanding resistance of lead to soil corrosion. Lead also has excellent resistance to corrosion in many environments as a result of the rapid formation...
Journal Articles
Alloy Digest (2006) 55 (5): SS-962.
Published: 01 May 2006
... such as brackish water, sea water, caustic chlorides, and pulp mill bleach systems. Product Forms Available: Standard product forms are pipe, tube, sheet, strip, plate, round bar, forging stock, and wire.The products are available in a wide range of sizes. Cold-rolled sheet and strip are produced to one-half ASTM...
Journal Articles
Alloy Digest (1988) 37 (1): Cu-534.
Published: 01 January 1988
.... Applications: Coastal and sea-water condensers, condenser plates, distiller tubes, evaporator and heat-exchanger tubes, ferrules, and salt-water piping. Manufacturers: Into Alloys International, Inc. Huntington, West Virginia 25720. ...
Journal Articles
Alloy Digest (1959) 8 (7): Cu-77.
Published: 01 July 1959
... certain operating conditions compares favorably. Forms Available: Sheet, strip, plate, rod, bar, tube. Applications: Condenser tubes and plates, distiller tubes, tube sheets for condensers and heat exchangers, evaporator and heat-exchanger tubes, ferrules, salt water piping. The American Brass Co...
Journal Articles
Alloy Digest (2020) 69 (6): Ni-760.
Published: 01 June 2020
... equipment; sea water piping in shipbuilding; stress-corrosion cracking resistant compensators; furnace linings Grade 2(b) Flaring systems in refineries and offshore platforms; recuperators and compensators for hot exhaust gases. (a) Soft annealed. (b) Solution annealed Supplier VDM Metals GmbH Plettenberger...
Journal Articles
Alloy Digest (1971) 20 (4): Cu-231.
Published: 01 April 1971
.... Applications: Condenser tubes and plates, distiller tubes, tube sheets for condensers and heat exchangers, evaporator and heat exchanger tubes, ferrules, salt water piping, distillers tubes, hot water tanks for domestic service, tips for welding torches. Manufacturer: Most copper alloy mills. ...
Journal Articles
Alloy Digest (2009) 58 (8): Cu-773.
Published: 01 August 2009
... for wire and B135 for tube. General Characteristics: Red Brass C23000 is generally regarded as the most durable of all metals for commercial water pipe in the practical price range. Nominally composed of 85% Cu and 15% Zn, this alloy is excellent for its resistance to dezincification and season cracking...
Journal Articles
Alloy Digest (1991) 40 (2): Cu-557.
Published: 01 February 1991
... and heat-exchanger tubes, ferrules, salt water piping, off- shore drilling platform equipment. Producers: Copper and copper alloy mills. ...