Journal Articles
Alloy Digest (1977) 26 (1): SA-328.
Published: 01 January 1977
... ASTM A 533 Grade B is a manganese-molybdenum-nickel alloy steel for use in the quenched-and-tempered condition for plate for the construction of pressure vessels and other pressure equipment. It is used in 6 to 12-inch sections and is the most widely used steel for nuclear reactor pressure vessels...
Journal Articles
Alloy Digest (2011) 60 (8): SA-630.
Published: 01 August 2011
... Diros 500 is a fine-grained pressure vessel steel delivered in two grades: one as high strength, the other for sour service. This datasheet provides information on composition, physical properties, and tensile properties as well as fracture toughness. It also includes information on forming, heat...
Journal Articles
Alloy Digest (2018) 67 (10): SA-825.
Published: 01 October 2018
... This alloy is a special steel grade for pressure vessels with HIC (hydrogen-induced cracking) resistance. This datasheet provides information on composition. It also includes information on corrosion resistance as well as forming and joining. Filing Code: SA-825. Producer or source: ThyssenKrupp...
Journal Articles
Alloy Digest (2019) 68 (5): SA-844.
Published: 01 May 2019
... Bisalloy Structural 80 Pressure Vessel Steel (80 ksi minimum yield strength) is a low-carbon, low-alloy, high-strength structural steel for pressure vessel applications. It exhibits excellent cold formability and low-temperature fracture toughness. This datasheet provides information...
Journal Articles
Alloy Digest (2011) 60 (7): SA-629.
Published: 01 July 2011
... DICREST is a series of fine grained pressure vessel steels with resistance to hydrogen induced cracking (HIC). This datasheet provides information on and physical properties. It also includes information on forming, heat treating, and joining. Filing Code: SA-629. Producer or source: Dillinger...
Journal Articles
Alloy Digest (1994) 43 (8): SA-478.
Published: 01 August 1994
...-molybdenum ferritic pressure vessel steel) The 3Cr-lMo-1/4V-Cb-Ca ferritic steel is a micro-alloyed version of 3Cr-1Mo alloys for applications at high temperature and high pressures of hydrogen in the petrochemical arena. Chemical Composition, Wt., %: Heat Product Properties: Carbon Manganese Phosphorus, max...
Journal Articles
Alloy Digest (1994) 43 (9): SA-479.
Published: 01 September 1994
.... Orange, N.J. 07054 I USA - - - 3 cr-1 M0=1/4V=Ti+3 (Chromium molybdenum pressure vessel steel) The 3Cr-lMo-1/4V-Ti-B alloy was developed as one of the best compositions to meet values for coal liquefaction reactor materials. The alloy is hydrogen resistant at high temperatures and pressures...
Journal Articles
Alloy Digest (1999) 48 (6): CS-132.
Published: 01 June 1999
... plates tensile properties thermal properties AMERICAN ALLOY TUF-37® (Pressure Vessel Steel Alloy) TUF-37 plate products are produced to special compositions of A/SA 516 and exhibit hydrogen-induced cracking (HIC) resistance. The sulfur maximum is 0.002 and the carbon equivalent (CE) averages 0.37...
Journal Articles
Alloy Digest (2020) 69 (11): Ni-764.
Published: 01 November 2020
... VDM 825 (Nicrofer 4221) is a titanium-stabilized fully austenitic Ni-Fe-Cr-Mo-Cu alloy that is designed for use in extremely corrosive environments. It is approved for pressure vessels with wall temperatures up to 450 °C (842 °F) according to VdTÜV and 538 °C (1000 °F) for Section VIII Division 1...
Journal Articles
Alloy Digest (2022) 71 (9): Ti-187.
Published: 01 September 2022
... Wright Titanium Grade 12 is used in mildly reducing conditions, or where conditions vary from oxidizing to reducing. It is particularly resistant to crevice corrosion in hot brines. AS 1210, and ASME Boiler and Pressure Vessel Code pre-qualify Austral Wright Titanium Grade 12 for use in pressure vessels...
Journal Articles
Alloy Digest (2011) 60 (10): SA-635.
Published: 01 October 2011
... CarElso 60/65 is a steel alloy with special melt practice producing a pressure vessel material with resistance to mild sour service. This datasheet provides information on composition and tensile properties as well as fracture toughness. It also includes information on forming, heat treating...
Journal Articles
Alloy Digest (2012) 61 (3): Ni-695.
Published: 01 March 2012
... Pyromet Alloy 617 is both oxidation resistant and very strong at high temperatures. It has one of the highest allowable stress values in the ASME Boiler and Pressure Vessel Code at 982 deg C (1800 deg F). This datasheet provides information on composition, physical properties, elasticity, tensile...
Journal Articles
Alloy Digest (2018) 67 (3): SA-813.
Published: 01 March 2018
... ArcelorMittal 9% nickel alloy steel plates are for use in the water quenched and tempered or double normalized condition. They are intended for the fabrication of welded pressure vessels. This datasheet provides information on composition, physical properties, elasticity, and tensile properties...
Journal Articles
Alloy Digest (1978) 27 (5): SS-350.
Published: 01 May 1978
... includes process vessels and containers in the chemical industry, steam superheaters and pickling vats. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on low...
Journal Articles
Alloy Digest (2021) 70 (1): Ni-766.
Published: 01 January 2021
... Vessel Code with design stresses up to 980 °C (1800 °F). This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-766...
Journal Articles
Alloy Digest (2015) 64 (4): SS-1205.
Published: 01 April 2015
... engines and superchargers for various high-temperature components and is one of the few age-hardenable alloys used for bolting in the ASME Boiler and Pressure Vessel Code. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture...
Journal Articles
Alloy Digest (2010) 59 (9): Al-431.
Published: 01 September 2010
... Kaiser Alloy 6005 is a pressure vessel material with corrosion resistance and weldability. This datasheet provides information on composition, physical properties, tensile properties, and shear strength as well as fatigue. It also includes information on corrosion resistance as well as forming...
Journal Articles
Alloy Digest (1967) 16 (1): SS-190.
Published: 01 January 1967
... AISI No. 634 is a transformation and precipitation hardening stainless steel. It is used for applications such as pressure vessels, aircraft constructural components and jet engine compressor components. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (1967) 16 (2): CS-26.
Published: 01 February 1967
... USS CHAR-PAC is a heat treated carbon steel having exceptionally good notch toughness as well as high strength. It is recommended for pressure vessels, low temperature storage containers, earth moving equipment, offshore drilling rigs, etc. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1967) 16 (5): SS-194.
Published: 01 May 1967
... ESSHETE 1250 is an austenitic creep resistant alloy steel recommended for high temperature service in the range 550-675 C. It is used for superheaters, pressure vessels, fasteners and turbine blades. This datasheet provides information on composition, physical properties, hardness, elasticity...