Alloy Digest (1980) 29 (8): TS-368.
Published: 01 August 1980
... toughness and resistance to splitting stresses. It has found a number of other uses requiring resistance to shock loading and splitting stresses, such as clutch parts, vise jaws and expander punches. This datasheet provides information on composition, hardness, and tensile properties as well as fracture...
Journal Articles
Alloy Digest (1955) 4 (6): CS-3.
Published: 01 June 1955
..., engine bolts, feed miII hammers, gauges, gears, roller dies, shafts. spindles. vise jaws, piston pins. link and valve motion parts, seaming roils, sprockets, wrist pins, thread gauges and plup. Manufacturer: Crucible Steel Company of America Pittsburgh 30, Pennsylvania ...
Journal Articles
Alloy Digest (1962) 11 (5): SA-128.
Published: 01 May 1962
..., dowel pins, straightening rolls, swaging rolls, screw drivers, nail sets, arbors, mandrels, ratchets, cams, conveyor pins, hammers, vise jaws, chuck jaws, etc. Forming inch up to 1 1 to 2 in./rev. sfpm - - 0.0015 70-80 0.00125 70-80 Circular or dovetail Cutoff Camfering and facir.g 2 co 2 l/2 0.001 70...
Journal Articles
Alloy Digest (1969) 18 (12): TS-225.
Published: 01 December 1969
... cutters, vise jaws, and hammer tools. Manufacturer: Bethlehem Steel Corporation Bethlehem, Pennsylvania ...
Journal Articles
Alloy Digest (1977) 26 (1): TS-312.
Published: 01 January 1977
... coUets. In addition, it is suitable for pneumatic tools, chipping chisels, beading, caulking, flaring and starting tools, button sets, rivet sets, shear blades, clutch dogs, vise jaws, etc. It should be considered for use wherever extreme toughness is a requirement. Manufacturer: Carpenter Technology...
Journal Articles
Alloy Digest (1956) 5 (7): SA-45.
Published: 01 July 1956
... at relatively high temperatures. Forms Available: Hot rolled bars, annealed or hat treated; cold drawn or cen- ;urAakse.round bars, annealed or hat treated; sheet and plate, Applications (Typical): Machine tools such as tool posts, back gear shafts, clutches, drive and feed gears, arbors, spindles, vise jaws...
Journal Articles
Alloy Digest (1958) 7 (4): TS-69.
Published: 01 April 1958
.... Applications: Pneumatic tools, chipping chisels, backing-out punches; bead- ing, caulking, blaring and scarfing tools; button sets, concrete busters, rivet sets, shear blades, clutch dogs, vise jaws, spring collet~, sledges, mauls, heavy duty perforating punches, drift pins, knockout pins, track chisels...
Journal Articles
Alloy Digest (1971) 20 (3): SA-262.
Published: 01 March 1971
..., but also minimizes distortion normally encountered in heat treating finished parts. Forms Available: Forging stock, billets, bars, rods. Applications: Shafts, ciutches, gears, pinions, arbors, spindles, tool posts and tool-post set screws, boring bars, vise jaws, bolts, studs, ditch-digger teeth...