1-20 of 103 Search Results for

vibration properties

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2020) 69 (1): CI-65.
Published: 01 January 2020
... Dura-Bar G2 is a gray cast iron bar is used for continuous cast products. It is a good fit for a variety of applications due to its good machinability, wear resistance, and vibration damping properties. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (2020) 69 (2): CI-66.
Published: 01 February 2020
... Dura-Bar G2 is a gray cast iron bar is used for continuous cast products. It is a good fit for a variety of applications due to its good machinability, wear resistance, and vibration damping properties. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (1960) 9 (2): Mn-1.
Published: 01 February 1960
... C.D.C. Manganese Alloy No. 772 offers a combination of high strength and ductility. It has a high temperature coefficent of expansion, high electrical resistivity, low thermal conductivity, and high vibration damping constant. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (2018) 67 (6): Mg-85.
Published: 01 June 2018
... Magnesium K1A is the casting alloy with the highest vibration-damping index. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear strength. It also includes information on corrosion resistance as well as casting, machining, and joining...
Journal Articles
Alloy Digest (1983) 32 (7): TS-416.
Published: 01 July 1983
... AISI Type 1.2 is a chromium-vanadium tool steel of modest hardenability and variable carbon content (nominally 0.50-1.10% carbon). At its lower carbon levels, it is used for tools requiring toughness and resistance to shock and vibration. At its higher carbon levels, it is recommended for...
Journal Articles
Alloy Digest (1954) 3 (2): TS-17.
Published: 01 February 1954
... Halvan tool steel is a tough alloy steel used for tools requiring resistance to shock and vibration. It is used for both cold and hot work applications. This datasheet provides information on composition, hardness, tensile properties, and shear strength as well as fracture toughness. It also...
Journal Articles
Alloy Digest (1954) 3 (8): Mn-2.
Published: 01 August 1954
... C.D.C. Manganese Alloy No. 780 is a manganese-copper binary alloy offering unusual combination of properties for power transmission. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes...
Journal Articles
Alloy Digest (1969) 18 (1): SS-219.
Published: 01 January 1969
... Crucible CG27 is a forgeable iron-nickel base alloy having an excellent combination of high temperature stress-rupture and tensile properties. It resists oxidation up to 1500 F and is recommended for gas turbine engines and turbine wheels. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1984) 33 (2): Cu-472.
Published: 01 February 1984
... number of design requirements because it can be altered easily through cold working and heat treating (annealing) to develop a wide range of properties. Its many uses include electrical springs and contacts, radiator fins, tinsel wire in telecommunications and high-strength hook-up wire in aircraft. This...
Journal Articles
Alloy Digest (2008) 57 (8): TS-670.
Published: 01 August 2008
... TOOLOX 33 is a member of the Toolox family of quenched-and-tempered prehardened tool and machine steel, delivered with guaranteed properties. Toolox 33 has a through hardness of HBW 300. This datasheet provides information on composition, physical properties, hardness, and tensile properties as...
Journal Articles
Alloy Digest (2008) 57 (9): TS-671.
Published: 01 September 2008
... TOOLOX 44 is a member of the Toolox family of quenched and tempered prehardened tool and machine steel, delivered with guaranteed properties. Toolox 44 has a hardness if HRC 45 and is ideal for nitriding. This datasheet provides information on composition, physical properties, hardness, and...
Journal Articles
Alloy Digest (1977) 26 (8): Cu-338.
Published: 01 August 1977
... Copper Alloy No. 993 is a copper-nickel-aluminum-cobalt alloy with unusually good heat-resisting properties. It was developed for use in molds for glass containers and also is used for sheet-glass rolls. Compared to cast-iron (the alloy commonly used for molds), Copper Alloy No. 993 has four...
Journal Articles
Alloy Digest (1979) 28 (5): Al-130.
Published: 01 May 1979
... ALUMINUM 2018 is an age-hardenable aluminum forging alloy characterized by relatively high tensile and yield strengths along with fairly good ductility. It has good elevated-temperature properties. Its applications include engine pistons and engine cylinder heads. This datasheet provides...
Journal Articles
Alloy Digest (1967) 16 (1): Cu-173.
Published: 01 January 1967
... Incramet 800 is a copper-base alloy exhibiting an excellent combination of mechanical, physical and corrosion resistant properties at both room and elevated temperatures. It is recommended for glass container molds and sheet glass rolls. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1957) 6 (5): Ti-12.
Published: 01 May 1957
... REM-CRU C-120AV is an alpha-beta titanium-base alloy having good high temperature strength, low temperature impact and notch rupture properties, and good creep resistance. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as...
Journal Articles
Alloy Digest (1978) 27 (11): SS-358.
Published: 01 November 1978
... AL Tech 203EZ and 303EZ are non-magnetic, austenitic, free-machining stainless steels specifically designed for use in high-speed, automatic machining operations. These modifications retain, in so far as possible, the good mechanical properties and corrosion resistance of the basic compositions...
Journal Articles
Alloy Digest (1970) 19 (5): Cu-215.
Published: 01 May 1970
... CDA 710 is a cupro-nickel alloy having high resistance to seawater corrosion and good stress-rupture properties. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep and fatigue. It also includes information on low...
Journal Articles
Alloy Digest (1967) 16 (2): SA-206.
Published: 01 February 1967
... UDIMAR B-250 is a fabricable and weldable ultra-high strength maraging steel combining the mechanical properties derived from precipitation hardening and martensitic transformation. It exhibits very high ultimate and yield strengths combined with excellent ductility and notched/unnotched ratio...
Journal Articles
Alloy Digest (2000) 49 (6): SS-794.
Published: 01 June 2000
... Allegheny Ludlum Type 303 stainless steel is a free-machining austenitic stainless steel, which retains almost all of the basic 18 chromium-8 nickel stainless steel properties. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as...
Journal Articles
Alloy Digest (2000) 49 (7): SS-796.
Published: 01 July 2000
... Allegheny Ludlum Type 416 stainless steel is a free-machining martensitic stainless steel, which can be hardened by heat treatment to higher strengths. It has better machining properties than the austenitic grades but lower corrosion resistance. This datasheet provides information on composition...