Alloy Digest (1963) 12 (3): TS-130.
Published: 01 March 1963
... Silvan Star is a water hardening high-carbon tool steel recommended for general applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating...
Journal Articles
Alloy Digest (1977) 26 (4): TS-316.
Published: 01 April 1977
... GREEN LABEL DRILL ROD is a high-quality, tough, fine-grain, straight-carbon, water-hardening tool steel with a medium hardness penetration. It is supplied with a smooth, decarburization-free surface and can be used with very little machining for applications such as shafts. This datasheet provides...
Journal Articles
Alloy Digest (1974) 23 (2): TS-267.
Published: 01 February 1974
... AISI Type W2 is a water-hardening high-carbon tool steel recommended for general applications. Its vanadium content prevents austenite grain growth and improves its toughness and its resistance to fatigue and abrasion. It is shallow hardening and in sizes over 1/2-inch in diameter, it hardens...
Journal Articles
Alloy Digest (1986) 35 (11): TS-466.
Published: 01 November 1986
... and a tough unhardened core (See Figure 2). IIS case provides the hardness and wear resistance. the softer core gives u toughness. Inasmuch as it is a water-hardening steel. it will not hold its exact size or shape during hardening. Forms Available: Billets. bars and forgmgs. Applications: COLUMBIA SPECIAL...
Journal Articles
Alloy Digest (2011) 60 (12): SA-638.
Published: 01 December 2011
... are wear-resistant steels of Dillinger Hütte GTS. They are used for such applications as slide conveyors, steel plating, screen plates, cutting edges, dump trucks, loading shovel, and other construction uses. DILLIDUR 450V (Water-Quenched Wear-Resistant Steel) DILLIDUR 450V Chemical Composition, wt (Ladle...
Journal Articles
Alloy Digest (2012) 61 (1): SA-641.
Published: 01 January 2012
... Dillidur 500V is a water hardened wear-resistant steel with surface hardness at room temperature of 470-530 HB. It has the highest wear resistance of the Dillidur steels. It is used in the production of transport systems, earth-moving plants, recycling plants, and stone crushers. This datasheet...
Journal Articles
Alloy Digest (2011) 60 (11): SA-636.
Published: 01 November 2011
... International, Materials Park, OH 44073-0002, 440-338-5151 MemberServiceCenter@asminternational.org Fax 440-338-8542 www.asminternational.org Filing Code: Steel Alloy November 2011 SA-636 Dillidur steels are wear-resistant steels of Dillinger Hütte GTS. They are used for such applications as slide conveyors...
Journal Articles
Alloy Digest (1987) 36 (6): TS-477.
Published: 01 June 1987
... WATERDIE EXTRA is a high-quality water-hardening tool steel alloyed with chromium to give increased depth of hardened case with added resistance to abrasion. When quenched in water or brine, it develops a deep, uniform high-hardness case with a tough shock-dampening core. This steel gives...
Journal Articles
Alloy Digest (1983) 32 (5): CS-94.
Published: 01 May 1983
... AISI 1030 is a plain carbon steel containing nominally 0.30% carbon. It is used in the hot-rolled, normalized, oil-quenched-and-tempered or water-quenched-and-tempered conditions for general-purpose engineering and construction. It provides medium strength and toughness at low cost. Among its many...
Journal Articles
Alloy Digest (1988) 37 (12): TS-494.
Published: 01 December 1988
... forgings in air inadryplace. Specification Equivalents: AISI Type S2 UNS T41902 General Characteristics: SOLAR alloy is a water-hardening tool steel of exceptional toughness. Even at Rockwell C 59/60 it will bend before breaking. Its extreme toughness makes it suitable in many applications where no other...
Journal Articles
Alloy Digest (1965) 14 (6): TS-166.
Published: 01 June 1965
.... Welding by the gas and arc methods is difficult and the resulting welds are only moderately satisfactory. Specification Equivalents: AISI Type W2 SAE Type W2 General Characteristics: VS4 is a water hardening carbon-vanadium tool steel. It is useful for general shop applications which do not warrant...
Journal Articles
Alloy Digest (1970) 19 (6): CS-34.
Published: 01 June 1970
... AISI C1030 a medium-carbon steel used in the hot-rolled, normalized or water quenched and tempered condition for general purpose engineering and construction. It provides medium strength and toughness at low cost. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1956) 5 (12): TS-53.
Published: 01 December 1956
... COLONIAL NO. 4 is a water-hardening, high carbon tool steel containing about 3 1/2% tungsten. This datasheet provides information on composition and hardness. It also includes information on forming, heat treating, and machining. Filing Code: TS-53. Producer or source: Vanadium-Alloys Steel...
Journal Articles
Alloy Digest (1978) 27 (9): SA-350.
Published: 01 September 1978
... AISI 5132 is a medium-hardenability, through-hardening steel of low (0.75-1.00%) chromium content. It is recommended for uses where moderate strength and toughness are satisfactory. It may be used in the unhardened condition or after quenching in water or oil followed by tempering to the desired...
Journal Articles
Alloy Digest (1965) 14 (12): TS-173.
Published: 01 December 1965
... PIGIST -DATA ON WORLD WIDE METALS AND ALLOYS Pvblisbrd by Engineering Alloys Digest, Inc. RED STAR TUNGSTEN (Oil or Water Hardening Tool Steel, Type 07) Upper Montclair, New Jms Red Star Tungsten is a high-carbon low-alloy tool steel having high hardness, good toughness, and keen cutting edge...
Journal Articles
Alloy Digest (1986) 35 (3): SA-416.
Published: 01 March 1986
... UNS No. H51321 is a medium-hardenability, through-hardening steel of low (0.75-1.00%) chromium content. It is recommended for uses where moderate strength and toughness are satisfactory. It may be used in the unhardened condition or after quenching in water or oil followed by tempering...
Journal Articles
Alloy Digest (1991) 40 (9): TS-32.
Published: 01 September 1991
... SOLAR TOOL STEEL is a very tough water hardening tool steel. Even at Rockwell C 59/60, it will bend before breaking. If medium and large sections, the steel develops a hard case and tough core when hardened. This datasheet provides information on composition, physical properties, and hardness...
Journal Articles
Alloy Digest (1959) 8 (2): TS-79.
Published: 01 February 1959
... CARPENTER K-W is a water-hardening tool steel of the fast finishing type. This datasheet provides information on composition and hardness as well as fracture toughness. It also includes information on forming, heat treating, and machining. Filing Code: TS-79. Producer or source: Carpenter...
Journal Articles
Alloy Digest (1957) 6 (2): TS-55.
Published: 01 February 1957
... Special, when quenched in water or brine from 1450 deg. F., will have the maximum com- bination of hardness and toughness when drawn for one hour at 350-375 deg. F. Forms Available: Bars, rods, and wire. Applications: Taps, drills, reamers, punches, stamps, bushings, knurls, mandrels, threading...
Journal Articles
Alloy Digest (1976) 25 (3): TS-298.
Published: 01 March 1976
... AISI is a water-hardening tool steel that resists wear and abrasion from four to ten times longer than plain carbon tool steels. When hardened, it acquires a hard-slippery surface that is difficult to scratch. Its many uses for tools include dies for a variety of products, reamers and finishing...