1-20 of 130 Search Results for

washers

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1976) 25 (4): Cu-311.
Published: 01 April 1976
... Copper Alloy No. 370 is a medium-leaded brass (formerly known as Free-Cutting Muntz metal) with good machinability. It is suitable for high-speed screw machine work and is used for a wide variety of products such as gears, nuts and washers. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1985) 34 (5): CS-106.
Published: 01 May 1985
... AISI 1010 is a low-carbon steel having good formability and weldability. It is recommended for sheet stock for deep-drawing operations and in sheet and stock for structural shapes and carburized parts. Among its many applications are bushings, clutch discs, flanges, thrust washers, tinplate, nails...
Journal Articles
Alloy Digest (1984) 33 (3): Cu-473.
Published: 01 March 1984
... clips, contact springs and washers. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-473...
Journal Articles
Alloy Digest (1984) 33 (4): Cu-474.
Published: 01 April 1984
... Copper Alloy No. C40800 is brass with an addition of tin (nominally 2%). It can be machined and formed successfully. It can be joined by several methods and as good resistance to corrosion. A typical use is electrical connectors but it also can be used for bushings, washers and costume jewelry...
Journal Articles
Alloy Digest (2023) 72 (12): Cu-943.
Published: 01 December 2023
... to that of pure copper. See Table 3 for ratings of fabrication characteristics. Product Forms Bar; rod; wire; tube; shapes; plate; strip. Applications Electrical Fasteners Industrial Ordnance Others Belleville washers; clips; connectors; contact bridges; current carrying spring connectors; electrical switch...
Journal Articles
Alloy Digest (1953) 2 (12): Ag-1.
Published: 01 December 1953
... range. It is well adapted to torch, furnace, induction, resistance or dip brazing processes. It may be hand fed or preplaced. This alloy is ideal for preplacing about the joint to be brazed in the form of ri.ns washers or other special shapes. Being free of cadmium and low in zinc content, Sild~~ 355...
Journal Articles
Alloy Digest (1993) 42 (5): SS-544.
Published: 01 May 1993
... to crevice corrosion. Triplicate specimens, 100 x 150 mm were in contact with multiple crevice washers (acetyl resin) having 20 grooves and plateaus. A washer was affixed to each side of a speci- men at a torques of 8.5 Nm. The total number of poten- tial crevice sites for each specimen was 40. Seawater...
Journal Articles
Alloy Digest (1991) 40 (10): Cp-18.
Published: 01 October 1991
... THRUST WASHER TEST* Wear factor+* in air vs steel, cu in*min/ft*lb*hr 29 x 1V O Critical PV, ksi=ft/min 50 Coefficient of friction in air PV = 2Oksi*ft/min, P = 0.5 ksi 0.36 *Test perpendicular to fiber direction **Wear factor = wear rate/PV Table 4 - CHEMICAL RESISTANCE TO IMMERSION EXPOSURE Immersion...
Journal Articles
Alloy Digest (1961) 10 (12): CS-17.
Published: 01 December 1961
... vearmenr arc rc quired ro mea part service requirements with respect IO strength and wear resistance Forms Available: Cold-rolled strip. hot-rolled strip. flar bars forgings, and rods. Applications: Springs. hand tools. thrust washers lock washers drill shanks dowel pins. bushings. ball bearings. hammer...
Journal Articles
Alloy Digest (2001) 50 (7): Cu-670.
Published: 01 July 2001
..., and shapes are available in a variety of sizes. Brush Wellman has the ca- pability to provide up to 24 in. diam by long mill lengths. For special shapes, consult the producer. Applications: Mobile equipment. Linkage bushings, thrust washers, wheel bearings Pumps. Cylinder barrels, wear plates, slippers...
Journal Articles
Alloy Digest (2020) 69 (11): Ni-764.
Published: 01 November 2020
...). Product Forms Bar, rod, wire, plate, sheet, strip. Other shapes are subject to special enquiry. Applications Pipes, tubes, and fittings used in oil and gas extraction, e.g., in heat exchangers, evaporators, washers, immersion pipes in sea water cooled heat exchangers, offshore piping. Components...
Journal Articles
Alloy Digest (1983) 32 (7): CS-95.
Published: 01 July 1983
... machinability. Springs. hand 1001s. thrust washers, lock washers. drill shanks, dowel pins. bushings. ball bearings. hammer drills, punches, dies. culrrvator discs, coulter blades, plows, plow shares, springs. shovels and harrows. High-speed steel single-point cuttrng tools should be ground IO 20 Manufacturers...
Journal Articles
Alloy Digest (1968) 17 (11): Cu-193.
Published: 01 November 1968
... or die changes in forming. It has high strength. high uniformity. superior electrical and thermal conductivity, excellent wear resistance and high corrosion resistance. Forms Available: Strip Applications: Fuse clips. fasteners, lock washers. springs. electrical components. Manufacturer: Bridgeport...
Journal Articles
Alloy Digest (1981) 30 (5): Cu-417.
Published: 01 May 1981
..., diaphragms, fasteners, bellows, lock washers, clamps, etc. The combination of strength, form- ability, and stress relaxation resistance offered by this alloy exceeds that of any of the traditional high-performance alloys and also makes the alloy highly suitable for a wide variety of specialized applications...
Journal Articles
Alloy Digest (2018) 67 (5): Cu-871.
Published: 01 May 2018
... Applications Typical uses: Architectural: bridge bearing plates Hardware: beater bars, bellows, Bourdon tubing, clutch disks, cotter pins, diaphragms, fuse clips, fasteners, lock washers, sleeve bushing, springs, switch parts, truss wire, wire brushes Industrial: chemical hardware, perforated sheets...
Journal Articles
Alloy Digest (2010) 59 (6): Cu-783.
Published: 01 June 2010
... contacts, switches, connectors, chemical hardware, textile machinery plants, fuse clips, lock washers, sleeve bushing, perforated sheets, friction springs, wear guides, sprinklers. Producer: Luvata Sales, (USA), Inc. Bloomingdale, IL 60108 Tel: 630-980-8400 Fax: 630-980-8891 www.luvata.com ISSN: 002-614X...
Journal Articles
Alloy Digest (2008) 57 (8): Cu-757.
Published: 01 August 2008
...). Applications: Typical applications include bushings, bearings, shafts, gears, pinions, thrust washers, valve parts, screw machine products, and electrical connecters. Producer: Ansonia Copper & Brass, Inc. Waterbury, CT 06708 Tel: 800/512-1703 Tel: 203/735-3787 www.ansoniacb.com ISSN: 002-614X Cu-757B ...
Journal Articles
Alloy Digest (1966) 15 (1): Cu-160.
Published: 01 January 1966
... and similar applications in which the part is stressed by external loading, high operating temperatures are limited to 2250F because a constantly deflected spring undergoes relaxation or loss of load with time. Forms Available: Strip Applications: Instrument diaphrams, electrical switch parts, washers...
Journal Articles
Alloy Digest (1997) 46 (1): Cu-609.
Published: 01 January 1997
...: General utility bearings and bushings, washers. Products Available: Ingot, sand castings, centrifugal castings, permanent mold cast- ings, and continuous cast products. Effecrofseaionsize Medium -8 Lour -8 hkdium Fluidity Maiium - -gyield Producer: Magnolia Metal Corporation -NE68119 (402) 455-8760 Ingot...
Journal Articles
Alloy Digest (2013) 62 (6): Cu-819.
Published: 01 June 2013
... and stators, heavy equipment trailer thrust washers, chemical processing valves, and heavily loaded journal bearings. Producer: Materion Brush Performance Alloys Mayfield Heights, OH 44124, USA Tel: (216) 486-4200 Fax: (216) 383-4005 www.brushwellman.com ISSN: 002-614X Cu-819B ...